Hydroxyapatite-calcium carbonate ceramic composite materials

Authors:

Abstract
Hydroxyapatite/calcium carbonate (CC) composite powders containing up to 50 wt % CO 3 2− , have been prepared via precipitation from aqueous solutions. According to chemical analysis data, the CO 3 2− content of the powders coincides with the intended one over the entire composition range studied. With increasing CO 3 2− content, the specific surface area of the powders decreases because of the formation and growth of large needlelike CC crystals up to 1.5 μm in size. The addition of low-melting-point alkali carbonates to the starting powder mixture reduces the sintering temperature of the powders to below 720°C, thereby preventing the thermal decomposition of CC. The highest bending strength, up to 76 MPa, is offered by the materials with the lowest CC content, about 20 wt %, and an average crystal size of 100 nm. The solubility of the composites gradually increases with CC content. In vitro experiments with a human fibroblast model (MTT test) demonstrate that the composites have zero cytotoxicity.