  • Open Access

    Investigation of CMT welding for end-surfacing applications in bimetallic mechanical composite pipes

    by Xianqiao Fu, Bin Han, Xiao Jun, Liying Li, Xueda Li

    Pipe end surfacing represents a standard welding technique employed in the fabrication of bimetallic mechanical composite pipes. This study investigates the application of cold metal transfer (CMT) welding technology for pipe end surfacing of bimetallic composite pipes. The effect of CMT welding parameters, including welding current, welding speed, weave width, weave frequency, and dwell time, on the weld width, weld height, heat-affected zone (HAZ) width, and fusion ratio was analysed. The results show that the main factors affecting welding forming are welding current, welding speed and weave width, which basically determine both the width and height of the weld. The orthogonal test shows that the more suitable welding parameters are 120 A welding current, 3.28 mm/s welding speed, 5 mm weave width, 3 Hz weave frequency, and 0.05 s dwell time on both sides. To improve welding efficiency and ensure arc stability, the adjusted surfacing welding parameters are 120 A welding current, 5.12 mm/s welding speed, 5 mm weave width, 2 Hz weave frequency, and 0.05 s dwell time on both sides. The lap surfacing weld was well formed.

  • Open Access

    Microstructure and Wear Resistance of Si-TC4 Composite Coatings by High-Speed Wire-Powder Laser Cladding

    by Boxuan Men, Shenzhen Sun, Chunyang Hu, Qi Zhang, Bin Han

    The hardness and wear resistance of the surface of TC4 titanium alloy, which is widely used in aerospace and other fields, need to be improved urgently. Considering the economy, environmental friendliness, and high efficiency, Si-reinforced Ti-based composite coatings were deposited on the TC4 surface by the high-speed wire-powder laser cladding method, which combines the paraxial feeding of TC4 wires with the coaxial feeding of Si powders. The microstructures and wear resistance of the coatings were analyzed using X-ray diffraction (XRD), scanning electron microscopy (SEM), Vickers hardness tester, and friction and wear tester. The results indicate that the primary composition of the coating consisted of α-Ti and Ti5Si3. The microstructure of the coating underwent a notable transformation process from dendritic to petal, bar, and block shapes as the powder feeding speed increased. The hardness of the composite coatings increased with the increasing Si powder feeding rate, and the average hardness of the composite coating was 909HV0.2 when the feeding rate reached 13.53 g/min. The enhancement of the microhardness of the coatings can be attributed primarily to the reinforcing effect of the second phase generated by Ti5Si3 in various forms within the coatings. As the powder feeding speed increased, the wear resistance initially improved before deteriorating. The optimal wear resistance of the coating was achieved at a powder feeding rate of 6.88 g/min (wear loss of 2.55 mg and friction coefficient of 0.12). The main wear mechanism for coatings was abrasive wear.


  • Open Access

    Study on the Effect of Welding Sequence on Residual Stress in Post Internal-Welding Joint of Bimetal Composite Pipe

    by Zhenhua Gao, Bin Han, Shengyuan Niu, Liying Li

    With the rapid development of industry and globalization, the demand and strategic importance of oil and natural gas have become increasingly significant, leading to energy extraction in more complex corrosive environments [1, 2]. Bimetallic composite pipes, which offer strength and corrosion resistance, exhibit promising potential. For the welding of bimetallic composite plates, it is optimal to follow the welding sequence of the base layer, transition layer, and inner layer [3, 4]. For the welding of bimetal composite pipes, due to the diameter limit, the inner layer is usually welded first, followed by the transition layer, and the base layer finally, which is referred to as the single-side welding process. There is a significant martensitic layer in the fusion zone when using less costly mixed welding material in the single-side welding process, resulting in cracks in the bending specimen and a deterioration in mechanical properties. With the application and miniaturization of internal welding machines, the welding of bimetal composite pipes can be accomplished by first welding the base layer, followed by using an internal welding machine to weld the inner layer, which is known as the post internal-welding process proposed by Han and Li [5, 6]. Studies have shown that the properties of the post internal-welding joints meet the required standards, especially the bending properties. The post internal-welding process diversifies the welding sequence, significantly influencing the residual stress in welding [7]. Therefore, it is necessary to explore the effect of the welding sequence on residual stress. The bimetal composite pipe of L415/316L with specifications of φ355×(11+2) is used in this work, where the base material is L415 (thickness of 11 mm) and the inner layer is 316L (thickness of 2 mm). The welding groove is an asymmetric double V-groove, divided into 7 weld layers. The weld beads with names 6 and 7 are formed in the internal weld layer using an internal welding machine. By adjusting the internal welding sequence throughout the entire welding process, the welding sequence is categorized into four types. Fig. 1 (a) shows the groove and sequence division. The 1:1 scale model with actual dimensions is built by a combination of 2D and 3D models (Fig. 1 (b)). Transition meshes are used to balance computational efficiency and accuracy. To ensure the accuracy of the calculation, the length of the single side is 1000 mm, and the minimum grid is 0.3 mm×0.3 mm. The mesh size gradually increases in regions away from the welding joint to improve computational efficiency [8]. As shown in Figure 2(a), the heat source loading of the backing weld layer in the 3D model is primarily used for determining the welding heat source parameters. The thermal cycle of the entire welding process is extracted, with point 1 (L415 material) and point 2 (316L material), which are adjacent positions. During the internal welding process, the thermal cycle of the two materials differs significantly, because their thermophysical parameters are not the same. This difference in the thermal process also leads to variations in residual stress. The evolution of Von Mises stresses during the welding process is shown in Fig. 2(b). The high-stress region begins to appear during internal welding or filler welding. With the change in the welding sequence, the high-stress region transfers between the backing weld layer and the filler layer, and the stress in the backing weld layer undergoes a process of increase and decrease. Reasonable adjustment of the welding sequence can transfer the high-stress region in the backing weld layer to the filler layer, reducing the stresses in the root weld layer and the inner surface. The residual stress distribution on the inner and outer surfaces under different welding sequences is shown in Fig. 3. The stress distribution of four sequences is approximately as same on the outer surface. However, the difference is mainly reflected in the stress levels between S1 and the other three sequences. For the stresses of the inner surface, the stresses of the four sequences are different, which is mainly reflected in the hoop stresses and Von Mises stresses. The welding sequence mainly affects the level of residual stresses but has little effect on the distribution. Changing the welding sequence, the residual stresses on the inner surface change more significantly than that of the outer surface. The welding between the inner welding layer and the backing welding layer involves dissimilar metals, leading to the brittle hard layer of martensitic inevitably [9]. The combination of this structure and stress causes cracks. The S4 welding is the best sequence and the residual stresses in weak positions are effectively reduced. Through the reasonable adjustment of the welding sequence, the residual stress in weak positions such as the backing welding layer and the inner welding layer can be reduced, thereby improving the safety of the joints. This provides theoretical guidance for optimizing the welding process of bimetal composite pipes. The mechanical composite pipe needs to consider the effect of pipe end overlay welding on residual stress. Therefore, the welding sequence planning for mechanical composite pipes and metallurgical composite pipes in the post internal-welding process needs to be considered separately.


  • Open Access

    Investigation of the Microstructure and Properties of CoCrFeNiMo High-Entropy Alloy Coating Prepared through High-Speed Laser Cladding

    by Qi Zhang, Meiyan Li, Qin Wang, Fuhao Qi, Mengkai Kong, Bin Han

    High-speed laser cladding was introduced to prepare a CoCrFeNiMo high-entropy alloy (HEA) coating. The microstructure, composition distribution, micromechanical properties, and corrosion resistance of the CoCrFeNiMo coating were characterized. As a result, the coating exhibited a dual FCC- and BCC-phase structure, and the grain size of the coating prepared through high-speed laser cladding was only 2~5 μm. The upper and lower parts of the coating were composed of equiaxed cellular crystals and slender columnar crystals, respectively. The interdendritic structure was a Mo-rich phase that was distributed in a network-like pattern. The nanoindentation tests revealed that the interdendritic BCC phase had high hardness and an elastic modulus as well as excellent resistance to deformation, while the intradendritic FCC phase possessed superior crack propagation resistance. In addition, the two phases could generate cooperative elastic deformation during the elastic deformation stage. The electrochemical performance of the coating was tested in 3.5 wt% NaCl solution, and the corrosion potential Ecorr and corrosion current density Icorr of the coating were −0.362 V and 3.69 × 10−6 A/cm2, respectively. The high-speed laser cladding CoCrFeNiMo HEA coating had excellent corrosion resistance thanks to the presence of the easily passivating element Mo and grain refinement.


  • Open Access

    Microstructure and Wear Property of Graphene Nanoplatelets Reinforced Nickel-Based Composite Coating by Laser Cladding

    by Bin Han, Ge Li, Zubin Chen, Guoguang Zhang

    Nickel-based composite coatings containing graphene nanoplatelets (GNPs) were prepared on Q235 steel using laser cladding. In order to retain the multilayer GNPs in the composite coatings after laser cladding, NiGNPs were prepared by electroless nickel plating on GNPs as the additive phase. All the coatings contain γ-(Ni, Fe), Cr23C6, Cr7C3, Fe3C and WC phases, and multilayer GNPs were retained successfully in the composite coatings. With the addition of GNPs, the microstructure of the coatings was obviously refined and the content of Cr-C compounds were increased along with its changed morphology. The mean microhardness of the Ni-based composite coatings containing GNPs was significantly improved compared to that of Ni45 coating, and the maximum microhardness was 745.06 when 20% NiGNPs was added. The results indicated that, due to the refinement and lubricating effects of GNPs, the friction coefficients of composite coatings were reduced and the wear resistance was improved compared to Ni45 coating.


  • Open Access

    Influence of ICCGHAZ on the Low-Temperature Toughness in HAZ of Heavy-Wall X80 Pipeline Steel

    by Chao Fu, Xueda Li, Haichuan Li, Tao Han, Bin Han, Yong Wang

    Low-temperature embrittlement in the heat-affected zone (HAZ) of heavy-wall X80 weld joints is a primary challenge for arctic oil & gas exploitation. In this paper, the influence of intercritically reheated coarse-grained HAZ (ICCGHAZ) on the low-temperature toughness of the weld joint in a 22 mm thick X80 spiral submerged arc welded pipe was studied through instrumented Charpy V-notch impact test at −80~20 °C and corresponding fracture surface characterization. The results indicated that the influence of ICCGHAZ on the overall toughness of the weld joint is related to temperature. At temperatures below −45 °C, individual and tiny martensite-austenite (MA) constituent debonding can trigger cleavage fracture–which was proved to be nucleation-controlled–and the probability of embrittlement of the ICCGHAZ increases. At temperatures higher than −45 °C, only relatively large or closely distributed MA constituent in ICCGHAZ satisfies the conditions to trigger propagation-controlled cleavage fractures, and the influence of ICCGHAZ on the overall toughness is not remarkable.