Degradation of the Ceramics Based on MgO, Al2O3, or Si3N4 in the LiCl–KCl Melt with (Ce,Nd,U)Cl3 Additives
Authors:
- 1 February 2021
- journal article
- research article
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2021 (2) , 224-228
Abstract
The degradation of the ceramic materials based on magnesium oxide, aluminum oxide, or silicon nitride in the LiCl–KCl melt containing uranium, cerium, or neodymium trichloride of various concentrations is studied in the temperature range 470–650°C. Gravimetric, chemical–analytical, electron-probe microanalysis, and X-ray diffraction techniques are used. All ceramic materials are shown to be chemically resistant in the given melts. The porosity of the ceramics plays an important role in the choice of materials for structural elements. The higher the porosity, the larger the increase in the sample mass after an experiment. The mass increment increases with the temperature. The ceramics based on magnesium oxide reacts with aluminum oxide to form magnesium aluminate, which does not allow them to be used together. The best results are shown by the ceramics based on silicon nitride, since it is low-porous and chemically stable. The addition of cerium or neodymium trichloride to the melt weakly affects the ceramics under study.Keywords
This publication has 5 references indexed in Scilit:
- Investigation of the Structure of Si3N4-Based Ceramic with Al2O3 and Y2O3 AdditivesGlass and Ceramics, 2014
- Silicon Nitride Ceramics for Product and Process InnovationsAdvances in Science and Technology, 2010
- Ceramics1999
- Silicon nitride: synthesis and propertiesRussian Chemical Reviews, 1995
- Lifetime predictions for a ceramic cutting tool material at high temperaturesJournal of Materials Science, 1987