Lam Research (United States)

Types
Company, FunderLocations
Fremont, United StatesRelationships
Latest Publications
- Open Access
- 5 November 2026
- Published by MDPI AG in Nanomaterials
- Vol. 16 (21) , 1424
Cu–Cu Grain Intermixing Quantification for Hybrid Bonding Applications
Cu–Cu hybrid bonding at reduced thermal budgets depends critically on reliable grain intermixing across the bonding interface. Yet interfacial evolution is still predominantly assessed qualitatively, precluding objective comparison across copper microstructures and process conditions. Here, we introduce Bond IQ, an automated image-based metrology framework that converts registered cross-sectional FIB-SEM datasets into physically interpretable descriptors using classical computer-vision methods. We apply the framework to five blanket chip-level pairings spanning three engineered copper microstructures: coarse-grain (CG), fine-grain locked (FG-L), and fine-grain thermally dynamic (FG-TD) Cu, thermocompression bonded at 210 °C for 2 h. Three coupled but distinct metrics are extracted: Bridged Interface Fraction (BIF), Interface Void Loading (IVL), and normalized Grain Penetration Depth (GPD). The symmetric CG/CG interface exhibited the weakest evolution, combining high IVL (5.4 nm) with low BIF (6.1%) and low GPD (0.20). By contrast, CG/FG-TD achieved the highest BIF (54.5%) at low IVL (0.6 nm), signifying broad but comparatively shallow bridging, whereas CG/FG-L reached the highest GPD (0.89) at moderate BIF (32.7%), indicating localized yet deeper directional grain advancement. Among symmetric fine-grained interfaces, FG-L/FG-L displayed the lowest IVL (0.5 nm), underscoring the role of fine-grain stability in void suppression. Collectively, these results demonstrate that interface bridging, void elimination, and penetration depth are governed by distinct but interrelated contributions of grain-size contrast and microstructural stability. By reducing subjective interfacial assessment to quantitative, mechanistically interpretable descriptors, Bond IQ offers a scalable route to screen copper microstructures and bonding conditions, and it can be extended to other metal–metal interfaces where microstructural evolution governs low-temperature bonding reliability.
- 5 November 2026
- Published by MDPI AG in Nanomaterials
- Vol. 16 (21) , 1424
Open AccessCu–Cu Grain Intermixing Quantification for Hybrid Bonding Applications
Cu–Cu hybrid bonding at reduced thermal budgets depends critically on reliable grain intermixing across the bonding interface. Yet interfacial evolution is still predominantly assessed qualitatively, precluding objective comparison across copper microstructures and process conditions. Here, we introduce Bond IQ, an automated image-based metrology framework that converts registered cross-sectional FIB-SEM datasets into physically interpretable descriptors using classical computer-vision methods. We apply the framework to five blanket chip-level pairings spanning three engineered copper microstructures: coarse-grain (CG), fine-grain locked (FG-L), and fine-grain thermally dynamic (FG-TD) Cu, thermocompression bonded at 210 °C for 2 h. Three coupled but distinct metrics are extracted: Bridged Interface Fraction (BIF), Interface Void Loading (IVL), and normalized Grain Penetration Depth (GPD). The symmetric CG/CG interface exhibited the weakest evolution, combining high IVL (5.4 nm) with low BIF (6.1%) and low GPD (0.20). By contrast, CG/FG-TD achieved the highest BIF (54.5%) at low IVL (0.6 nm), signifying broad but comparatively shallow bridging, whereas CG/FG-L reached the highest GPD (0.89) at moderate BIF (32.7%), indicating localized yet deeper directional grain advancement. Among symmetric fine-grained interfaces, FG-L/FG-L displayed the lowest IVL (0.5 nm), underscoring the role of fine-grain stability in void suppression. Collectively, these results demonstrate that interface bridging, void elimination, and penetration depth are governed by distinct but interrelated contributions of grain-size contrast and microstructural stability. By reducing subjective interfacial assessment to quantitative, mechanistically interpretable descriptors, Bond IQ offers a scalable route to screen copper microstructures and bonding conditions, and it can be extended to other metal–metal interfaces where microstructural evolution governs low-temperature bonding reliability.
- 16 October 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (6)
Polyurea films deposited by molecular layer deposition for surface and sidewall passivation during HF plasma etching of high-aspect-ratio structures
Molecular layer deposition (MLD) was used to deposit polyurea films using toluene diisocyanate and ethylenediamine as precursors. Polyurea was deposited on SiO2 and SiNx blanket films and exposed to an HF plasma to evaluate plasma-surface interactions. The surface composition was monitored using in situ infrared spectroscopy. During the initial stages of HF plasma exposure, polyurea was sacrificially etched, while etching of the underlying SiO2 or SiNx films was negligible. Once polyurea was completely consumed by reactions with plasma species, the underlying SiO2 or SiNx films were etched at their baseline etch rates. Despite the high porosity of the MLD films, the presence of polyurea prevented etching of the underlying material, showing that polyurea efficiently consumed the reactive plasma species. Fluorination of polyurea was observed prior to its removal, suggesting that polyurea was removed as hydrofluorocarbons during HF plasma etching. Finally, polyurea was deposited on ∼65:1 aspect-ratio holes in SiO2-SiNx stacks and then exposed to an etching plasma to evaluate the sidewall passivation. We show that polyurea was deposited throughout the entire hole using the saturation doses for a flat surface, although the thickness on the sidewalls was lower than the planar surface. After MLD, in the second etch step, the polyurea film preserved the critical dimension throughout the high-aspect-ratio feature.
- 16 October 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (6)
Polyurea films deposited by molecular layer deposition for surface and sidewall passivation during HF plasma etching of high-aspect-ratio structures
Molecular layer deposition (MLD) was used to deposit polyurea films using toluene diisocyanate and ethylenediamine as precursors. Polyurea was deposited on SiO2 and SiNx blanket films and exposed to an HF plasma to evaluate plasma-surface interactions. The surface composition was monitored using in situ infrared spectroscopy. During the initial stages of HF plasma exposure, polyurea was sacrificially etched, while etching of the underlying SiO2 or SiNx films was negligible. Once polyurea was completely consumed by reactions with plasma species, the underlying SiO2 or SiNx films were etched at their baseline etch rates. Despite the high porosity of the MLD films, the presence of polyurea prevented etching of the underlying material, showing that polyurea efficiently consumed the reactive plasma species. Fluorination of polyurea was observed prior to its removal, suggesting that polyurea was removed as hydrofluorocarbons during HF plasma etching. Finally, polyurea was deposited on ∼65:1 aspect-ratio holes in SiO2-SiNx stacks and then exposed to an etching plasma to evaluate the sidewall passivation. We show that polyurea was deposited throughout the entire hole using the saturation doses for a flat surface, although the thickness on the sidewalls was lower than the planar surface. After MLD, in the second etch step, the polyurea film preserved the critical dimension throughout the high-aspect-ratio feature.
- Open Access
- 4 August 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1) , 24012
A class-wise quantum relational calibration network for brain tumor diagnosis
- 4 August 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1) , 24012
Open AccessA class-wise quantum relational calibration network for brain tumor diagnosis
- 29 July 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (5)
Detection of silicon-containing etch products during SiN x etching in a hydrogen fluoride plasma using quadrupole mass spectrometry
We have designed and fabricated a two-stage differentially pumped setup for a quadrupole mass spectrometer to identify stable etch products generated during etching of SiNx in an HF plasma under an applied bias voltage of −240 V to the substrate. In this setup, the etch products can be directly collected into a sampling cone with a 1 mm aperture at a distance of ∼3 mm from the sample surface, which is shorter than the mean free path in the HF plasma at 10 mTorr. We show that SiF4 is the primary Si-containing etch product. It is unlikely that SiF2 is an etch product during SiNx etching at the conditions employed in this study. We also detected small fractions of SiH2F2 and SiHF3 released from the SiNx surface during etching. Since the electron impact ionization cross sections for SiH2F2 and SiHF3 are not available in the literature, we could not estimate their relative abundance compared to SiF4. We were unable to conclusively detect NH3 as the primary N-containing etch product due to background H2O in the chamber, which has a cracking pattern that overlaps with NH3 at mass-to-charge ratios of 16 and 17.
- 29 July 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (5)
Detection of silicon-containing etch products during SiN x etching in a hydrogen fluoride plasma using quadrupole mass spectrometry
We have designed and fabricated a two-stage differentially pumped setup for a quadrupole mass spectrometer to identify stable etch products generated during etching of SiNx in an HF plasma under an applied bias voltage of −240 V to the substrate. In this setup, the etch products can be directly collected into a sampling cone with a 1 mm aperture at a distance of ∼3 mm from the sample surface, which is shorter than the mean free path in the HF plasma at 10 mTorr. We show that SiF4 is the primary Si-containing etch product. It is unlikely that SiF2 is an etch product during SiNx etching at the conditions employed in this study. We also detected small fractions of SiH2F2 and SiHF3 released from the SiNx surface during etching. Since the electron impact ionization cross sections for SiH2F2 and SiHF3 are not available in the literature, we could not estimate their relative abundance compared to SiF4. We were unable to conclusively detect NH3 as the primary N-containing etch product due to background H2O in the chamber, which has a cracking pattern that overlaps with NH3 at mass-to-charge ratios of 16 and 17.
- 11 June 2026
- Published by AIP Publishing in The Journal of Chemical Physics
- Vol. 164 (22)
Aggregation dynamics of molybdenum-based precursors in rarefied carrier gas mixtures under sub-nucleation conditions
Precise control of fluid flow and chemical reactions under low-pressure conditions is critical for next-generation semiconductor manufacturing, where vapor-phase transport of precursor molecules governs the quality and reliability of thin-film deposition. Among emerging alternatives to conventional metals, transition metal-based compounds are gaining attention due to their favorable thermal and structural properties. In particular, molybdenum oxychloride molecules are being explored for their stability and compatibility with high-temperature processes. However, the behavior of these precursor gases in rarefied environments remains poorly understood, especially concerning spontaneous aggregation and its impact on uniformity and defect formation. This study investigates the aggregation dynamics of gas-phase molybdenum oxychloride species using atomistic simulations under varying thermodynamic conditions relevant to semiconductor processing. We explore the influence of temperature, pressure, molecular ratio, and initial density on the formation and dissociation of molecular clusters. To quantify aggregation behavior, we track the evolution of cluster size distributions and assess the likelihood and timescales of large-cluster formation. The analysis reveals that aggregation is favored at lower temperatures and higher densities, while larger clusters tend to dissociate rapidly under thermodynamically unfavorable conditions. The results indicate no persistent critical cluster size, but transient aggregation events may influence deposition outcomes. These findings provide new insights into the gas-phase behavior of transition metal precursors under low-pressure conditions and offer guidance for optimizing process parameters in vapor-phase fabrication techniques.
- 11 June 2026
- Published by AIP Publishing in The Journal of Chemical Physics
- Vol. 164 (22)
Aggregation dynamics of molybdenum-based precursors in rarefied carrier gas mixtures under sub-nucleation conditions
Precise control of fluid flow and chemical reactions under low-pressure conditions is critical for next-generation semiconductor manufacturing, where vapor-phase transport of precursor molecules governs the quality and reliability of thin-film deposition. Among emerging alternatives to conventional metals, transition metal-based compounds are gaining attention due to their favorable thermal and structural properties. In particular, molybdenum oxychloride molecules are being explored for their stability and compatibility with high-temperature processes. However, the behavior of these precursor gases in rarefied environments remains poorly understood, especially concerning spontaneous aggregation and its impact on uniformity and defect formation. This study investigates the aggregation dynamics of gas-phase molybdenum oxychloride species using atomistic simulations under varying thermodynamic conditions relevant to semiconductor processing. We explore the influence of temperature, pressure, molecular ratio, and initial density on the formation and dissociation of molecular clusters. To quantify aggregation behavior, we track the evolution of cluster size distributions and assess the likelihood and timescales of large-cluster formation. The analysis reveals that aggregation is favored at lower temperatures and higher densities, while larger clusters tend to dissociate rapidly under thermodynamically unfavorable conditions. The results indicate no persistent critical cluster size, but transient aggregation events may influence deposition outcomes. These findings provide new insights into the gas-phase behavior of transition metal precursors under low-pressure conditions and offer guidance for optimizing process parameters in vapor-phase fabrication techniques.
- 8 June 2026
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 65 (11) , 11SP13
Enabling 3D NAND bit cost scaling with merged etches
High aspect ratio (AR) etches play a critical role in defining 3D NAND memory devices. As 3D NAND devices scale predominantly in the z direction, AR dependent etching becomes a major limiting factor in cost scaling. In this work, deposition and etch process development understanding combined with integration and feature scale modeling is applied to cost-effectively merge etches with minimal downstream device impact. Merged SiO 2 /Si 3 N 4 (ONON) memory channel and SiO 2 interlayer dielectric (ILD) contact etch was achieved by doping the ILD to enable SiO x contact etch depth and profile control while maintaining the same memory channel cryo etch process. Furthermore, co-doping the SiO x ILD layer shows high etch rates while enabling profile control through etch byproduct redeposition management. In addition, co-doping minimizes downstream integration impact and device properties based on hot phosphoric wet etch rate and blanket oxide leakage current measurements, respectively.
- 8 June 2026
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 65 (11) , 11SP13
Enabling 3D NAND bit cost scaling with merged etches
High aspect ratio (AR) etches play a critical role in defining 3D NAND memory devices. As 3D NAND devices scale predominantly in the z direction, AR dependent etching becomes a major limiting factor in cost scaling. In this work, deposition and etch process development understanding combined with integration and feature scale modeling is applied to cost-effectively merge etches with minimal downstream device impact. Merged SiO 2 /Si 3 N 4 (ONON) memory channel and SiO 2 interlayer dielectric (ILD) contact etch was achieved by doping the ILD to enable SiO x contact etch depth and profile control while maintaining the same memory channel cryo etch process. Furthermore, co-doping the SiO x ILD layer shows high etch rates while enabling profile control through etch byproduct redeposition management. In addition, co-doping minimizes downstream integration impact and device properties based on hot phosphoric wet etch rate and blanket oxide leakage current measurements, respectively.
- 9 April 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (3)
Effect of gas additives on reaction barriers in cryo etching of silicon oxide and nitride
Vertical scaling of 3D NAND devices calls for higher SiO2 and SiN etching rates and meaningful reduction of aspect ratio dependent etching. Recently, evolutionary improvements of the fluorocarbon gas process have been replaced by novel so-called cryo etching processes using HF as the main etch gas. In this paper, we report computational results for the activation Gibbs free energies ΔG‡ for the reaction of HF and various additive gases with SiO2 and SiN. The results are compared with available experimental trends. We find that the dipole moment of the additive gas is an indicator of its catalytic effect.
- 9 April 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (3)
Effect of gas additives on reaction barriers in cryo etching of silicon oxide and nitride
Vertical scaling of 3D NAND devices calls for higher SiO2 and SiN etching rates and meaningful reduction of aspect ratio dependent etching. Recently, evolutionary improvements of the fluorocarbon gas process have been replaced by novel so-called cryo etching processes using HF as the main etch gas. In this paper, we report computational results for the activation Gibbs free energies ΔG‡ for the reaction of HF and various additive gases with SiO2 and SiN. The results are compared with available experimental trends. We find that the dipole moment of the additive gas is an indicator of its catalytic effect.
- 1 April 2026
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanopatterning, Materials, and Metrology
- Vol. 25 (02) , 1-18
Physics-based dry metal–oxide–resist simulations
BackgroundMetal oxide resists (MORs) have demonstrated exceptional performance in high-resolution extreme ultraviolet (EUV) lithography, primarily due to their high EUV absorptivity and minimal blur radius. Innovative solutions involving dry deposition and dry development processes, tailored for MOR, significantly enhance resist compositional control and mitigate pattern collapse. However, photon shot noise and process variations continue to pose substantial challenges in meeting key performance indicators for defectivity and line-edge roughness.AimTo address these stringent requirements, a comprehensive understanding of the multistep MOR patterning process flow and the dry processing mechanisms is essential.ApproachWe introduce a bottom-up modeling approach for MOR, enabling the construction of a physically grounded, module-based digital twin for the photolithography patterning process flow. This platform captures the effects of various process steps on the deposited MOR system, including photon absorption derived from aerial images, secondary electron-induced blurring, post-exposure bake cleavage and cross-linking reactions, progressive dry development characteristics, and scanning electron microscope-based postprocessing insights. Each module is built upon key mechanistic insights and is mathematically formulated using probabilistic algorithms. Model parameters are directly extracted from meticulously designed blanket and checkerboard exposure experiments, ensuring physical relevance without relying on empirical fitting to patterning data.ResultsThe end-to-end model demonstrates strong predictive capability for dose and roughness metrics, including frequency decomposition, and shows good agreement with experimental wafer benchmark data.ConclusionsThe validated model brings mechanistic and physical insights for resists and processes and may help reduce the complexity in MOR optical proximity correction applications.
- 1 April 2026
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanopatterning, Materials, and Metrology
- Vol. 25 (02) , 1-18
Physics-based dry metal–oxide–resist simulations
BackgroundMetal oxide resists (MORs) have demonstrated exceptional performance in high-resolution extreme ultraviolet (EUV) lithography, primarily due to their high EUV absorptivity and minimal blur radius. Innovative solutions involving dry deposition and dry development processes, tailored for MOR, significantly enhance resist compositional control and mitigate pattern collapse. However, photon shot noise and process variations continue to pose substantial challenges in meeting key performance indicators for defectivity and line-edge roughness.AimTo address these stringent requirements, a comprehensive understanding of the multistep MOR patterning process flow and the dry processing mechanisms is essential.ApproachWe introduce a bottom-up modeling approach for MOR, enabling the construction of a physically grounded, module-based digital twin for the photolithography patterning process flow. This platform captures the effects of various process steps on the deposited MOR system, including photon absorption derived from aerial images, secondary electron-induced blurring, post-exposure bake cleavage and cross-linking reactions, progressive dry development characteristics, and scanning electron microscope-based postprocessing insights. Each module is built upon key mechanistic insights and is mathematically formulated using probabilistic algorithms. Model parameters are directly extracted from meticulously designed blanket and checkerboard exposure experiments, ensuring physical relevance without relying on empirical fitting to patterning data.ResultsThe end-to-end model demonstrates strong predictive capability for dose and roughness metrics, including frequency decomposition, and shows good agreement with experimental wafer benchmark data.ConclusionsThe validated model brings mechanistic and physical insights for resists and processes and may help reduce the complexity in MOR optical proximity correction applications.
- 19 March 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (3)
Plasma pretreatment to increase benzaldehyde attachment to the SiN x surface before atomic layer etching
During atomic layer etching, the selective surface prefunctionalization of plasma-deposited SiNx over SiO2 with benzaldehyde has been shown to effectively retard the etching of SiNx by accelerating the formation of an etch-stop layer: this, in turn, enhances the etch selectivity for SiO2 over SiNx. The uptake of benzaldehyde is lower if the SiNx surface has been pre-exposed to the atmosphere or an etching plasma. We demonstrate a H2/Ar plasma pretreatment strategy to improve the uptake of benzaldehyde on a pre-etched SiNx surface. Using in situ attenuated total reflection Fourier transform infrared spectroscopy, we first show that surface treatment of as-deposited SiNx with Ar or H2 plasmas reduces the surface reactivity to benzaldehyde most likely due to a loss of surface —NHx (x = 1, 2) groups. In contrast, surface pretreatment of the as-deposited SiNx surface with an Ar-diluted H2 plasma largely retains the surface reactivity to benzaldehyde under optimal conditions. We then translate this H2/Ar plasma pretreatment step to practical applications. We first remove a thin surface layer of SiNx with one ALE cycle, which consists of a C4F6/Ar plasma modification step followed by an Ar plasma activation step: this step mimics a SiNx surface that has been exposed to an etching plasma, which leaves a surface CFx residue. Using in situ infrared spectroscopy, we show that surface pretreatment with a H2/Ar plasma under these optimal conditions can partially remove the CFx residue on the SiNx surface. We further show that H2/Ar plasma treatment can restore benzaldehyde uptake to ∼80% of that on an as-deposited surface. Finally, we show that after treating the pre-etched SiO2 surface with an H2/Ar plasma, the SiO2 surface reactivity with benzaldehyde remains low, leading to an increase in the aldehyde attachment selectivity to pre-etched SiNx over SiO2 surfaces by ∼50%, and a recovery of ∼80% of that on as-deposited surfaces.
- 19 March 2026
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 44 (3)
Plasma pretreatment to increase benzaldehyde attachment to the SiN x surface before atomic layer etching
During atomic layer etching, the selective surface prefunctionalization of plasma-deposited SiNx over SiO2 with benzaldehyde has been shown to effectively retard the etching of SiNx by accelerating the formation of an etch-stop layer: this, in turn, enhances the etch selectivity for SiO2 over SiNx. The uptake of benzaldehyde is lower if the SiNx surface has been pre-exposed to the atmosphere or an etching plasma. We demonstrate a H2/Ar plasma pretreatment strategy to improve the uptake of benzaldehyde on a pre-etched SiNx surface. Using in situ attenuated total reflection Fourier transform infrared spectroscopy, we first show that surface treatment of as-deposited SiNx with Ar or H2 plasmas reduces the surface reactivity to benzaldehyde most likely due to a loss of surface —NHx (x = 1, 2) groups. In contrast, surface pretreatment of the as-deposited SiNx surface with an Ar-diluted H2 plasma largely retains the surface reactivity to benzaldehyde under optimal conditions. We then translate this H2/Ar plasma pretreatment step to practical applications. We first remove a thin surface layer of SiNx with one ALE cycle, which consists of a C4F6/Ar plasma modification step followed by an Ar plasma activation step: this step mimics a SiNx surface that has been exposed to an etching plasma, which leaves a surface CFx residue. Using in situ infrared spectroscopy, we show that surface pretreatment with a H2/Ar plasma under these optimal conditions can partially remove the CFx residue on the SiNx surface. We further show that H2/Ar plasma treatment can restore benzaldehyde uptake to ∼80% of that on an as-deposited surface. Finally, we show that after treating the pre-etched SiO2 surface with an H2/Ar plasma, the SiO2 surface reactivity with benzaldehyde remains low, leading to an increase in the aldehyde attachment selectivity to pre-etched SiNx over SiO2 surfaces by ∼50%, and a recovery of ∼80% of that on as-deposited surfaces.
- 1 March 2026
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanopatterning, Materials, and Metrology
- Vol. 25 (02) , 1-14
Dry resist process development toward depth of focus improvement in high NA EUV lithography
High numerical aperture (NA) extreme ultraviolet lithography enables device scaling and improves resolution. However, it also brings the challenge of reduced depth of focus (DOF) due to the optics with increased NA. New resist innovations are being targeted toward addressing this patterning challenge. We present how dry deposited and dry developed resists can be used to improve the focus window. Modulating the resist composition in the vertical direction and co-optimizing the process conditions have shown benefits in improving patterning metrics, including DOF. Test vehicles based on bright field pitch 32 nm hexagonal contact hole with 0.33 NA and pitch 18 nm line/space imaging with 0.55 NA are discussed to showcase the patterning improvements.
- 1 March 2026
- Published by SPIE-Intl Soc Optical Eng in Journal of Micro/Nanopatterning, Materials, and Metrology
- Vol. 25 (02) , 1-14
Dry resist process development toward depth of focus improvement in high NA EUV lithography
High numerical aperture (NA) extreme ultraviolet lithography enables device scaling and improves resolution. However, it also brings the challenge of reduced depth of focus (DOF) due to the optics with increased NA. New resist innovations are being targeted toward addressing this patterning challenge. We present how dry deposited and dry developed resists can be used to improve the focus window. Modulating the resist composition in the vertical direction and co-optimizing the process conditions have shown benefits in improving patterning metrics, including DOF. Test vehicles based on bright field pitch 32 nm hexagonal contact hole with 0.33 NA and pitch 18 nm line/space imaging with 0.55 NA are discussed to showcase the patterning improvements.