Type
Company
Locations
Montreal, Canada
Relationships
Parent Organizations

Latest Publications

  • Enzymatic treatment processes for the production of cellulose nanomaterials: A review

    by Xin Tong, Zhibin He, Linqiang Zheng, Harshad Pande, Yonghao Ni


  • A new technique for the measurement of show-through mottle of fine paper

    by Jean-Philippe Bernie, Julie Talbot, Harshad Pande

    Mottling within print-through and show-through is caused by the variability of the local optical properties of the sheet. This mottling is visually disturbing and a mark of poor paper quality. The ability to predict print-through mottle of printed paper by measuring show-through mottle on the unprinted sheet would be a valuable asset for paper machine control. We examined the relationship between print-through mottle and show-through mottle. We worked with nine samples of 60 lb. uncoated fine paper (90 g/m2), from various North American paper companies, that were printed on an offset press, 400K (400% Black), on both sides. A show-through mottle instrumental determination technique was developed using an existing Fast Fourier Transform-based algorithm. The nine samples examined were ranked similarly by the visual evaluation of print-through mottle and by the instrumental determination of show-through mottle. We thus established that show-through on the unprinted sheet can be used as a reliable predictor of print-through, therefore saving time and money for papermakers. We also found a significant two-sidedness in show-through for some of the samples.

  • Using cupriethylenediamine (CED) solution to decrease cellulose fibre network strength for removal of pulp fibre plugs

    by Wen‐Hui Zhang, Ryan Mitchell Christensen, Ryan Lutes, Xuesi Liu, Jinli Zhang, Mark Martinez, Harshad Pande, Bruno Marcoccia, Yonghao Ni

    The pulp and paper industry is the largest industrial sector that converts wood‐based materials into fibre‐related products. It is common for pulp fibre plugs to develop within pipelines and equipment causing operational downtime, which ultimately requires the use of costly procedures for plug removal. In this study, a laboratory‐scale set‐up was developed to measure the breakup pressure of pre‐formed plugs to indicate the plug (fibre network) strength. A cupriethylenediamine (CED) solution was investigated with regards to its ability to decrease the plug strength. When the concentration of the CED solution is 0.1 M or lower, the plug breakup pressure increases due to fibre swelling. Conversely, when the CED concentration is 0.2 M or greater, the plug breakup pressure decreases significantly due to partial fibre dissolution.


  • Analysis of the permeability tensor and the correlation length of heterogeneities in paper using X-ray microtomography

    by S. Lavrykov, S. K. Singh, B. V. Ramarao, S. Ramaswamy, H. Pande

    A technique to determine the permeability from X-ray microtomographic images was developed and applied to paper structures. The images are thresholded and a skeleton of the pore space is obtained from the images. The skeleton is represented by means of a network of resistances. The total resistance of the network along the principal directions is now determined both in the in-plane (X, Y) as well as through the plane (Z) directions. The network resistance for structures at each section is determined. From this data, a correlation length for the network resistance is obtained. Correlation length data are used for determining the effect of heterogeneities on transport properties of paper structures. From this analysis, it is possible to analyze and simulate the moisture transport processes such as wicking and drying in paper, reproducing smaller-scale variations. Permeabilities in the thickness direction were calculated from the X-ray microtomographic reconstructions of the pore space. A set of paper samples prepared with different amounts of fines but with similar porosity and density was analyzed. The permeabilities of the X-ray reconstructions were reduced significantly in papers with fines in agreement with macroscopic measurements of flow through the same sheets. This demonstrated the higher tortuosities of the papers and their increased flow resistance, although the macroscopic porosity and density were relatively unchanged. The same analysis was repeated for a set of pilot machine sample papers to demonstrate variations in permeability predicted by X-ray microtomographic analyses in agreement with expected increases due to refining of pulps.


  • Method for Improving Separation of Carbohydrates from Wood Pulping Liquors and Wood or Biomass Hydrolysis Liquors

    by Alicia Compere, San Diego General Atomics, Bruno Marcoccia, James Elliott

    The U.S. Department of Energy's Office of Scientific and Technical Information

  • Some Aspects of Materials Selection for Condensing Economizers

    by Joseph Kish, Neville Stead, Douglas Singbeil, Fernando Preto, François Jetté

    The use of a condensing economizer within a biomass combustion system is a potentially attractive heat recovery solution for the pulp and paper industry. Selecting materials from which to construct condensing economizers for installation within utility power boiler units is, however, not trivial considering that aqueous sulphuric acid (H2SO4) condensates are typically formed. The expected corrosiveness of the flue gas condensate derived from pulp and paper biomass fuels is likely higher than that derived from natural gas (lower sulphur and chlorine contents), but lower than that derived from fossil fuels (higher sulphur and chlorine contents). To help guide materials selection, a laboratory corrosion testing program was initiated to evaluate the corrosion resistance of candidate alloys to synthetic acidic flue gas condensates expected to be derived from pulp and paper biomass fuels. The initial work, which is reported here, was focused on evaluating the resistance of carbon steel and stainless steel to dewpoint corrosion in chloride-free aqueous H2SO4 condensates and to stress corrosion cracking in a saturated aqueous ammonium nitrate (NH4NO3) solution.

  • Assesment of Molten Na2S●xH2O/NaOH Solutions as a Cause of Composite Tube Corrosion in Kraft Recovery Boilers

    by J. R. Kish, D. L. Singbeil, J. R. Keiser, F. R. Jetté

    Cladding/overlay thickness measurements were made on several primary air ports fabricated from alternative composite tubes installed in a kraft recovery boiler to document the fireside corrosion. Laboratory corrosions tests were then conducted to reproduce the relative corrosion rates determined by the field thickness measurments. It was found that all of the major available composite tube systems are suceptible to corrosion. Hydrated sodium sulphide and oxygen in combination with sodium hydroxide are implicated as major components in the liquid environment that causes the corrosion. Prevenative measures discussed include the need for a well-sealed port, and the likely need to avoid having black liquor droplets contacting the port tubes while dehydration is incomplete.

  • A Note On The Theory Of Replacement

    by David Toole

    Most models of economic life to replacement of equipment liable to deterioration with age but not catastrophic failure may be reduced to a basic model. Serious errors could result from use of this model if economic life is sensitive to errors in estimates of its parameters or mistaken assumptions as to the functional relationships between costs and age. Results of an investigation into the sensitivity of economic life to such errors are presented in this paper. The extent to which the model adequately maps the real problem is also considered briefly