Outokumpu (Finland)

Type
CompanyLocations
Helsinki, FinlandRelationships
Latest Publications
- Open Access
- 11 August 2026
- Published by Wolters Kluwer Health in Journal of Occupational and Environmental Medicine
Pulmonary inflammatory markers in workers exposed to metal dusts and fumes in ferrochromium and stainless steel production
Objective: : Our aim was to determine the association between exposure to chromium compounds and the respiratory health of workers in ferrochromium and stainless steel production. Methods: : The study included 333 workers occupationally exposed/non-exposed to chromium compounds. Respiratory health was assessed using a questionnaire and spirometry. Bronchial and alveolar nitric oxide (NO) production, inflammatory markers in exhaled breath condensate, and serum samples were analyzed. Results: : There were no differences in symptoms or lung function between the study groups. Alveolar NO, 8-isprostane in exhaled breath and interleukin-8 in serum were higher in the study groups than in the controls. However, no consistent associations were found between inflammatory markers and exposure levels of air impurities. Conclusions: : Although the differences in some inflammatory markers were statistically significant, further research is needed to ascertain the clinical significance of the finding.
- 11 August 2026
- Published by Wolters Kluwer Health in Journal of Occupational and Environmental Medicine
Open AccessPulmonary inflammatory markers in workers exposed to metal dusts and fumes in ferrochromium and stainless steel production
Objective: : Our aim was to determine the association between exposure to chromium compounds and the respiratory health of workers in ferrochromium and stainless steel production. Methods: : The study included 333 workers occupationally exposed/non-exposed to chromium compounds. Respiratory health was assessed using a questionnaire and spirometry. Bronchial and alveolar nitric oxide (NO) production, inflammatory markers in exhaled breath condensate, and serum samples were analyzed. Results: : There were no differences in symptoms or lung function between the study groups. Alveolar NO, 8-isprostane in exhaled breath and interleukin-8 in serum were higher in the study groups than in the controls. However, no consistent associations were found between inflammatory markers and exposure levels of air impurities. Conclusions: : Although the differences in some inflammatory markers were statistically significant, further research is needed to ascertain the clinical significance of the finding.
- Open Access
- 28 November 2025
- Published by MDPI AG in Corrosion and Materials Degradation
- Vol. 6 (4) , 63
Field Exposure of Duplex Stainless Steel in the Marine Environment: The Impact of the Exposure Zone
Owing to its corrosion resistance, stainless steel is a sustainable alternative to carbon steel as a structural material in challenging seawater environments. Studies on carbon steel indicate that among all marine corrosion zones (i.e., atmospheric zone, splash zone, tidal zone, and immersed zone), the rate of corrosion is particularly high in the splash zone, above the seawater level, due to the recurrent splashing of seawater with high levels of oxygen and chloride content. Nevertheless, the information on the extent of localized corrosion (i.e., pitting and crevice corrosion) on stainless steel in the splash and tidal zones is scarce and, in most cases, limited to standard austenitic grades. In this work, we present the pitting and crevice corrosion results on lean duplex, duplex, and super duplex stainless steels after two years of field exposure in the North Sea (site at Heligoland South Harbour). The standard austenitic grade 1.4404 (316L) was also exposed as a reference material in atmosphere and splash zone conditions. Parallel exposure of coupons in splash, tidal, and immersed zones allows comparison of the extent of corrosion in each zone and enables proper material selection for structural applications in marine environments.
- 28 November 2025
- Published by MDPI AG in Corrosion and Materials Degradation
- Vol. 6 (4) , 63
Open AccessField Exposure of Duplex Stainless Steel in the Marine Environment: The Impact of the Exposure Zone
Owing to its corrosion resistance, stainless steel is a sustainable alternative to carbon steel as a structural material in challenging seawater environments. Studies on carbon steel indicate that among all marine corrosion zones (i.e., atmospheric zone, splash zone, tidal zone, and immersed zone), the rate of corrosion is particularly high in the splash zone, above the seawater level, due to the recurrent splashing of seawater with high levels of oxygen and chloride content. Nevertheless, the information on the extent of localized corrosion (i.e., pitting and crevice corrosion) on stainless steel in the splash and tidal zones is scarce and, in most cases, limited to standard austenitic grades. In this work, we present the pitting and crevice corrosion results on lean duplex, duplex, and super duplex stainless steels after two years of field exposure in the North Sea (site at Heligoland South Harbour). The standard austenitic grade 1.4404 (316L) was also exposed as a reference material in atmosphere and splash zone conditions. Parallel exposure of coupons in splash, tidal, and immersed zones allows comparison of the extent of corrosion in each zone and enables proper material selection for structural applications in marine environments.
- Open Access
Hydrogen-Induced Delayed Cracking in TRIP-Aided Lean-Alloyed Ferritic-Austenitic Stainless Steels
Susceptibility of three lean-alloyed ferritic-austenitic stainless steels to hydrogen-induced delayed cracking was examined, concentrating on internal hydrogen contained in the materials after production operations. The aim was to study the role of strain-induced austenite to martensite transformation in the delayed cracking susceptibility. According to the conducted deep drawing tests and constant load tensile testing, the studied materials seem not to be particularly susceptible to delayed cracking. Delayed cracks were only occasionally initiated in two of the materials at high local stress levels. However, if a delayed crack initiated in a highly stressed location, strain-induced martensite transformation decreased the crack arrest tendency of the austenite phase in a duplex microstructure. According to electron microscopy examination and electron backscattering diffraction analysis, the fracture mode was predominantly cleavage, and cracks propagated along the body-centered cubic (BCC) phases ferrite and α’-martensite. The BCC crystal structure enables fast diffusion of hydrogen to the crack tip area. No delayed cracking was observed in the stainless steel that had high austenite stability. Thus, it can be concluded that the presence of α’-martensite increases the hydrogen-induced cracking susceptibility.
Open AccessHydrogen-Induced Delayed Cracking in TRIP-Aided Lean-Alloyed Ferritic-Austenitic Stainless Steels
Susceptibility of three lean-alloyed ferritic-austenitic stainless steels to hydrogen-induced delayed cracking was examined, concentrating on internal hydrogen contained in the materials after production operations. The aim was to study the role of strain-induced austenite to martensite transformation in the delayed cracking susceptibility. According to the conducted deep drawing tests and constant load tensile testing, the studied materials seem not to be particularly susceptible to delayed cracking. Delayed cracks were only occasionally initiated in two of the materials at high local stress levels. However, if a delayed crack initiated in a highly stressed location, strain-induced martensite transformation decreased the crack arrest tendency of the austenite phase in a duplex microstructure. According to electron microscopy examination and electron backscattering diffraction analysis, the fracture mode was predominantly cleavage, and cracks propagated along the body-centered cubic (BCC) phases ferrite and α’-martensite. The BCC crystal structure enables fast diffusion of hydrogen to the crack tip area. No delayed cracking was observed in the stainless steel that had high austenite stability. Thus, it can be concluded that the presence of α’-martensite increases the hydrogen-induced cracking susceptibility.
- 26 April 2016
- Published by Taylor & Francis in Journal of Occupational and Environmental Hygiene
- Vol. 13 (7) , 558-568
Characterization of particle exposure in ferrochromium and stainless steel production
This study describes workers’ exposure to fine and ultrafine particles in the production chain of ferrochromium and stainless steel during sintering, ferrochromium smelting, stainless steel melting, and hot and cold rolling operations. Workers’ personal exposure to inhalable dust was assessed using IOM sampler with a cellulose acetate filter (AAWP, diameter 25 mm; Millipore, Bedford, MA). Filter sampling methods were used to measure particle mass concentrations in fixed locations. Particle number concentrations and size distributions were examined using an SMPS+C sequential mobile particle sizer and counter (series 5.400, Grimm Aerosol Technik, Ainring, Germany), and a hand-held condensation particle counter (CPC, model 3007, TSI Incorporated, MN). The structure and elemental composition of particles were analyzed using TEM-EDXA (TEM: JEM-1220, JEOL, Tokyo, Japan; EDXA: Noran System Six, Thermo Fisher Scientific Inc., Madison,WI). Workers’ personal exposure to inhalable dust averaged 1.87, 1.40, 2.34, 0.30, and 0.17 mg m−3 in sintering plant, ferrochromium smelter, stainless steel melting shop, hot rolling mill, and the cold rolling mill, respectively. Particle number concentrations measured using SMPS+C varied from 58 × 103 to 662 × 103 cm−3 in the production areas, whereas concentrations measured using SMPS+C and CPC3007 in control rooms ranged from 24 × 103 to 243 × 103 cm−3 and 5.1 × 103 to 97 × 103 cm−3, respectively. The elemental composition and the structure of particles in different production phases varied. In the cold-rolling mill non-process particles were abundant. In other sites, chromium and iron originating from ore and recycled steel scrap were the most common elements in the particles studied. Particle mass concentrations were at the same level as that reported earlier. However, particle number measurements showed a high amount of ultrafine particles, especially in sintering, alloy smelting and melting, and tapping operations. Particle number concentration and size distribution measurements provide important information regarding exposure to ultrafine particles, which cannot be seen in particle mass measurements.
- 26 April 2016
- Published by Taylor & Francis in Journal of Occupational and Environmental Hygiene
- Vol. 13 (7) , 558-568
Characterization of particle exposure in ferrochromium and stainless steel production
This study describes workers’ exposure to fine and ultrafine particles in the production chain of ferrochromium and stainless steel during sintering, ferrochromium smelting, stainless steel melting, and hot and cold rolling operations. Workers’ personal exposure to inhalable dust was assessed using IOM sampler with a cellulose acetate filter (AAWP, diameter 25 mm; Millipore, Bedford, MA). Filter sampling methods were used to measure particle mass concentrations in fixed locations. Particle number concentrations and size distributions were examined using an SMPS+C sequential mobile particle sizer and counter (series 5.400, Grimm Aerosol Technik, Ainring, Germany), and a hand-held condensation particle counter (CPC, model 3007, TSI Incorporated, MN). The structure and elemental composition of particles were analyzed using TEM-EDXA (TEM: JEM-1220, JEOL, Tokyo, Japan; EDXA: Noran System Six, Thermo Fisher Scientific Inc., Madison,WI). Workers’ personal exposure to inhalable dust averaged 1.87, 1.40, 2.34, 0.30, and 0.17 mg m−3 in sintering plant, ferrochromium smelter, stainless steel melting shop, hot rolling mill, and the cold rolling mill, respectively. Particle number concentrations measured using SMPS+C varied from 58 × 103 to 662 × 103 cm−3 in the production areas, whereas concentrations measured using SMPS+C and CPC3007 in control rooms ranged from 24 × 103 to 243 × 103 cm−3 and 5.1 × 103 to 97 × 103 cm−3, respectively. The elemental composition and the structure of particles in different production phases varied. In the cold-rolling mill non-process particles were abundant. In other sites, chromium and iron originating from ore and recycled steel scrap were the most common elements in the particles studied. Particle mass concentrations were at the same level as that reported earlier. However, particle number measurements showed a high amount of ultrafine particles, especially in sintering, alloy smelting and melting, and tapping operations. Particle number concentration and size distribution measurements provide important information regarding exposure to ultrafine particles, which cannot be seen in particle mass measurements.
- Open Access
- 8 December 2015
- Published by Oxford University Press (OUP) in Occupational Medicine
- Vol. 66 (3) , 241-246
Cause-specific mortality in Finnish ferrochromium and stainless steel production workers
Although stainless steel has been produced for more than a hundred years, exposure-related mortality data for production workers are limited. To describe cause-specific mortality in Finnish ferrochromium and stainless steel workers. We studied Finnish stainless steel production chain workers employed between 1967 and 2004, from chromite mining to cold rolling of stainless steel, divided into sub-cohorts by production units with specific exposure patterns. We obtained causes of death for the years 1971–2012 from Statistics Finland. We calculated standardized mortality ratios (SMRs) as ratios of observed and expected numbers of deaths based on population mortality rates of the same region. Among 8088 workers studied, overall mortality was significantly decreased (SMR 0.77; 95% confidence interval [CI] 0.70–0.84), largely due to low mortality from diseases of the circulatory system (SMR 0.71; 95% CI 0.61–0.81). In chromite mine, stainless steel melting shop and metallurgical laboratory workers, the SMR for circulatory disease was below 0.4 (SMR 0.33; 95% CI 0.07–0.95, SMR 0.22; 95% CI 0.05–0.65 and SMR 0.16; 95% CI 0.00–0.90, respectively). Mortality from accidents (SMR 0.84; 95% CI 0.67–1.04) and suicides (SMR 0.72; 95% CI 0.56–0.91) was also lower than in the reference population. Working in the Finnish ferrochromium and stainless steel industry appears not to be associated with increased mortality.
- 8 December 2015
- Published by Oxford University Press (OUP) in Occupational Medicine
- Vol. 66 (3) , 241-246
Open AccessCause-specific mortality in Finnish ferrochromium and stainless steel production workers
Although stainless steel has been produced for more than a hundred years, exposure-related mortality data for production workers are limited. To describe cause-specific mortality in Finnish ferrochromium and stainless steel workers. We studied Finnish stainless steel production chain workers employed between 1967 and 2004, from chromite mining to cold rolling of stainless steel, divided into sub-cohorts by production units with specific exposure patterns. We obtained causes of death for the years 1971–2012 from Statistics Finland. We calculated standardized mortality ratios (SMRs) as ratios of observed and expected numbers of deaths based on population mortality rates of the same region. Among 8088 workers studied, overall mortality was significantly decreased (SMR 0.77; 95% confidence interval [CI] 0.70–0.84), largely due to low mortality from diseases of the circulatory system (SMR 0.71; 95% CI 0.61–0.81). In chromite mine, stainless steel melting shop and metallurgical laboratory workers, the SMR for circulatory disease was below 0.4 (SMR 0.33; 95% CI 0.07–0.95, SMR 0.22; 95% CI 0.05–0.65 and SMR 0.16; 95% CI 0.00–0.90, respectively). Mortality from accidents (SMR 0.84; 95% CI 0.67–1.04) and suicides (SMR 0.72; 95% CI 0.56–0.91) was also lower than in the reference population. Working in the Finnish ferrochromium and stainless steel industry appears not to be associated with increased mortality.
- 30 March 2015
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 38 (10) , 1219-1227
Delayed cracking of low‐nickel austenitic stainless steel studied with constant load tensile testing
Delayed cracking in unstable low‐Ni austenitic stainless steel 204Cu was studied by constant load tensile testing. The developed testing arrangement enabled a systematical examination on the effect of applied stress, strain‐induced α′‐martensite and internal hydrogen content on time to fracture. Volume fraction of strain‐induced α′‐martensite was shown to affect cracking kinetics, except at a very high stress level. Hydrogen content had a marked effect on time to fracture, also at the highest applied stress level. When hydrogen content was reduced by annealing, delayed cracking kinetics and susceptibility were suppressed, and cracking required a considerably higher stress level. The apparent critical hydrogen content, below which delayed cracking was not observed, was about 0.85 wppm. According to scanning electron microscope and electron backscattering diffraction examination, fracture mechanism in the constant load test specimens was mainly transgranular quasi‐cleavage, and cracking propagated along α′‐martensite.
- 30 March 2015
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 38 (10) , 1219-1227
Delayed cracking of low‐nickel austenitic stainless steel studied with constant load tensile testing
Delayed cracking in unstable low‐Ni austenitic stainless steel 204Cu was studied by constant load tensile testing. The developed testing arrangement enabled a systematical examination on the effect of applied stress, strain‐induced α′‐martensite and internal hydrogen content on time to fracture. Volume fraction of strain‐induced α′‐martensite was shown to affect cracking kinetics, except at a very high stress level. Hydrogen content had a marked effect on time to fracture, also at the highest applied stress level. When hydrogen content was reduced by annealing, delayed cracking kinetics and susceptibility were suppressed, and cracking required a considerably higher stress level. The apparent critical hydrogen content, below which delayed cracking was not observed, was about 0.85 wppm. According to scanning electron microscope and electron backscattering diffraction examination, fracture mechanism in the constant load test specimens was mainly transgranular quasi‐cleavage, and cracking propagated along α′‐martensite.
- 8 July 2014
- Published by Wiley in Materials and Corrosion
- Vol. 66 (2) , 95-104
Grain boundary engineering of metastable 204Cu, 301, and 301LN austenitic stainless steels to improve their sensitization resistance
Grain boundary engineering (GBE) of 304 and 316 austenitic stainless steels has been widely researched but studies on other grades of austenitic stainless steels are less common. In this study, application of GBE on metastable austenitic stainless steels 204Cu, 301, and 301LN was assessed. Thermomechanical processing parameters were obtained for each of the tested steel grades by varying cold rolling reduction and annealing temperature, and analyzing the acquired grain boundary character distributions (GBCD) in scanning electron microscope (SEM) with electron backscatter diffraction (EBSD). A high fraction of about 80% low‐Σ CSL boundaries was attained in all of the tested steels. Effect of the GBE‐treatments on sensitization and intergranular corrosion properties was studied with Streicher and DL‐EPR tests. GBE‐treating was found to beneficially decrease the rate of intergranular corrosion and sensitization in 204Cu and 301 steels, but in low‐carbon 301LN steel no improvement was observed.
- 8 July 2014
- Published by Wiley in Materials and Corrosion
- Vol. 66 (2) , 95-104
Grain boundary engineering of metastable 204Cu, 301, and 301LN austenitic stainless steels to improve their sensitization resistance
Grain boundary engineering (GBE) of 304 and 316 austenitic stainless steels has been widely researched but studies on other grades of austenitic stainless steels are less common. In this study, application of GBE on metastable austenitic stainless steels 204Cu, 301, and 301LN was assessed. Thermomechanical processing parameters were obtained for each of the tested steel grades by varying cold rolling reduction and annealing temperature, and analyzing the acquired grain boundary character distributions (GBCD) in scanning electron microscope (SEM) with electron backscatter diffraction (EBSD). A high fraction of about 80% low‐Σ CSL boundaries was attained in all of the tested steels. Effect of the GBE‐treatments on sensitization and intergranular corrosion properties was studied with Streicher and DL‐EPR tests. GBE‐treating was found to beneficially decrease the rate of intergranular corrosion and sensitization in 204Cu and 301 steels, but in low‐carbon 301LN steel no improvement was observed.
- 16 June 2014
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 38 (1) , 29-39
Characterization of delayed cracking in deep‐drawn Swift cups of metastable austenitic stainless steels
- 16 June 2014
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 38 (1) , 29-39
Characterization of delayed cracking in deep‐drawn Swift cups of metastable austenitic stainless steels
- Open Access
Cancer incidence among Finnish ferrochromium and stainless steel production workers in 1967–2011: a cohort study
Objectives The aim of the study was to assess the risk of cancer among workers employed in the Finnish ferrochromium and stainless steel industry since the beginning of production in 1967. Methods The study cohort was made up of all persons employed by the Finnish stainless steel production chain from chromite mining to cold rolling of stainless steel during the period 1967–2004, and it was divided into subcohorts by production units with specific exposure patterns of the subcohorts assessed in previous studies. Follow-up for cancer through the files of the Finnish Cancer Registry was performed using the personal identity code as key. Standardised incidence ratios (SIRs) were calculated as the ratios of observed numbers of cancer cases and numbers expected on the basis of incidence rates in the population of the same region. Results The overall cancer incidence was at the expected level. The lung cancer risk was decreased in the whole cohort (SIR 0.79; 95% CI 0.65 to 1.08). The incidence of prostate cancer was significantly increased (1.31; 1.05 to 1.61) and that for kidney cancer was significantly decreased (0.38; 0.14 to 0.82). None of the department-specific SIRs for lung cancer were significantly different from 1.0. No cancers of the nose and nasal sinuses were observed among workers in the ferrochromium smelter or the stainless steel melting shop. Conclusions It is not likely that the occupational exposures in the Finnish ferrochromium and stainless steel industry would have increased the risk of cancer.
Open AccessCancer incidence among Finnish ferrochromium and stainless steel production workers in 1967–2011: a cohort study
Objectives The aim of the study was to assess the risk of cancer among workers employed in the Finnish ferrochromium and stainless steel industry since the beginning of production in 1967. Methods The study cohort was made up of all persons employed by the Finnish stainless steel production chain from chromite mining to cold rolling of stainless steel during the period 1967–2004, and it was divided into subcohorts by production units with specific exposure patterns of the subcohorts assessed in previous studies. Follow-up for cancer through the files of the Finnish Cancer Registry was performed using the personal identity code as key. Standardised incidence ratios (SIRs) were calculated as the ratios of observed numbers of cancer cases and numbers expected on the basis of incidence rates in the population of the same region. Results The overall cancer incidence was at the expected level. The lung cancer risk was decreased in the whole cohort (SIR 0.79; 95% CI 0.65 to 1.08). The incidence of prostate cancer was significantly increased (1.31; 1.05 to 1.61) and that for kidney cancer was significantly decreased (0.38; 0.14 to 0.82). None of the department-specific SIRs for lung cancer were significantly different from 1.0. No cancers of the nose and nasal sinuses were observed among workers in the ferrochromium smelter or the stainless steel melting shop. Conclusions It is not likely that the occupational exposures in the Finnish ferrochromium and stainless steel industry would have increased the risk of cancer.
- 2 November 2013
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 45 (3) , 1238-1246
Effect of Residual Stress and Strain-Induced α′-Martensite on Delayed Cracking of Metastable Austenitic Stainless Steels
- 2 November 2013
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 45 (3) , 1238-1246
Effect of Residual Stress and Strain-Induced α′-Martensite on Delayed Cracking of Metastable Austenitic Stainless Steels