Nippon Steel (Germany)

Latest Publications
- 15 January 2019
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 59 (1) , 144-151
Effect of Surface Textures of Iron Substrate on the Crystal Orientation Relationship between Electrodeposited Zinc and Iron
To investigate the effect of iron texture on the crystal orientation relationship between iron and zinc, Zn deposition was performed galvanostatically at 1500 A/m2 at a charge density of 1.48 × 104 C/m2 onto high-purity electrolytic iron and cold rolled steel sheets in an agitated sulfate solution at 40°C. Fe with a large grain size showed an orientation relationship of {110}Fe//{0001}Zn. However, when the angle of inclination between the {110}Fe plane and the surface of electrolytic Fe was increased, the deviation in the orientation relationship {110}Fe//{0001}Zn increased. This result suggests that the orientation relationship of {110}Fe//{0001}Zn is difficult to maintain during the deposition when the inclination angle of the {110}Fe plane from the surface of electrolytic Fe increases. As a result, the epitaxial growth of Zn changes to random growth. Zn deposited on cold rolled steel sheets with a small grain size showed an orientation of {0001}, regardless of the orientation of Fe. This indicates that the orientation of the deposited Zn is more affected by the overpotential for deposition than by the orientation of steel sheets at the initial stage of deposition. Although strain was introduced into the high-purity electrolytic Fe with sandblasting, the orientation relationship of {110}Fe//{0001}Zn did not change remarkably, showing that the strain of Fe substrate has little effect on the orientation relationship between Fe and deposited Zn.
- 15 January 2019
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 59 (1) , 144-151
Effect of Surface Textures of Iron Substrate on the Crystal Orientation Relationship between Electrodeposited Zinc and Iron
To investigate the effect of iron texture on the crystal orientation relationship between iron and zinc, Zn deposition was performed galvanostatically at 1500 A/m2 at a charge density of 1.48 × 104 C/m2 onto high-purity electrolytic iron and cold rolled steel sheets in an agitated sulfate solution at 40°C. Fe with a large grain size showed an orientation relationship of {110}Fe//{0001}Zn. However, when the angle of inclination between the {110}Fe plane and the surface of electrolytic Fe was increased, the deviation in the orientation relationship {110}Fe//{0001}Zn increased. This result suggests that the orientation relationship of {110}Fe//{0001}Zn is difficult to maintain during the deposition when the inclination angle of the {110}Fe plane from the surface of electrolytic Fe increases. As a result, the epitaxial growth of Zn changes to random growth. Zn deposited on cold rolled steel sheets with a small grain size showed an orientation of {0001}, regardless of the orientation of Fe. This indicates that the orientation of the deposited Zn is more affected by the overpotential for deposition than by the orientation of steel sheets at the initial stage of deposition. Although strain was introduced into the high-purity electrolytic Fe with sandblasting, the orientation relationship of {110}Fe//{0001}Zn did not change remarkably, showing that the strain of Fe substrate has little effect on the orientation relationship between Fe and deposited Zn.
- 15 November 2018
- Published by Japan Society of Corrosion Engineering in Corrosion Engineering
- Vol. 67 (11) , 442-449
Establishment and Amendment of Test Standards for Evaluating Stress Corrosion Cracking Initiation in High temperature Water
高温高純度水環境での応力腐食割れ発生試験方法に対する既存の規格はほとんどないことから,原子力発電プラントに用いられる金属材料を対象とした応力腐食割れ発生試験方法の規格化を進めている.単軸引張定荷重試験方法の腐食防食学会規格JSCE S 1501を制定するとともに,逆U曲げ試験方法の日本工業規格JIS G 0511を改正した.さらに,この活動で検討した技術的内容をISO規格に反映することを試みている.
- 15 November 2018
- Published by Japan Society of Corrosion Engineering in Corrosion Engineering
- Vol. 67 (11) , 442-449
Establishment and Amendment of Test Standards for Evaluating Stress Corrosion Cracking Initiation in High temperature Water
高温高純度水環境での応力腐食割れ発生試験方法に対する既存の規格はほとんどないことから,原子力発電プラントに用いられる金属材料を対象とした応力腐食割れ発生試験方法の規格化を進めている.単軸引張定荷重試験方法の腐食防食学会規格JSCE S 1501を制定するとともに,逆U曲げ試験方法の日本工業規格JIS G 0511を改正した.さらに,この活動で検討した技術的内容をISO規格に反映することを試みている.
- Open Access
- 15 November 2018
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 58 (11) , 2117-2124
Effect of Surface Textures of Steel Sheets on the Crystal Orientation of Electrodeposited Zinc
Prior to electrodeposition, steel sheets underwent polishing using emery paper, buff, and then electrolytic polishing. Zn deposition was performed galvanostatically at 1500 A/m2 in an agitated sulfate solution at 40°C to investigate the effect of the surface textures of steel sheets on the crystal orientation of Zn. The strain of the steel surface and the decrease in Fe grain size due to this strain were largest with emery paper polishing, then with buff polishing, then when unpolished, and were smallest after electrolytic polishing. The preferred orientation of the {0001} Zn basal plane of the hcp structure was largest with electrolytic polishing, and decreased in the following order: unpolished, buff polishing, and then with emery paper polishing. Thus, the preference of the {0001} orientation of Zn increased with decreasing the strain of steel sheets and increasing the grain size of Fe. With electrolytic polishing, the strain applied to the steel sheets was decreased, the grain size of Fe increased, and therefore the epitaxial growth of deposited Zn occurred easily. The initial Zn deposits appeared to grow epitaxially as indicated by the orientation relationship of {111}Fe//{0001}Zn because the preferred orientation of the steel substrate used in this study is {111} Fe. The preferred orientation of {0001} Zn seems to be more common under conditions where the epitaxial growth of deposited Zn is easy to occur.
- 15 November 2018
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 58 (11) , 2117-2124
Open AccessEffect of Surface Textures of Steel Sheets on the Crystal Orientation of Electrodeposited Zinc
Prior to electrodeposition, steel sheets underwent polishing using emery paper, buff, and then electrolytic polishing. Zn deposition was performed galvanostatically at 1500 A/m2 in an agitated sulfate solution at 40°C to investigate the effect of the surface textures of steel sheets on the crystal orientation of Zn. The strain of the steel surface and the decrease in Fe grain size due to this strain were largest with emery paper polishing, then with buff polishing, then when unpolished, and were smallest after electrolytic polishing. The preferred orientation of the {0001} Zn basal plane of the hcp structure was largest with electrolytic polishing, and decreased in the following order: unpolished, buff polishing, and then with emery paper polishing. Thus, the preference of the {0001} orientation of Zn increased with decreasing the strain of steel sheets and increasing the grain size of Fe. With electrolytic polishing, the strain applied to the steel sheets was decreased, the grain size of Fe increased, and therefore the epitaxial growth of deposited Zn occurred easily. The initial Zn deposits appeared to grow epitaxially as indicated by the orientation relationship of {111}Fe//{0001}Zn because the preferred orientation of the steel substrate used in this study is {111} Fe. The preferred orientation of {0001} Zn seems to be more common under conditions where the epitaxial growth of deposited Zn is easy to occur.
- 15 October 2018
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 58 (10) , 1761-1767
Quantitative Evaluation of Reaction Mode and Reduction Disintegration Behavior of Iron Ore Agglomerates during Low Temperature Reduction
- 15 October 2018
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 58 (10) , 1761-1767
Quantitative Evaluation of Reaction Mode and Reduction Disintegration Behavior of Iron Ore Agglomerates during Low Temperature Reduction
- 15 August 2018
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 58 (8) , 1413-1419
In-situ Evaluation Method for Crack Generation and Propagation Behaviors of Iron Ore Burden during Low Temperature Reduction by Applying Acoustic Emission Method
In the field of ironmaking, there are few in situ non-destructive techniques for systematically evaluating the reduction behaviors of blast furnace (BF) burden materials. The standard method for the evaluation of the reduction disintegration index (RDI) includes low temperature reduction with a constant gas composition at a constant temperature followed by a cold strength test after cooling. During the reduction of iron ore burden in the BF, reduction disintegration proceeds in the course of increasing temperature through crack generation and propagation caused by volume expansion due to the reduction from hematite to magnetite. Acoustic emission (AE) method is an in situ non-destructive technique to evaluate the crack generation and propagation phenomena in various fields. In this study, we first attempted to apply AE method for a detailed in situ observation of BF burden materials by a combinational experiment of reduction disintegration. In the case of single-particle reduction, it was possible to detect AEs without friction between the sample and the waveguide giving rise to noise. Although a large number of AEs were measured during cooling of both sinter and pellet, the AE energy of the sinter was larger than that of the pellet. Furthermore, a significant number of AEs were also detected during heating of lump ore containing larger amount of combined water indicating possibility to evaluate the decrepitation behavior of such ores. By the packed bed reduction tests, which could evaluate average properties of iron ore burden, it was found that the AE energy attributed to thermal stress observed during cooling was higher than that to reduction degradation. These results suggest that it will be possible to eliminate the influence of crack generation within the iron ore burdens in the cooling stage by applying the in-situ non-destructive evaluation method developed in this study. It is also expected to apply for the quantitative estimation of the reduction disintegration behavior of burdens in the working BF.
- 15 August 2018
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 58 (8) , 1413-1419
In-situ Evaluation Method for Crack Generation and Propagation Behaviors of Iron Ore Burden during Low Temperature Reduction by Applying Acoustic Emission Method
In the field of ironmaking, there are few in situ non-destructive techniques for systematically evaluating the reduction behaviors of blast furnace (BF) burden materials. The standard method for the evaluation of the reduction disintegration index (RDI) includes low temperature reduction with a constant gas composition at a constant temperature followed by a cold strength test after cooling. During the reduction of iron ore burden in the BF, reduction disintegration proceeds in the course of increasing temperature through crack generation and propagation caused by volume expansion due to the reduction from hematite to magnetite. Acoustic emission (AE) method is an in situ non-destructive technique to evaluate the crack generation and propagation phenomena in various fields. In this study, we first attempted to apply AE method for a detailed in situ observation of BF burden materials by a combinational experiment of reduction disintegration. In the case of single-particle reduction, it was possible to detect AEs without friction between the sample and the waveguide giving rise to noise. Although a large number of AEs were measured during cooling of both sinter and pellet, the AE energy of the sinter was larger than that of the pellet. Furthermore, a significant number of AEs were also detected during heating of lump ore containing larger amount of combined water indicating possibility to evaluate the decrepitation behavior of such ores. By the packed bed reduction tests, which could evaluate average properties of iron ore burden, it was found that the AE energy attributed to thermal stress observed during cooling was higher than that to reduction degradation. These results suggest that it will be possible to eliminate the influence of crack generation within the iron ore burdens in the cooling stage by applying the in-situ non-destructive evaluation method developed in this study. It is also expected to apply for the quantitative estimation of the reduction disintegration behavior of burdens in the working BF.
- 13 April 2018
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2018-01 (14) , 1096
Terahertz Spectrum Measurement of Corrosion Products on Coated Steel Sheet Surface
Our research group has developed a terahertz light source with high luminance and broadband, and is developing research on non-destructive inspection technology. As a nondestructive inspection technology for hot-dip galvanized steel sheets, we have built a terahertz spectrum database for corrosion products that may exist there. In this research, we aim to newly obtain spectral data of β-FeOOH. Absorption Spectrum is shown in Figure.1. Optical system is shown in Figure.2. The terahertz wave was generated by difference frequency mixing using a GaP crystal which is a nonlinear optical crystal. The standard powder sample was diluted with polyethylene powder and pelletized, and it was measured at room temperature by a permeation method. As a result of spectroscopic measurement, an absorption peak was obtained around 3.06 THz. On the day of the presentation, in addition to discussions on attribution of peaks, report together with ATR-FTIR results. Figure 1
- 13 April 2018
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2018-01 (14) , 1096
Terahertz Spectrum Measurement of Corrosion Products on Coated Steel Sheet Surface
Our research group has developed a terahertz light source with high luminance and broadband, and is developing research on non-destructive inspection technology. As a nondestructive inspection technology for hot-dip galvanized steel sheets, we have built a terahertz spectrum database for corrosion products that may exist there. In this research, we aim to newly obtain spectral data of β-FeOOH. Absorption Spectrum is shown in Figure.1. Optical system is shown in Figure.2. The terahertz wave was generated by difference frequency mixing using a GaP crystal which is a nonlinear optical crystal. The standard powder sample was diluted with polyethylene powder and pelletized, and it was measured at room temperature by a permeation method. As a result of spectroscopic measurement, an absorption peak was obtained around 3.06 THz. On the day of the presentation, in addition to discussions on attribution of peaks, report together with ATR-FTIR results. Figure 1
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of the Transportation and Logistics Conference
- Vol. 2018.27, 3310
Stress Assessment of Welded Joints in Railway Bogie Frame
Railway bogie frames are commonly constructed by welding of several components. It is one of the most important points of view in the frame design that welded joints have satisfactory strength durability in their service life. The present paper focuses on welded joints with unfinished weld toes, i.e. as-weld joints, and its objective is to clarify the influence of experimental stress assessment methods. Statistic load tests were conducted on cruciform as-weld joints by using three different strain gauge attachments and finite element analyses were performed. It is clarified that a new stress assessment method, where the edge of strain gauge is attached at the weld toe, shows the smallest deviation and little dependency on the weld toe shape variations.
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of the Transportation and Logistics Conference
- Vol. 2018.27, 3310
Stress Assessment of Welded Joints in Railway Bogie Frame
Railway bogie frames are commonly constructed by welding of several components. It is one of the most important points of view in the frame design that welded joints have satisfactory strength durability in their service life. The present paper focuses on welded joints with unfinished weld toes, i.e. as-weld joints, and its objective is to clarify the influence of experimental stress assessment methods. Statistic load tests were conducted on cruciform as-weld joints by using three different strain gauge attachments and finite element analyses were performed. It is clarified that a new stress assessment method, where the edge of strain gauge is attached at the weld toe, shows the smallest deviation and little dependency on the weld toe shape variations.
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of the Materials and Mechanics Conference
- Vol. 2018, OS0831
Examination of fatigue crack propagation mechanism under cyclic Mode II loading.
Research on “Mode II fatigue crack propagation” is being conducted by many researchers. However, its understanding has not progressed as much as that of Mode I. We think that this cause is the name: “Mode II fatigue crack propagation.” Originally, Modes I and II represented the loading modes for still cracks in fracture mechanics, and not the fatigue crack propagation mechanism. There are many cases where the knowledge of fatigue crack propagation under Mode I loading is applied to that under Mode II loading without consideration. The rolling contact fatigue is a typical example of fatigue crack propagation under cyclic Mode II loading. In the region where the fatigue crack propagates, a large plastic deformation is caused by the rolling contact load. Therefore, it is necessary for the test method to reproduce the effects of an actual machine to test materials that exhibit large plastic deformation. Therefore, in this study, we aim to classify the fatigue crack propagation phenomena, regardless of Mode I and II loadings, and examine the mechanisms. To that end, we developed a novel test method that enables pure cyclic Mode II loading. We used a micro-thin film disc as a specimen, making it possible to cut out and test a part subjected to a large plastic deformation from the actual machine. By successive observation of the fatigue crack propagation behavior, we propose a crack propagation mechanism, namely, damage accumulation type fatigue crack propagation under Mode II loading, which is different from the opening type fatigue crack propagation.
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of the Materials and Mechanics Conference
- Vol. 2018, OS0831
Examination of fatigue crack propagation mechanism under cyclic Mode II loading.
Research on “Mode II fatigue crack propagation” is being conducted by many researchers. However, its understanding has not progressed as much as that of Mode I. We think that this cause is the name: “Mode II fatigue crack propagation.” Originally, Modes I and II represented the loading modes for still cracks in fracture mechanics, and not the fatigue crack propagation mechanism. There are many cases where the knowledge of fatigue crack propagation under Mode I loading is applied to that under Mode II loading without consideration. The rolling contact fatigue is a typical example of fatigue crack propagation under cyclic Mode II loading. In the region where the fatigue crack propagates, a large plastic deformation is caused by the rolling contact load. Therefore, it is necessary for the test method to reproduce the effects of an actual machine to test materials that exhibit large plastic deformation. Therefore, in this study, we aim to classify the fatigue crack propagation phenomena, regardless of Mode I and II loadings, and examine the mechanisms. To that end, we developed a novel test method that enables pure cyclic Mode II loading. We used a micro-thin film disc as a specimen, making it possible to cut out and test a part subjected to a large plastic deformation from the actual machine. By successive observation of the fatigue crack propagation behavior, we propose a crack propagation mechanism, namely, damage accumulation type fatigue crack propagation under Mode II loading, which is different from the opening type fatigue crack propagation.
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of Conference of Kyushu Branch
- Vol. 2018.71, K11
Development of Speech Production System by Pneumatic Artificial Larynx
総合学術電子ジャーナルサイト「J-STAGE」-国内で発行された学術論文全文を読むことのできる、日本最大級の総合電子ジャーナルプラットフォームです。
- 1 January 2018
- Published by Japan Society of Mechanical Engineers in The Proceedings of Conference of Kyushu Branch
- Vol. 2018.71, K11
Development of Speech Production System by Pneumatic Artificial Larynx
総合学術電子ジャーナルサイト「J-STAGE」-国内で発行された学術論文全文を読むことのできる、日本最大級の総合電子ジャーナルプラットフォームです。
- 1 January 2018
- Published by Architectural Institute of Japan in Journal of Structural and Construction Engineering (Transactions of AIJ)
- Vol. 83 (747) , 739-749
EXPERIMENTAL STUDY ON SQUARE STEEL TUBULAR COLUMNS UNDER COMPRESSIVE AXIAL FORCE WITH MONOTONIC DOUBLE CURVATURE BENDING MOMENT
In Japan, square steel tubular columns are widely used. When the building is under a seismic action, columns will be subjected to axial force with double curvature bending moment. Therefore, it is important to design the column under these combined loading in the ultimate limit state to guarantee the safety. Recommendation for Limit State Design of Steel Structure (LSD) and Recommendation for the Plastic Design of Steel Structures specify the requirements for column to guarantee sufficient strength and ductility. The plastic deformation capacity of the column that is subjected to compressive axial force with one end monotonic bending moment is ensured more than 3 by LSD. However, deformation capacity of the column that are subjected to compressive axial force with monotonic double curvature bending moment is not shown clearly. Test results that can confirm the appropriateness of LSD requirements for square steel tubular column are limited. It is necessary to gather more data of maximum strength, deformation capacity, and elasto-plastic behavior of square steel tubular columns by testing. Moreover, column that is subjected to compressive axial force is important to take into account second-order effects. In this study, testing where axial force with monotonic double curvature bending moment (end bending moment ratio equal to 0.5) are applied to the columns simultaneously are conducted. Maximum bending moment, plastic deformation capacity, and second-order effect that will be caused by Pδ moment were evaluated from the test results. Comparison between LSD requirements and test results were also shown. From the test results, followings are found. 1) Two types of collapse mechanism are confirmed. i) Local buckling occurred at one end of the column determined the ultimate state and deformation capacity. ii) Pδ moment determined the moment capacity at the loading point; increment of the bending deflection determined the ultimate state. Local buckling was not observed during the testing. 2) When the value of ny·λc02 is greater than 0.20, second-order effects determined the plastic deformation capacity. Plastic deformation capacity R of the columns that were determined by Pδ moment had a linear relation between ny·λc02. When the value of ny·λc02 is smaller than 0.17, plastic hinge was formed at the end of the column and determined the collapse mechanism. Nominal width-to-thickness ratio equals to 20.8 that was used in the testing had a plastic deformation capacity around 4.0 when it was determined by local buckling collapse. 3) Plastic deformation capacity greater than 3 were observed even if the current LSD limitation was not satisfied. However, from the point of view of collapse mechanism, LSD limitation can form a plastic hinge at the end of the column which is expected in design. 4) Even if moment amplification factor calculated by LSD is 1.0, the location of the maximum moment may appear in the middle of the column. i) ii)
- 1 January 2018
- Published by Architectural Institute of Japan in Journal of Structural and Construction Engineering (Transactions of AIJ)
- Vol. 83 (747) , 739-749
EXPERIMENTAL STUDY ON SQUARE STEEL TUBULAR COLUMNS UNDER COMPRESSIVE AXIAL FORCE WITH MONOTONIC DOUBLE CURVATURE BENDING MOMENT
In Japan, square steel tubular columns are widely used. When the building is under a seismic action, columns will be subjected to axial force with double curvature bending moment. Therefore, it is important to design the column under these combined loading in the ultimate limit state to guarantee the safety. Recommendation for Limit State Design of Steel Structure (LSD) and Recommendation for the Plastic Design of Steel Structures specify the requirements for column to guarantee sufficient strength and ductility. The plastic deformation capacity of the column that is subjected to compressive axial force with one end monotonic bending moment is ensured more than 3 by LSD. However, deformation capacity of the column that are subjected to compressive axial force with monotonic double curvature bending moment is not shown clearly. Test results that can confirm the appropriateness of LSD requirements for square steel tubular column are limited. It is necessary to gather more data of maximum strength, deformation capacity, and elasto-plastic behavior of square steel tubular columns by testing. Moreover, column that is subjected to compressive axial force is important to take into account second-order effects. In this study, testing where axial force with monotonic double curvature bending moment (end bending moment ratio equal to 0.5) are applied to the columns simultaneously are conducted. Maximum bending moment, plastic deformation capacity, and second-order effect that will be caused by Pδ moment were evaluated from the test results. Comparison between LSD requirements and test results were also shown. From the test results, followings are found. 1) Two types of collapse mechanism are confirmed. i) Local buckling occurred at one end of the column determined the ultimate state and deformation capacity. ii) Pδ moment determined the moment capacity at the loading point; increment of the bending deflection determined the ultimate state. Local buckling was not observed during the testing. 2) When the value of ny·λc02 is greater than 0.20, second-order effects determined the plastic deformation capacity. Plastic deformation capacity R of the columns that were determined by Pδ moment had a linear relation between ny·λc02. When the value of ny·λc02 is smaller than 0.17, plastic hinge was formed at the end of the column and determined the collapse mechanism. Nominal width-to-thickness ratio equals to 20.8 that was used in the testing had a plastic deformation capacity around 4.0 when it was determined by local buckling collapse. 3) Plastic deformation capacity greater than 3 were observed even if the current LSD limitation was not satisfied. However, from the point of view of collapse mechanism, LSD limitation can form a plastic hinge at the end of the column which is expected in design. 4) Even if moment amplification factor calculated by LSD is 1.0, the location of the maximum moment may appear in the middle of the column. i) ii)