Abstract
The Mo-40wt.%Cu pseudo-alloy, prized for thermal conductivity and electrical performance, is used as heat sinks for high-density integrated circuits and power semiconductors, ultrahigh-voltage electric contact materials in heavy-duty switches, circuit breakers and electrodes, blocking materials in microwave packages, substrates for radar transistors and MEMS sensors. The oxidation behavior of the Mo-40wt.%Cu alloy was investigated at 450–550 °C in air, revealing a two-stage process comprising initial catastrophic oxidation caused by a liquid phase formation in the oxide scale followed by self-passivation. Thermogravimetric analysis demonstrated parabolic kinetics during the catastrophic stage, governed by diffusion-controlled mechanisms, with parabolic rate constant increasing from 0.5·10⁻⁵ to 2.6·10⁻⁵ kg² m⁻⁴ s⁻¹ as temperature rose from 480 to 520 °C (three orders of magnitude higher than the constant of pure copper oxidation 2.5·10⁻8 kg² m⁻⁴ s⁻¹ at 500°C). Subsequent passivation led to a marked reduction in oxidation rate, culminating in a mass-gain plateau. X-ray diffraction and scanning electron microscopy with energy-dispersive X-ray spectroscopy elucidated the formation of a two-layered oxide scale: an inner layer of copper molybdates (CuMoO₄, Cu₃Mo₂O₉, Cu₃.₈₅Mo₃O₁₂, Cu₆Mo₅O₁₈) and an outer dense CuO layer after the passivation begins. This CuO layer upon achieving continuity, exhibiting low ionic conductivity, impedes both copper cation and oxygen anion diffusion, thereby arresting further oxidation. Unlike the MoO₃-deposit induced catastrophic oxidation of copper, this self-passivation mechanism in the Mo-40wt.%Cu alloy offers insights into designing a technology to protect pseudo-alloys from catastrophic oxidation.

This publication has 20 references indexed in Scilit: