Shiman Li
Research Subjects
Shiman Li has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
Gangcheng Jiao
4 shared publicationsYijun Zhang
3 shared publicationsYugang Zeng
3 shared publicationsYunsheng Qian
3 shared publicationsFeng Shi
2 shared publicationsHongchang Cheng
2 shared publications
Latest Publications
- 15 May 2025
- Published by Elsevier in Surfaces and Interfaces
- Vol. 68
Optimizing surface chemical etching process to improve photoemission from AlGaAs photocathodes
- 15 May 2025
- Published by Elsevier in Surfaces and Interfaces
- Vol. 68
Optimizing surface chemical etching process to improve photoemission from AlGaAs photocathodes
- Open Access
- 19 August 2024
- Published by Elsevier in SSRN Electronic Journal
Optimizing Surface Chemical Etching Process to Improve Photoemission from Algaas Photocathodes
Negative-electron-affinity AlGaAs photocathodes offer applications in underwater detection and green-laser driven electron sources due to their adjustable response threshold, long operating lifetime and fast response time. However, the difficulty of removing surface Al oxide is a key factor limiting the improvement of photoemission performance of AlGaAs photocathodes. To prevent oxidation of AlGaAs from exposure to air, a thin GaAs cap layer is commonly employed as the protective layer. Removing the GaAs cap layer and obtaining a clean and smooth AlGaAs surface are prerequisites for achieving high photoemission performance. Three sets of two-step chemical etching experiments were designed to remove the GaAs cap layer and obtain an AlGaAs emission surface favorable for Cs-O activation. By surface elemental analysis and surface topography test, it was found that the sample treated by the two-step chemical etching with the C6H8O7: H2O2 mixed solution and diluted HCl solution exhibited the lowest surface oxidation degree and roughness, and possessed the highest quantum efficiency over the entire waveband after activation. In additional, by fitting the experimental quantum efficiency curves, it is confirmed that the lower surface oxidation degree and roughness can effectively optimize surface barrier and enhance the photoelectron escape probability, resulting in the higher quantum efficiency.
- 19 August 2024
- Published by Elsevier in SSRN Electronic Journal
Open AccessOptimizing Surface Chemical Etching Process to Improve Photoemission from Algaas Photocathodes
Negative-electron-affinity AlGaAs photocathodes offer applications in underwater detection and green-laser driven electron sources due to their adjustable response threshold, long operating lifetime and fast response time. However, the difficulty of removing surface Al oxide is a key factor limiting the improvement of photoemission performance of AlGaAs photocathodes. To prevent oxidation of AlGaAs from exposure to air, a thin GaAs cap layer is commonly employed as the protective layer. Removing the GaAs cap layer and obtaining a clean and smooth AlGaAs surface are prerequisites for achieving high photoemission performance. Three sets of two-step chemical etching experiments were designed to remove the GaAs cap layer and obtain an AlGaAs emission surface favorable for Cs-O activation. By surface elemental analysis and surface topography test, it was found that the sample treated by the two-step chemical etching with the C6H8O7: H2O2 mixed solution and diluted HCl solution exhibited the lowest surface oxidation degree and roughness, and possessed the highest quantum efficiency over the entire waveband after activation. In additional, by fitting the experimental quantum efficiency curves, it is confirmed that the lower surface oxidation degree and roughness can effectively optimize surface barrier and enhance the photoelectron escape probability, resulting in the higher quantum efficiency.
- 10 December 2022
- Published by World Scientific Pub Co Pte Ltd in Modern Physics Letters B
- Vol. 36 (34)
Reflection-mode nanostructured GaAlAs photocathode with narrow-band response to 532 nm
The underwater photoelectric detection equipment mainly uses 532 nm laser as the light source, but the corresponding photocathodes like Na2KSbCs, GaAs and GaAsP have a wide spectral response region and are easily affected by other signals. Thereby, GaAlAs are materials worth developing because of their adjustable band gap, which usually is used as a window layer of GaAs-based photocathode. In this paper, the finite difference time domain (FDTD) method is used to carry out nanostructure design simulations. The results show that GaAlAs with Al component of 0.63 can obtain the cutoff wavelength near 532 nm, which is an excellent photocathode material to meet the requirement of narrow-band spectral response of 532 nm laser. Furthermore, the light absorptance can be improved effectively by the quadrangular prism or cylinder nanostructured array prepared on the Ga[ ]Al[ ]As emission layer surface, and the maximum light absorptance can reach 96.2% at 532 nm for the cylinder nanostructure array with a height of 900 nm and a base width of 100 nm. Nevertheless, the reflection-mode Ga[ ]Al[ ]As photocathode with the quadrangular prism nanostructured array can be slightly influenced with incident angle of light.
- 10 December 2022
- Published by World Scientific Pub Co Pte Ltd in Modern Physics Letters B
- Vol. 36 (34)
Reflection-mode nanostructured GaAlAs photocathode with narrow-band response to 532 nm
The underwater photoelectric detection equipment mainly uses 532 nm laser as the light source, but the corresponding photocathodes like Na2KSbCs, GaAs and GaAsP have a wide spectral response region and are easily affected by other signals. Thereby, GaAlAs are materials worth developing because of their adjustable band gap, which usually is used as a window layer of GaAs-based photocathode. In this paper, the finite difference time domain (FDTD) method is used to carry out nanostructure design simulations. The results show that GaAlAs with Al component of 0.63 can obtain the cutoff wavelength near 532 nm, which is an excellent photocathode material to meet the requirement of narrow-band spectral response of 532 nm laser. Furthermore, the light absorptance can be improved effectively by the quadrangular prism or cylinder nanostructured array prepared on the Ga[ ]Al[ ]As emission layer surface, and the maximum light absorptance can reach 96.2% at 532 nm for the cylinder nanostructure array with a height of 900 nm and a base width of 100 nm. Nevertheless, the reflection-mode Ga[ ]Al[ ]As photocathode with the quadrangular prism nanostructured array can be slightly influenced with incident angle of light.
- 5 November 2020
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 128 (17) , 173103
Effect of excessive Cs and O on activation of GaAs(100) surface: From experiment to theory
The surface Cs–O activation process directly determines quantum efficiency and stability of negative-electron-affinity photocathodes. To investigate the effects of excessive Cs and O supply on activation and to explore a more effective Cs–O activation recipe, Cs–O activation experiments of GaAs(100) photocathodes are carried out based on the current-driven solid Cs and O dispensers. By a comparison of differences in activation photocurrent, quantum efficiency, and photocurrent decay, it is found that the recipe of excessive O and non-excessive Cs is not suitable for activating GaAs photocathodes, while the recipe of continuous and completely excessive Cs along with intermittent and non-excessive O can achieve the most excellent photoemission performance, including the highest quantum efficiency in the long-wave threshold region and best stability under intense light irradiation after activation. Furthermore, this improved activation recipe with the least Cs–O alternating cycles is easier to operate. Combined with density functional calculations and dipole layer model, it is found that the activation recipe of completely excessive Cs and non-excessive O can form effective dipoles to the greatest extent, and avoid the direct interaction between As atoms and O atoms to form As–O–Ga oxides on the GaAs(100) reconstructed surface.
- 5 November 2020
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 128 (17) , 173103
Effect of excessive Cs and O on activation of GaAs(100) surface: From experiment to theory
The surface Cs–O activation process directly determines quantum efficiency and stability of negative-electron-affinity photocathodes. To investigate the effects of excessive Cs and O supply on activation and to explore a more effective Cs–O activation recipe, Cs–O activation experiments of GaAs(100) photocathodes are carried out based on the current-driven solid Cs and O dispensers. By a comparison of differences in activation photocurrent, quantum efficiency, and photocurrent decay, it is found that the recipe of excessive O and non-excessive Cs is not suitable for activating GaAs photocathodes, while the recipe of continuous and completely excessive Cs along with intermittent and non-excessive O can achieve the most excellent photoemission performance, including the highest quantum efficiency in the long-wave threshold region and best stability under intense light irradiation after activation. Furthermore, this improved activation recipe with the least Cs–O alternating cycles is easier to operate. Combined with density functional calculations and dipole layer model, it is found that the activation recipe of completely excessive Cs and non-excessive O can form effective dipoles to the greatest extent, and avoid the direct interaction between As atoms and O atoms to form As–O–Ga oxides on the GaAs(100) reconstructed surface.