Study of alpha-case depth in Ti-6Al-2Sn-4Zr-2Mo and Ti-6Al-4V
Open Access
- 12 December 2013
- conference paper
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 48 (1) , 012002
Abstract
At temperatures exceeding 480°C titanium alloys generally oxidises and forms a hard and brittle layer enriched with oxygen, which is called alpha case. This layer has negative effects on several mechanical properties and lowers the tensile ductility and the fatigue resistance. Therefore any alpha-case formed on titanium alloys during various manufacturing processes, such as heat treatment procedures, must be removed before the final part is mounted in an engine. In addition, long time exposure at elevated temperatures during operation of an engine could possibly also lead to formation of alpha-case on actual parts, therefore knowledge and understanding of the alpha-case formation and its effect on mechanical properties is important. Factors that contribute for growth of alpha-case are: presence of oxygen, exposure time, temperature and pressure. In the present study, isothermal oxidation experiments in air were performed on forged Ti-6Al-2Sn-4Zr-2Mo at 500°C and 593°C up to 500 hours. Similar studies were also performed on Ti-6Al-4V plate at 593°C and 700°C. Alpha-case depth for both alloys was quantified using metallography techniques and compared.Keywords
This publication has 11 references indexed in Scilit:
- A Study on Alpha-Case Depth in Ti-6Al-2Sn-4Zr-2MoMetallurgical and Materials Transactions A, 2011
- Oxidation of Ti–6Al–4V alloyJournal of Alloys and Compounds, 2009
- Modeling of Alpha-Case Formation and Its Effects on the Mechanical Properties of Titanium Alloy CastingsMetallurgical and Materials Transactions A, 2007
- The Effects of the Oxygen-enriched Surface Layer on Mechanical Properties of .ALPHA.+.BETA. Type Titanium AlloysISIJ International, 2005
- Titanium and Titanium Alloys2003
- An overview on the use of titanium in the aerospace industryMaterials Science and Engineering: A, 1996
- Various aspects of the air oxidation behaviour of a Ti6Al4V alloy at temperatures in the range 600–700 °CJournal of Materials Science, 1994
- Oxidation and embrittlement of Ti-6Al-2Sn-4Zr-2Mo alloyOxidation of Metals, 1986
- The effect of exposure on fracture of Ti-6AL-4V alloyEngineering Fracture Mechanics, 1980
- THE EFFECT OF ELEVATED TEMPERATURE AND ENVIRONMENT ON THE FATIGUE CRACK GROWTH CHARACTERISTICS OF Ti?6Al?2Sn?4Zr?2Mo?0 1SiFatigue & Fracture of Engineering Materials & Structures, 1979