Junzhao Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Junzhao Liu has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
Ganghu Cheng
State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China
1 shared publication- Haojun Li
College of Surveying and Geo‐Informatics Tongji University Shanghai China
1 shared publication - Jiraphorn Sawasdiruk
Innovation management college, Suan Sunandha Rajabhat University Bangkok, Thailand
1 shared publication - Kexuan Chen
Biomedical Pioneering Innovative Center, School of Life Sciences, Peking University, Beijing, China
1 shared publication Liangke Huang
1 shared publicationSujun Lu
State Key Laboratory of Nickel and Cobalt Resources Comprehensive Utilization, Jinchang 737100, China
1 shared publication
Latest Publications
- 30 July 2024
- Published by Elsevier in Measurement
- Vol. 238
Improvement of BDS-3 inter-frequency clock bias estimation and its application in multi-frequency precise point positioning
- 30 July 2024
- Published by Elsevier in Measurement
- Vol. 238
Improvement of BDS-3 inter-frequency clock bias estimation and its application in multi-frequency precise point positioning
- Open Access
- 1 September 2023
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 2587 (1) , 012005
The Influence of Ball Milling Time and Sintering Temperature on the Structural and Capabilities of FeCoCrNiMn High-Entropy Alloy
This study reports the fabrication of FeCoCrNiMn high-entropy alloy using high-purity powders of Fe, Co, Cr, Ni, and Mn through the processes of mechanical alloying (MA) and spark plasma sintering (SPS). We systematically investigated the effects of different ball milling times (10 h, 20 h, 30 h, 40 h, 50 h) and sintering temperatures (700°C, 800°C, 900°C, 1000°C, 1100°C) on the structure and capabilities of the alloy. The findings indicate that the atomic proportion of Fe:Co:Cr:Ni:Mn approach 1:1:1:1:1. The distribution of all elements is basically uniform, but the Cr element is slightly biased in the structure after 40 h ball milling. The voids in the structure are gradually decreasing as temperatures rise. The matrix structure is mainly composed of a white FCC matrix phase and a gray Cr-rich σ phase. The alloy structure is the densest. It has the highest density of 7.060 g/cm3, the highest compressive strength of 1480 MPa, and a plastic deformation of 13% when the SPS temperature reaches 1000°C. The FeCoCrNiMn high-entropy alloy is prepared by a ball milling time of 40 h, and spark plasma sintering of 1000°C has the best comprehensive properties.
- 1 September 2023
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 2587 (1) , 012005
Open AccessThe Influence of Ball Milling Time and Sintering Temperature on the Structural and Capabilities of FeCoCrNiMn High-Entropy Alloy
This study reports the fabrication of FeCoCrNiMn high-entropy alloy using high-purity powders of Fe, Co, Cr, Ni, and Mn through the processes of mechanical alloying (MA) and spark plasma sintering (SPS). We systematically investigated the effects of different ball milling times (10 h, 20 h, 30 h, 40 h, 50 h) and sintering temperatures (700°C, 800°C, 900°C, 1000°C, 1100°C) on the structure and capabilities of the alloy. The findings indicate that the atomic proportion of Fe:Co:Cr:Ni:Mn approach 1:1:1:1:1. The distribution of all elements is basically uniform, but the Cr element is slightly biased in the structure after 40 h ball milling. The voids in the structure are gradually decreasing as temperatures rise. The matrix structure is mainly composed of a white FCC matrix phase and a gray Cr-rich σ phase. The alloy structure is the densest. It has the highest density of 7.060 g/cm3, the highest compressive strength of 1480 MPa, and a plastic deformation of 13% when the SPS temperature reaches 1000°C. The FeCoCrNiMn high-entropy alloy is prepared by a ball milling time of 40 h, and spark plasma sintering of 1000°C has the best comprehensive properties.