Type
Company
Locations
Richmond, Canada

Latest Publications

  • Interpretation of force profiles in mill-scale LC refining

    by Matthias Aigner, James Olson, Yu Sun, Peter Wild

    A set of piezo electric force sensors is implemented in a 52-inch mill-scale low consistency refiner to explore the effect of varying operating conditions on bar force profiles. The sensor replaces a short length of a stator bar and measures normal and shear forces applied during the passage of each rotor bar. In previous work with this type of force sensor a rotary encoder was used to investigate force profiles for individual bar passing events (BPE) on a 16-inch laboratory-scale refiner. In the work presented here, force profiles for individual BPEs are identified based on key features in the time domain force data. The individual bar force profiles are classified as single peak events which feature one peak corresponding to the fiber compression force and as dual peak events corresponding to fiber compression force and the corner force. The bar passing events are then analysed based on their mean force profiles and their dual peak ratio in the bar passing event. Findings are compared and validated by previous work on bar force profiles. It is shown that dual peak events which are considered to represent the corner force, are present through out the whole range of refining and increase with increased refining energy. This increases the understanding of the way corner force contributes to the refining process. Furthermore, it is found that different radial positions on the stator plate are subjected to different force profiles. This is thought to be due to the difference in tangential speed and a change in the fiber and floc material properties at different radial positions.


  • Corrosion of Thermowells in a Coastal Fluidized Bed Biomass Power Boiler

    by Joseph Kish, Douglas Singbeil, Ray Seguin

    A metallographic examination was conducted on a set of degraded alloy thermowells, which were installed in the fluidized bed of a coastal fluidized bed biomass (waste-wood) power boiler. Because of the importance of temperature measurement in the boiler control strategy, the plant wanted to understand the corrosion mechanism and choose longer-lived materials. The analytical results suggest that the corrosion was caused by contact with a molten chloride-containing salt. The relative corrosion resistance ranking order of Alloy 600 > Alloy 625 > Type 310H stainless steel > Type 446 stainless steel is consistent with the reported influence of nickel and chromium alloying on corrosion resistance in molten chloride-containing salts.

  • Corrosion of High Alloy Superheater Tubes in a Coastal Biomass Power Boiler

    by J. R. Kish, D. L. Singbeil, C. Reid, R. Seguin

    Metallurgical examinations were conducted on a set of damaged high alloy (Type 310H stainless steel and Alloy 625 weld overlay) superheater tubes removed from a coastal fluidized bed biomass power boiler, to better understand the degradation mode. Active oxidation (gas-solid reaction occurring underneath the chloride-containing fireside deposit) was found to be the mechanism responsible for the significant loss in tube wall thickness observed on damaged superheater tubes. There exists a complex, poorly-understood, synergy between the critical factors that affect active oxidation, primarily tube temperature and the supply of reactants in the flue gas, namely sodium chloride (NaCl), sulphur dioxide (SO2) and water vapour (H2O). Overall ranking in terms of increasing corrosion resistance to active oxidation follows the expected trend: T22 < SS310H < A625WO. Despite the favourable ranking, the Alloy 625 weld overlay can corrode by active oxidation at an appreciable rate [0.45 mm/yr (18 mpy)] under existing boiler operating conditions. A promising corrosion control strategy involves reducing the steam temperatures in the outlet tubes of the three superheater sections to below 500 °C.

  • Corrosion of Bed Nozzle Alloys in a Wood-Waste Fluidized Bed Power Boiler

    by J.R. Kish, D.L. Singbeil, P. Eng, O. Posein, R. Seguin

    A field test was conducted to identify a more corrosion-resistant material than Type 310H (UNS S31009) stainless steel, from which to fabricate bed nozzles for a fluidized bed power boiler that burns salt-laden wood-waste (hogged) fuel. Test nozzles fabricated from Type 310H stainless steel, Alloys 556 (UNS R30556), 59 (UNS N06059), HR160 (UNS N12160), and 625 (UNS N06625) were installed, subsequently removed, and examined as a function of time. Of the various alloys tested, Alloys 625 and HR160 had the best performance in terms of the amount of thickness loss, and the extent of internal damage exhibited. However, those alloys were still susceptible to corrosion by the fireside (fluidized bed) environment and, therefore, will require replacement over time. Despite the observed corrosion, those two alloys significantly extended the nozzle life beyond that of Type 310H stainless steel. Nozzle design was found to have a strong influence on the apparent corrosion resistance of Alloy 625 and, therefore, represents a promising preventive solution possibility. The reason for the marked improvement remains unresolved at this time.


  • Combustion and Emission Performance of a Hog Fuel Fluidized Bed Boiler With Addition of Tire Derived Fuel

    by Wenli Duo, Ibrahim Karidio, Larry Cross, Bob Ericksen

    Salt-laden hog fuel (wood waste) is burnt in a fluidized bed boiler converted from a traveling grate boiler to generate steam for a specialty paper mill. The converted boiler has a design capacity of 156t∕h of steam from hog and actual generation has varied from 76% to 107% of the design capacity. The conversion has resulted in more stable operation, more complete combustion, less ash production, reduced boiler maintenance, and lower fossil fuel consumption. Tire derived fuel (TDF) is used as a supplementary fuel. With an energy content of 31GJ∕t for TDF, as compared to 8GJ∕t for wet hog, addition of 2%–5% TDF by weight increased the bed temperature by an average of 55°C, stabilized and improved the combustion of low quality hog and high moisture content sludge. The impact of TDF addition was studied in detail. Stack emissions were tested and bottom and flyash samples were analyzed. Although TDF contains an average of 1.6% zinc and 9.2% steel wire by weight, addition of TDF did not affect total particulate emissions from the boiler. SO2 emissions were increased due to the high sulfur content of TDF (1.4%), while NOx emissions were reduced. A good correlation was obtained from the test results, showing that the addition of TDF resulted in a reduction in both the total formation and the stack emissions of dioxins and furans.