Type
Company
Locations
Beijing, China

Latest Publications

  • Open Access

    Two Episodes of Au and Ag–Pb–Zn Mineralization in the Kangshan Deposit, the Southern Margin of the North China Craton: Constraints from C–O–S Isotopes and Sphalerite Rb–Sr Dating

    by Zheming Zhang, Qingdong Zeng, Yongbin Wang

    Polymetallic deposits are significant repositories of both bulk commodities and critical metals. However, determining the ages of multiple mineralization events in these deposits remains a persistent challenge. The Kangshan Au-polymetallic deposit, located in the southern margin of the North China Craton, exhibits distinct mineralization zonation, transitioning from deep-seated gold mineralization to shallow Ag–Pb–Zn mineralization, making it a natural laboratory for investigating composite mineralization processes. Based on mineral paragenetic assemblages, the ore-forming process can be divided into four stages: quartz with minor pyrite (Stage 1); quartz–pyrite–chalcopyrite with minor native gold (Stage 2); polymetallic sulfides–quartz–ankerite with native gold (Stage 3); and quartz–calcite–fluorite (Stage 4). In situ sulfur isotope analysis of pyrite from Stage 3 yields δ34SV-CDT values of 7.30‰–8.30‰, higher than the typical magmatic range and indicative of a heavier crustal (marine-sulfate) sulfur component incorporated into the late-stage ore fluids. Sphalerite from Stage 3 has an initial 87Sr/86Sr ratio of 0.708576 ± 0.000056, suggesting a mixed crust–mantle source. Calcite from Stage 4 has δ13CPDB values of −4.63‰ to −3.45‰ and δ18OSMOW values of 15.76‰–16.41‰, indicating that the late-stage ore-forming fluids were contaminated by carbonate wall rocks. Rb–Sr isotopic dating of sphalerite yields an age of 109.2 ± 2.3 Ma for the Ag–Pb–Zn orebodies, indicating that they formed in the Early Cretaceous, approximately 20 Myr later than the regional gold mineralization event (131.7 ± 4.6 Ma). This temporal gap suggests two distinct magmatic-hydrothermal mineralization events rather than a continuous evolutionary sequence. Integrating our results with the regional magmatic geochronological framework, we propose that the gold mineralization and Ag–Pb–Zn mineralization at the Kangshan deposit represent two separate hydrothermal events. Both events formed in an extensional tectonic setting associated with the destruction of the North China Craton and were spatially superimposed within the same fault system. The deposit is classified as a medium–low-temperature, post-magmatic hydrothermal vein system with a weak epithermal affinity.

  • A Chromium‐Free Fe‐Added MgO–SiC–C Refractory With Superior Dynamic Matte Slag Corrosion Resistance

    by Xu Zhao, Tianbin Zhu, Weijie Guo, Qilong Chen, Yuhang Zhang, Yawei Li, Yajie Dai, Wengang Yang, Honggang Sun

    To develop a chromium‐free alternative to MgO–Cr 2 O 3 refractories for matte smelting furnaces, this study investigated three novel MgO–SiC–C refractories (with Fe, Si 3 N 4 , or Si 3 N 4 –Fe additions) via induction furnace tests simulating actual smelting. Results showed MgO–Cr 2 O 3 sample had poor slag penetration resistance due to a porous layer filled with low‐melting (Mg 1 − x , Fe x ) 2 SiO 4 , impairing stability and allowing partial Cu 2 S penetration. The Fe‐containing MgO–SiC–C sample exhibited superior dynamic corrosion resistance (comparable to MgO–Cr 2 O 3 , better in penetration resistance), attributed to low porosity, protective Mg(Fe, Al) 2 O 4 and MgAl 2 O 4 phases, Fe–Si alloy void filling, and graphite‐inhibited Cu 2 S penetration. Si 3 N 4 ‐containing samples degraded dynamically (despite good static slag resistance) as Si 3 N 4 formed low‐melting (Mg 1 − x , Fe x ) 2 SiO 4 , weakening stability. Overall, the Fe‐containing MgO–SiC–C refractory is a promising chromium‐free alternative for matte smelting furnaces.

  • Open Access

    Rapid Microwave Plasma Engineering of HfO 2 /C@C Core‐Shell Fibrous Membrane Toward Flexible High‐Performance Electromagnetic Wave Absorption

    by Qichao Ding, Limeng Song, Wei Li, Jiangtao Hao, Xuewen Jiang, Mengru Li, Xinglai Yuan, Gang Wang, Yanqiu Zhu, Mi Tian, et al.

    Flexible electromagnetic wave (EMW) absorbers that simultaneously exhibit excellent impedance matching, strong attenuation capability, and mechanical robustness remain highly desirable yet challenging to realize, particularly for dielectric HfO 2 ‐based materials owing to their intrinsically low conductivity and limited polarization capability. Herein, a rapid and environmentally friendly CO 2 microwave plasma torch strategy is developed to fabricate flexible HfO 2 /C@C core‐shell fibrous membranes with tunable defects. The ultrafast plasma process simultaneously regulates the crystalline structure of HfO 2 , the graphitization of the carbon shell, and the concentration of oxygen vacancies, thereby constructing highly coupled dielectric‐conductive heterointerfaces. Therefore, the optimized HfO 2 /C@C‐2 sample exhibits outstanding microwave absorption, with a minimum reflection loss of −65.75 dB at 3.2 mm and an effective absorption bandwidth of 7.37 GHz. Meanwhile, the interconnected one‐dimensional fibrous network endows the material with excellent flexibility and fatigue resistance, while radar cross‐section simulations further demonstrate its superior stealth capability. This work establishes a clear processing‐structure‐property relationship and proposes a green plasma strategy to overcome the performance‐practicality trade‐off of HfO 2 ‐based absorbers, providing a promising route toward next‐generation flexible EMW absorbing materials.

  • Open Access

    CFD-Based Evaluation of a Serial Air-Supply Strategy in a Continuous Annular Cooler for Uniform Sinter Discharge Temperature

    by Jiayu Pi, Hui Li, Jingxuan Xie, Liang Wang, Hongfei Liu, Leping Dang, Hongyuan Wei

    Non-uniform discharge temperature during sinter cooling is a practical issue in ironmaking, as local overheating may increase the thermal load on downstream conveying equipment. To mitigate insufficient cooling in the upper sinter bed under the conventional bottom-blowing mode, this study developed a three-dimensional transient CFD model for an industrial continuous annular cooler and optimized the air-supply strategy in Zones IV and V. Under the conventional condition, ambient air is supplied independently to Zones IV and V from the bottom wind boxes. In the novel air-supply strategy, while keeping the total fresh cooling-air flow rate in the final cooling region unchanged, ambient air is introduced from the upper side of Zone V and discharged from its bottom; the outlet gas from Zone V is then supplied to the bottom of Zone IV, forming a serial air-supply path. The results show that the novel arrangement improves the spatial matching between the cooling gas and the sinter bed during final cooling and suppresses the local high-temperature region near the discharge end. The maximum discharge temperature decreases from 459 K to 410 K, below the process limit of 423 K, while the average discharge temperature decreases from 377 K to 364 K. Based on the enthalpy-flow difference calculation, the predicted recoverable waste heat also increases under the novel condition. These findings suggest that redesigning the gas-flow route in the final cooling region can effectively enhance the uniformity of the discharge temperature in industrial annular coolers.

  • Effects of Submerged Entry Nozzle Treated by Pulsed Positive Electric Field on Continuous Casting Process of Automotive Sheet Steel

    by Qiang Gu, Sengwang Yan, Weikui Ma, Guoqi Liu, Wengang Yang, Lei Yuan, Hongxia Li

    This study investigates the effects of a pulsed positive electric field applied to the Submerged Entry Nozzle (SEN) on the continuous casting of automotive sheet steel. The results indicate that the pulsed positive electric field (average current of 75 A, pulsed current of 150 A, and frequency of 10 000 Hz) provides an electrostatic driving force for Al 2 O 3 inclusions to migrate away from the SEN wall, while disrupting their original force balance and inhibiting interinclusion contact and agglomeration. Consequently, the SEN inner cavity clogging thickness is reduced by 79.37% (from 12.65 to 2.61 mm), the average qualification rate of mold level fluctuations (QRM) (>±3 mm) is increased by 45.76%, the amount of the large‐sized inclusions (>5 μm) is decreased from 266 to 199, the morphology and composition of inclusions are regulated, the tensile strength of the slab increased by 3.85% (from 338 to 351 MPa), and the nonproportional elongation strength of the slab improves by 6.67% (from 210 to 224 MPa). This ultimately reduces the downgrade rate during slab rolling by 41.75% (from 1.03% to 0.60%).

  • Open Access

    Effect of Basicity on Consolidation Behavior and Phase Evolution of Mg-Bearing Medium Silica Fluxed Pellets

    by Haoyu Cai, Jianliang Zhang, Yaozu Wang, Jixiang Han, Rui Deng, Zhengjian Liu

    Against the background of blast furnace burden optimization and the low-carbon transition of the steel industry, the development of high-quality Mg-bearing fluxed pellets is of great significance for the efficient utilization of medium-high silica iron ore concentrates. In this study, Mg-bearing medium-high silica fluxed pellets with a fixed SiO2 content of 5.5% were prepared, and the effect of basicity in the range of R = 1.0–1.4 on compressive strength, liquid phase behavior, slag phase composition, and pore structure evolution was systematically investigated. The results showed that the compressive strength of the pellets decreased from 2527 N/pellet to 2079 N/pellet as the basicity increased from 1.0 to 1.4. At 1250 °C, the liquid phase content first decreased from 2.66% to 1.30% and then increased to 7.38%, while the liquid phase viscosity decreased continuously. Meanwhile, the liquid phase composition evolved from a SiO2-rich calcium–iron silicate system to a Fe2O3− and CaO-rich system. XRD results indicated that Fe2O3 was the dominant crystalline phase in the pellets, accompanied by a small amount of Fe3O4, whereas no distinct highly crystalline slag phase was detected. The slag phase was mainly a Fe-Ca-Si composite slag, in which the Fe2O3 content increased and the SiO2 content decreased with increasing basicity. At higher basicity, the number and size of pores increased, and the pore morphology evolved from dispersed fine pores to irregular large pores and locally connected pores. Meanwhile, the slag phase became more widely distributed and locally enriched, weakening the continuity of the iron oxide load-bearing skeleton, which was the main reason for the decrease in compressive strength. This study provides a theoretical basis for preparing high-quality Mg-bearing fluxed pellets from medium-high silica iron ore concentrates.

  • Open Access

    Isothermal Reduction of Wustite Under Hydrogen Atmosphere at 1673 K–1773 K

    by Fulong Li, Jianliang Zhang, Yang Li, Tengfei Wang, Ben Feng, Yaozu Wang, Chunmei Yu, Zhengjian Liu

    The use of hydrogen for smelting reduction ironmaking can effectively reduce the consumption of coke, as well as the CO2 emission. However, the dynamic mechanism of this process is not clear. In this paper, isothermal thermogravimetric analysis (TGA) was used to study the reduction process of wustite by hydrogen at 1673–1773 K. Results show that wustite can be entirely reduced, and with the increase in temperature, the reduction reaction becomes more intense, and the time required for the entire reduction decreases. The hydrogen reduction of wustite at 1673–1773 K fits the Mampel power model: f(α) = 2α1/2. When the reactants are molten and the products are solid, the apparent activation energy of the reduction process calculated by the iso-conversional method is 9.15 kJ·mol−1. Molecular dynamics simulation results show that the adsorption of hydrogen molecule on FeO surface is spontaneous. With the increase in temperature, FeO substrate becomes more active, and hydrogen molecules move more violently. The average distance between a certain hydrogen atom and its neighboring atom was analyzed statistically. The increase in temperature will increase the average bond length of hydrogen molecules, reduce their bond energy, and facilitate the adsorption of hydrogen molecules on the FeO surface.


  • Binder Effect on Corrosion Mechanism of Al 2 O 3 ‒Cr 2 O 3 Castables for Copper Anode Fire Refining

    by Yu Qin, Qidu Li, Zhisen Yang, Zhaolin Xu, Jiaqi Wang, Honggang Sun, Hongrui Zhang, Liugang Chen

    To improve the performance and lifetime of refractories used at the tuyere zone in copper anode fire refining (CAFR) furnace, Al 2 O 3 ‒Cr 2 O 3 castables bonded with reactive magnesia (R‒C), hydratable alumina (H‒C), and calcium aluminate cement (C‒C) were comparatively investigated in terms of resistance to corrosion and infiltration by CAFR slag. The thermal shock resistance of the prepared castables was also studied. Results indicate that the R‒C castable formed Mg(Al,Cr) 2 O 4 spinel in situ at elevated temperatures. The Mg(Al,Cr) 2 O 4 spinel could incorporate Cu 2+ and Fe 2+ /Fe 3+ from the CAFR slag to form (Mg,Cu,Fe)(Al,Cr,Fe) 2 O 4 spinel, which blocked pores in the castable matrix and thus hindered further slag infiltration. Consequently, R‒C castables exhibited superior resistance to slag corrosion and infiltration compared with H‒C and C‒C castables. In addition, R‒C castables showed the highest residual strength ratio after thermal shock testing.

  • Open Access

    Study on the energy evolution mechanism and periodic micro-fracture of the BR under triaxial compression tests

    by Yuye Tan, Ziyi Zeng, Jiazhao Chen, Mochuan Guo, Weidong Song

    In underground metal mining, the complex environment and in-situ stress control requirements impose increasingly strict standards on backfill mining methods. Owing to its advantages of safety, high efficiency, economy, and environmental friendliness, backfill mining has become an inevitable choice for green mining. This study focuses on the two-step stope post-backfill method, where the stability of the backfill-encased-rock (BR) composite structure—formed by backfill wrapping rock—plays a crucial role in overall stope stability.Taking the BR composite structure as the research object, with single rock and backfill as controls, this study conducted triaxial compression tests combined with acoustic emission (AE), computed tomography (CT) technology, and theoretical analysis. It revealed the stage characteristics of the stress-strain curve during BR’s deformation and failure, as well as the energy evolution and crack propagation laws in each compression stage. The results indicate that BR’s stress-strain curve undergoes six stages, while its AE evolution is divided into five stages. As confining pressure increases, BR’s peak strength rises and energy release shows regular changes; CT scanning clearly presents its porosity variation and crack propagation rules.This study clarifies BR’s failure law under high stress: its peak strength is 20%–30% lower than pure rock, and residual strength is 65%–80% higher than pure backfill. These findings reflect the synergistic mechanical effect between backfill and rock under triaxial compression, and provide important guidance for stope structure stability research in practical mining engineering.


  • Top Cited Papers
    Open Access

    Microwave-assisted synthesis of high-performance TaC nanorods for enhanced electromagnetic wave absorption

    by Yongqiang Chen, Mao Chen, Haoyuan Lei, Limeng Song, Rui Zhang, Hongxia Li, Mi Tian, Bingbing Fan

    One-dimensional tantalum carbide (TaC) nanorods are considered promising candidates for high-temperature electromagnetic wave (EMW) absorption due to their intrinsic high electrical conductivity and exceptional thermal stability. However, conventional synthesis approaches typically yield products with low-quality and poor-efficiency, limiting their practical applicability. Here, we report a rapid and scalable synthesis of high-quality TaC nanorods via a molten salt-assisted carbothermal reduction strategy integrated with microwave heating. The formation of well-defined one-dimensional TaC nanorods was achieved within 20 minutes at 1300 °C by precisely tuning the precursor composition (Ta2O5:C:NaCl:Ni = 1:8:2:0.08). The resulting TaC nanorods exhibit notable EMW absorption properties, with a maximum effective absorption bandwidth (EABmax) of 3.0 GHz at a simulated thickness of 1.0 mm and a minimum reflection loss (RLmin) of –30.5 dB. Off-axis electron holography reveals pronounced charge accumulation at the Ta2O5 shell/TaC core interface, indicative of interfacial polarization effects. Furthermore, radar scattering cross-section (RCS) simulations demonstrate substantial attenuation of the backscattered signal from a PEC substrate coated with the TaC layer, with the strongest electromagnetic energy dissipation observed at a coating thickness of 1.0 mm. These results underscore the viability of microwave-assisted synthesis as an efficient and sustainable route for producing high-performance TaC nanorods for EMW absorption applications under extreme thermal conditions.