Abstract
In an effort to achieve the goal of carbon neutrality, countries around the world are aiming to phase out coal-fired power plants. Due to various reasons, electricity production through coal-fired power generation and sulfur oxide (SOx) emissions are expected to continue in the future. In the South Korea, sodium bicarbonate (NaHCO 3) and lime materials are used to treat SOx, and most of the sodium bicarbonate is imported. Therefore, this research was conducted to replace sodium bicarbonate by improving the physical properties of lime materials using domestic limestone. Limestone was heat-treated through a box-type electric furnace and a vertical electric furnace. Due to the structural characteristics of the vertical electric furnace, a lime material(quicklime) was possible to improve the physical properties like a specific surface area and a pore volume. Then, they were reached to 22.33 m 2 /g specific area and 0.14 cc/g pore volume.