QZQian Zhang

Qian Zhang

*This is an algorithmically generated author record based on publicly available information.

Qian Zhang has a total of 26 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Improving the processability of plane flow casting and quality of amorphous ribbons for high Bs Fe-Co-Si-B-P-C alloy by the purification of melts

    by Qian Zhang, Hao Wang, Kuang Lv, Fang Wang, Chuntao Chang, Haichen Yu, Guangqiang Zhang, Shaoxiong Zhou, Xidong Hui

  • Open Access

    Rapid-annealed FeSiBPCu nanocrystalline alloy with high Bs approaching 1.9 T and good bendability

    by Qian Zhang, Yang Meng, Chengliang Zhao, Chuntao Chang, Shujie Pang, Shaoxiong Zhou


  • Open Access

    Effects of Stress on Loss and Magnetic Properties of Fe80Co3Si3B10P1C3 Amorphous Iron Cores

    by Wei Zheng, Guangqiang Zhang, Qian Zhang, Haichen Yu, Zongzhen Li, Su Song, Mingyu Gu, Shaoxiong Zhou, Xuanhui Qu

    The research on how to reduce energy consumption and improve the efficiency of amorphous motors has extensive coverage. This study systematically investigates the influence of internal stress induced by impregnation curing and interference fit on the soft magnetic properties and loss characteristics of Fe80Co3Si3B10P1C3 (CAF4) amorphous alloy iron cores. The amorphous iron core samples undergo analysis through differential scanning calorimetry (DSC), transmission electron microscopy (TEM), X-ray diffraction (XRD), magnetic performance testing equipment, flexible pressure sensors, and magnetostriction testers. The CAF4 amorphous iron core after impregnation curing (AIC) exhibits the lowest loss of P1.2T,1.5 kHz = 22.8 W/kg when annealed at 260 °C, representing a 21% increase compared to the pre-impregnation curing (BIC) state. Within the commonly utilized interference fit range, the loss growth rate of CAF4 amorphous iron cores is lower than that of Fe80Si9B11 (1K101). Likewise, at a frequency of 50 Hz and an excitation of 1000 A/m, the magnetostriction coefficient of CAF4 is smaller than that of 1K101. Within the typical interference fit range, the magnetization performance of CAF4 amorphous iron cores surpasses that of 1K101, favoring lightweight and compact motor designs and reducing copper losses. Consequently, CAF4 amorphous iron cores exhibit significant advantages when employed in motors.


  • Open Access

    The Effect of Annealing on the Soft Magnetic Properties and Microstructure of Fe82Si2B13P1C3 Amorphous Iron Cores

    by Wei Zheng, Guangqiang Zhang, Qian Zhang, Haichen Yu, Zongzhen Li, Mingyu Gu, Su Song, Shaoxiong Zhou, Xuanhui Qu

    This research paper investigated the impact of normal annealing (NA) and magnetic field annealing (FA) on the soft magnetic properties and microstructure of Fe82Si2B13P1C3 amorphous alloy iron cores. The annealing process involved various methods of magnetic field application: transverse magnetic field annealing (TFA), longitudinal magnetic field annealing (LFA), transverse magnetic field annealing followed by longitudinal magnetic field annealing (TLFA) and longitudinal magnetic field annealing followed by transverse magnetic field annealing (LTFA). The annealed samples were subjected to testing and analysis using techniques such as differential scanning calorimetry (DSC), transmission electron microscopy (TEM), X-ray diffraction (XRD), magnetic performance testing equipment and magneto-optical Kerr microscopy. The obtained results were then compared with those of commercially produced Fe80Si9B11. Fe82Si2B13P1C3 demonstrated the lowest loss of P1.4T,2kHz = 8.1 W/kg when annealed in a transverse magnetic field at 370 °C, which was 17% lower than that of Fe80Si9B11. When influenced by the longitudinal magnetic field, the magnetization curve tended to become more rectangular, and the coercivity (B3500A/m) of Fe82Si2B13P1C3 reached 1.6 T, which was 0.05 T higher than that of Fe80Si9B11. During the 370 °C annealing process of the Fe82Si2B13P1C3 amorphous iron core, the internal stress in the strip gradually dissipated, and impurity domains such as fingerprint domains disappeared and aligned with the length direction of the strip. Consequently, wide strip domains with low resistance and easy magnetization were formed, thereby reducing the overall loss of the amorphous iron core.


  • Open Access

    Effect of Pre-Oxidation Treatment on Corrosion Resistance of FeCoSiBPC Amorphous Alloy

    by Qian Zhang, Xidong Hui, Zongzhen Li, Guangqiang Zhang, Jingcheng Lin, Xuelian Li, Wei Zheng, Xia Cao, Shaoxiong Zhou

    In this paper, the corrosion resistance of FeCoSiBPC amorphous alloy after pre-oxidation and non-oxidation heat treatment is investigated. The corrosion behaviors of Fe80Co3Si3B10P1C3 amorphous alloys in 1 mol/L NaCl solution were investigated by the electrochemical workstation. The pre-oxidation heat treatment can improve the corrosion resistance of FeCoSiBPC amorphous alloy through an increase in the Ecorr value from −0.736 to −0.668 V, which makes it easy to reach a passive state. The corroded morphology and products of amorphous alloys were tested by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The SEM/TEM analysis showed that, after pre-oxidation treatment, the oxide layer was divided into two layers: the inner layer was amorphous, the outer layer appeared crystalline, and the main oxide was Fe2O3. During the oxidation process, Co and P elements diffused from the inner layer to the outer layer, forming phosphorus and cobalt oxides with high corrosion resistance on the surface of the ribbon, thereby improving the corrosion resistance of the ribbon.


  • The role of P content on the glass-forming ability and the magnetic properties of FeSiBPC amorphous alloys

    by Qian Zhang, Zongzhen Li, Guangqiang Zhang, Wei Zheng, Xia Cao, Xidong Hui, Shaoxiong Zhou


  • Effects of Cr addition on the glass‐forming ability and the corrosion behaviors of FeCBSiP amorphous alloys

    by Qian Zhang, Shaoxiong Zhou, Zongzhen Li, Guangqiang Zhang, Wei Zheng, Xidong Hui

    The corrosion behaviors of Fe83‐XC1B11Si2P3CrX (X = 0, 1, 2, and 3 at%) amorphous alloys in 0.1 M NaCl solution have been investigated by immersion and electrochemical tests. With the addition of Cr content from 0 to 3 at%, the corrosion rate of amorphous alloys gradually decreases from 2.57 × 10−1 to 1.04 × 10−1 mm·year−1. The minor addition of Cr improves the corrosion resistance through the increase in the Ecorr value, which makes it easy to reach a passive state and suppress pitting corrosion. The corroded morphology and products of amorphous alloys have been tested by scanning electron microscopy (SEM) and energy‐dispersive spectroscopy (EDS). The SEM/EDS analysis shows that the high corrosion resistance is due to the formation of dense and stable chromium oxide during immersion in NaCl solutions.