SSAB (Sweden)

Type
CompanyLocations
Stockholm, SwedenLatest Publications
- 1 September 2026
- Published by Walter de Gruyter GmbH in Practical Metallography
- Vol. 63 (9) , 604-620
The new and improved ISO 4967
ISO 4967:2026 contains substantial technical changes and additions that enable the inclusion content in steel to be determined with significantly greater transparency and precision than before. They include the definition of width as caliper width; the redefinition of the maximum transverse distance for particles in a stringer based on facing tangents; the mandatory rating of the full length of an inclusion, regardless of its length; a categorization rule for stringers containing a mixture of low and high aspect ratio particles; redrawn images for the inclusion charts; minimum sampling recommendations for Method A; clarified rules for DS inclusions; and the introduction of new global metrics. The determination of inclusion size and type according to ISO 4967:2026 eliminates systematic underestimation of the true inclusion content in steel.
- 1 September 2026
- Published by Walter de Gruyter GmbH in Practical Metallography
- Vol. 63 (9) , 604-620
The new and improved ISO 4967
ISO 4967:2026 contains substantial technical changes and additions that enable the inclusion content in steel to be determined with significantly greater transparency and precision than before. They include the definition of width as caliper width; the redefinition of the maximum transverse distance for particles in a stringer based on facing tangents; the mandatory rating of the full length of an inclusion, regardless of its length; a categorization rule for stringers containing a mixture of low and high aspect ratio particles; redrawn images for the inclusion charts; minimum sampling recommendations for Method A; clarified rules for DS inclusions; and the introduction of new global metrics. The determination of inclusion size and type according to ISO 4967:2026 eliminates systematic underestimation of the true inclusion content in steel.
- Open Access
- 30 June 2026
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 10 (7) , 230
Influence of Heat Input and Strength Matching on the Microstructure and Mechanical Properties of GMAW Butt-Welded S700MC High-Strength Low-Alloy Steel
High-strength low-alloy (HSLA) steels produced by thermomechanical controlled processing (TMCP) are widely used in structural applications because of their high strength and weldability. However, the performance of welded joints is strongly affected by welding thermal cycles. This study investigated the effects of heat input (0.6, 1.4, and 1.8 kJ/mm) and filler metal strength (matching and undermatching) on the microstructure and mechanical properties of S700MC steel joints produced by metal-cored arc welding (MCAW). Microstructural characterization, hardness measurements, tensile testing, Charpy impact testing, and analysis of variance (ANOVA) were performed. Heat input was identified as the dominant factor controlling heat-affected zone (HAZ) development and mechanical performance. Increasing heat input enlarged the HAZ and reduced hardness through enhanced microstructural recovery. Filler metal strength mainly influenced failure location and joint strength. The lowest heat input (0.6 kJ/mm) provided the highest strength retention, particularly with the matching consumable, but also produced localized hardness peaks approaching 400 HV0.01 at the weld metal (WM)/HAZ interface, reducing ductility and impact toughness. An intermediate heat input (1.4 kJ/mm) produced the best balance between strength and toughness by promoting a more homogeneous microstructure and smoother hardness distribution. These results provide practical guidance for optimizing welding procedures for TMCP HSLA steels.
- 30 June 2026
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 10 (7) , 230
Open AccessInfluence of Heat Input and Strength Matching on the Microstructure and Mechanical Properties of GMAW Butt-Welded S700MC High-Strength Low-Alloy Steel
High-strength low-alloy (HSLA) steels produced by thermomechanical controlled processing (TMCP) are widely used in structural applications because of their high strength and weldability. However, the performance of welded joints is strongly affected by welding thermal cycles. This study investigated the effects of heat input (0.6, 1.4, and 1.8 kJ/mm) and filler metal strength (matching and undermatching) on the microstructure and mechanical properties of S700MC steel joints produced by metal-cored arc welding (MCAW). Microstructural characterization, hardness measurements, tensile testing, Charpy impact testing, and analysis of variance (ANOVA) were performed. Heat input was identified as the dominant factor controlling heat-affected zone (HAZ) development and mechanical performance. Increasing heat input enlarged the HAZ and reduced hardness through enhanced microstructural recovery. Filler metal strength mainly influenced failure location and joint strength. The lowest heat input (0.6 kJ/mm) provided the highest strength retention, particularly with the matching consumable, but also produced localized hardness peaks approaching 400 HV0.01 at the weld metal (WM)/HAZ interface, reducing ductility and impact toughness. An intermediate heat input (1.4 kJ/mm) produced the best balance between strength and toughness by promoting a more homogeneous microstructure and smoother hardness distribution. These results provide practical guidance for optimizing welding procedures for TMCP HSLA steels.
- 10 October 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (10) , 10267-10283
Static Bending Behavior of Welded Connections between Columns-to-Beam Square Hollow Sections in Strenx®700MC High-Strength Steel
- 10 October 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (10) , 10267-10283
Static Bending Behavior of Welded Connections between Columns-to-Beam Square Hollow Sections in Strenx®700MC High-Strength Steel
- Open Access
- 11 July 2025
- Published by Wiley in Steel Research International
- Vol. 97 (1) , 205-217
Experimental Study on the Melting of Hydrogen‐Reduced Iron Ore Pellets in Electric Arc Furnace‐Type Slags
Hydrogen direct reduced iron ore pellets (H‐DRI) are an increasingly relevant raw material for electric‐arc furnace steelmaking as steelmakers strives to reduce CO 2 emissions. Understanding the melting behavior of carbon‐free H‐DRI pellets in slag is needed to facilitate efficient industrial melting operations. The present study focuses on the role of slag during heating and subsequent melting of H‐DRI pellets. Experiments where single H‐DRI pellets are submerged in EAF slags with different FeO, Al 2 O 3 , and MgO contents have been done and evaluated. Results show that, within the experimental range, fastest melting progression is achieved with low FeO, high Al 2 O 3 content slags. At the most favorable conditions, 80% apparent melting is reached after 15 s, in contrast to 50% under least favorable conditions. This is likely due to differences in thermal conductivity of the slag. In pilot‐scale EAF trials where carbon‐free H‐DRI pellets is melted by continuous operation, melting performance improved with increasing FeO content. This can be explained by a decreasing viscosity which facilitated convective heat transfer. Therefore, the combination of experimental and pilot‐scale results shows that convection is the dominating heat transfer mechanism in the industrial case why it should be the focus of future research and development efforts.
- 11 July 2025
- Published by Wiley in Steel Research International
- Vol. 97 (1) , 205-217
Open AccessExperimental Study on the Melting of Hydrogen‐Reduced Iron Ore Pellets in Electric Arc Furnace‐Type Slags
Hydrogen direct reduced iron ore pellets (H‐DRI) are an increasingly relevant raw material for electric‐arc furnace steelmaking as steelmakers strives to reduce CO 2 emissions. Understanding the melting behavior of carbon‐free H‐DRI pellets in slag is needed to facilitate efficient industrial melting operations. The present study focuses on the role of slag during heating and subsequent melting of H‐DRI pellets. Experiments where single H‐DRI pellets are submerged in EAF slags with different FeO, Al 2 O 3 , and MgO contents have been done and evaluated. Results show that, within the experimental range, fastest melting progression is achieved with low FeO, high Al 2 O 3 content slags. At the most favorable conditions, 80% apparent melting is reached after 15 s, in contrast to 50% under least favorable conditions. This is likely due to differences in thermal conductivity of the slag. In pilot‐scale EAF trials where carbon‐free H‐DRI pellets is melted by continuous operation, melting performance improved with increasing FeO content. This can be explained by a decreasing viscosity which facilitated convective heat transfer. Therefore, the combination of experimental and pilot‐scale results shows that convection is the dominating heat transfer mechanism in the industrial case why it should be the focus of future research and development efforts.
- Open Access
- 2 April 2025
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 56 (3) , 2846-2872
Numerical Study on the Effect of Material Parameters and Process Conditions on the Melting Time of Hydrogen-Direct Reduced Iron
The melting time of hydrogen direct reduced iron pellets (H-DRI) is a limiting factor for productivity in electric arc furnace steelmaking for fossil-free steel. The effect of material and process parameters on melting time was evaluated under laminar conditions using computational fluid dynamics. The study found that the melting time of H-DRI is primarily determined by the properties of the slag bath and its movement, with H-DRI properties being secondary. The shortest melting time was achieved by combining high temperature (> 1950 K), high viscosity foam (> 0.1 Pa s), and high thermal conductivity (> 0.9 W m−1 K−1) of the slag. With optimal conditions a melting time of 4.56 seconds was observed for a 10 mm diameter H-DRI, although thicker slag with lower terminal velocity was shown to have greater potential for complete melting of the pellet within the slag. Decreasing H-DRI porosity from 65 to 50 pct with maintained mass increases melting time by 4 pct and increasing initial temperature from 300 K to 1100 K decreases melting time by 20 pct. Furthermore, an increased bath temperature from 1850 K to 1950 K results in approximately 55 pct reduction in melting time due to increased superheat. Forced convection in the system was also found to significantly reduce the melting time for H-DRI.
- 2 April 2025
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 56 (3) , 2846-2872
Open AccessNumerical Study on the Effect of Material Parameters and Process Conditions on the Melting Time of Hydrogen-Direct Reduced Iron
The melting time of hydrogen direct reduced iron pellets (H-DRI) is a limiting factor for productivity in electric arc furnace steelmaking for fossil-free steel. The effect of material and process parameters on melting time was evaluated under laminar conditions using computational fluid dynamics. The study found that the melting time of H-DRI is primarily determined by the properties of the slag bath and its movement, with H-DRI properties being secondary. The shortest melting time was achieved by combining high temperature (> 1950 K), high viscosity foam (> 0.1 Pa s), and high thermal conductivity (> 0.9 W m−1 K−1) of the slag. With optimal conditions a melting time of 4.56 seconds was observed for a 10 mm diameter H-DRI, although thicker slag with lower terminal velocity was shown to have greater potential for complete melting of the pellet within the slag. Decreasing H-DRI porosity from 65 to 50 pct with maintained mass increases melting time by 4 pct and increasing initial temperature from 300 K to 1100 K decreases melting time by 20 pct. Furthermore, an increased bath temperature from 1850 K to 1950 K results in approximately 55 pct reduction in melting time due to increased superheat. Forced convection in the system was also found to significantly reduce the melting time for H-DRI.
- 15 August 2024
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 55 (6) , 4257-4270
Reduction and Carburization Mechanisms for CO + H2 Reduction in Shaft Furnace Conditions
- 15 August 2024
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 55 (6) , 4257-4270
Reduction and Carburization Mechanisms for CO + H2 Reduction in Shaft Furnace Conditions
- 18 February 2024
- Published by Wiley in Steel Research International
- Vol. 95 (5)
The Influence of Nitrogen on Hydrogen Reduction of Iron Ore Pellets
As the iron and steel industry now strives for a carbon neutral industry, hydrogen‐based direct reduction shaft furnace technology has become an alternative to the heavily fossil‐depending blast furnace route. Research questions related to the future full‐scale production have, therefore, become more interesting. Depending on the operational conditions, the H2 concentration and temperature will vary across the length of the reactor. This work studies the effect of nitrogen in a hydrogen‐reducing gas during the reduction of commercial iron ore pellets using thermogravimetric analysis. The reducing gas consisted of either pure hydrogen or a mixture of 90–70 vol% hydrogen and 10–30 vol% nitrogen at 773, 873, 973, 1073, and 1173 K. It is found that the reduction rate decreased with decreasing temperature and increasing nitrogen content. The effect of nitrogen on the reduction rate is more profound than expected from the decreased hydrogen partial pressure alone. To aid the discussion, partially reduced pellets are studied using optical and scanning electron microscopy. It is found that the microstructure is strongly dependent on the temperature but independent of the nitrogen content.
- 18 February 2024
- Published by Wiley in Steel Research International
- Vol. 95 (5)
The Influence of Nitrogen on Hydrogen Reduction of Iron Ore Pellets
As the iron and steel industry now strives for a carbon neutral industry, hydrogen‐based direct reduction shaft furnace technology has become an alternative to the heavily fossil‐depending blast furnace route. Research questions related to the future full‐scale production have, therefore, become more interesting. Depending on the operational conditions, the H2 concentration and temperature will vary across the length of the reactor. This work studies the effect of nitrogen in a hydrogen‐reducing gas during the reduction of commercial iron ore pellets using thermogravimetric analysis. The reducing gas consisted of either pure hydrogen or a mixture of 90–70 vol% hydrogen and 10–30 vol% nitrogen at 773, 873, 973, 1073, and 1173 K. It is found that the reduction rate decreased with decreasing temperature and increasing nitrogen content. The effect of nitrogen on the reduction rate is more profound than expected from the decreased hydrogen partial pressure alone. To aid the discussion, partially reduced pellets are studied using optical and scanning electron microscopy. It is found that the microstructure is strongly dependent on the temperature but independent of the nitrogen content.
- Open Access
- 15 October 2023
- Published by Wiley in Steel Research International
- Vol. 95 (1)
The Melting Mechanism of Hydrogen Direct Reduced Iron in Liquid Slag
The heating and melting of hydrogen direct reduced iron (H‐DRI) in liquid slag is investigated experimentally at 1923 K. For the experiments, slags comprising the CaO‐SiO2‐MgO‐FeO‐Al2O3 system are first premelted at 1923 K in alumina crucibles. The molten slag bath is subsequently used to submerge samples of 7 g of H‐DRI with different degrees of reduction (90.4–99.8%). Following the submersion, the slag bath and the H‐DRI sample are quenched at different times (5–10 s). It is found that the liquid slag penetrates the porous network of the H‐DRI. The penetration is found to increase with lower reduction degrees. The reaction‐enhanced capillary action theory is proposed to explain the dependence. The reasoning is validated by a cold model consisting of a quartz capillary, water, and solid sugar. The slag penetration also enhances the heat transfer and the dephosphorization rate. The present findings can, therefore, aid in optimizing the hydrogen‐based steelmaking route.
- 15 October 2023
- Published by Wiley in Steel Research International
- Vol. 95 (1)
Open AccessThe Melting Mechanism of Hydrogen Direct Reduced Iron in Liquid Slag
The heating and melting of hydrogen direct reduced iron (H‐DRI) in liquid slag is investigated experimentally at 1923 K. For the experiments, slags comprising the CaO‐SiO2‐MgO‐FeO‐Al2O3 system are first premelted at 1923 K in alumina crucibles. The molten slag bath is subsequently used to submerge samples of 7 g of H‐DRI with different degrees of reduction (90.4–99.8%). Following the submersion, the slag bath and the H‐DRI sample are quenched at different times (5–10 s). It is found that the liquid slag penetrates the porous network of the H‐DRI. The penetration is found to increase with lower reduction degrees. The reaction‐enhanced capillary action theory is proposed to explain the dependence. The reasoning is validated by a cold model consisting of a quartz capillary, water, and solid sugar. The slag penetration also enhances the heat transfer and the dephosphorization rate. The present findings can, therefore, aid in optimizing the hydrogen‐based steelmaking route.
- 8 July 2023
- Published by Wiley in Steel Research International
- Vol. 94 (10)
Some Aspects of the Melting and Dephosphorization Mechanism of Hydrogen‐DRI
To meet the future environmental challenges, hydrogen direct reduced iron (H‐DRI) is expected to constitute the principal material for virgin steel production. For an efficient value chain, knowledge of the melting mechanism and dephosphorization mechanism of H‐DRI is needed. The in situ melting behavior, the melting mechanism, and the dephosphorization mechanism during heating of H‐DRI are investigated experimentally at 1773 and 1873 K. It is found that the melting rate of H‐DRI varies with the reduction degree (91–99.5%), increasing with decreasing reduction degree. An autogenous slag forms during heating and flows through the pores of the H‐DRI, thus increasing its effective thermal conductivity. The fraction of filled pores varies with reduction degree explaining the difference in melting rate. At this stage, the dissolution of apatite is initiated and completed upon melting of the metal phase. A gradual reversion of phosphorus from the autogenous slag to the liquid metal is observed after complete melting. The rate of reversion is discussed based on the properties of the H‐DRI, for example, reduction degree and carbon addition.
- 8 July 2023
- Published by Wiley in Steel Research International
- Vol. 94 (10)
Some Aspects of the Melting and Dephosphorization Mechanism of Hydrogen‐DRI
To meet the future environmental challenges, hydrogen direct reduced iron (H‐DRI) is expected to constitute the principal material for virgin steel production. For an efficient value chain, knowledge of the melting mechanism and dephosphorization mechanism of H‐DRI is needed. The in situ melting behavior, the melting mechanism, and the dephosphorization mechanism during heating of H‐DRI are investigated experimentally at 1773 and 1873 K. It is found that the melting rate of H‐DRI varies with the reduction degree (91–99.5%), increasing with decreasing reduction degree. An autogenous slag forms during heating and flows through the pores of the H‐DRI, thus increasing its effective thermal conductivity. The fraction of filled pores varies with reduction degree explaining the difference in melting rate. At this stage, the dissolution of apatite is initiated and completed upon melting of the metal phase. A gradual reversion of phosphorus from the autogenous slag to the liquid metal is observed after complete melting. The rate of reversion is discussed based on the properties of the H‐DRI, for example, reduction degree and carbon addition.