Abstract
This study investigates the feasibility of processing stale copper-nickel ore dressing tailings to recover non-ferrous metals and produce iron sulfate crystal hydrates. A method of heap bioleaching of pre-granulated tailings was proposed for the recovery of non-ferrous metals. The binding agents used for granulation were a 30 % sulfuric acid solution, a bacterial solution of Acidithiobacillus ferrooxidans, and polyvinyl acetate (PVA) glue. The results showed an inverse relationship between pellet strength and metal recovery efficiency. The highest metal concentrations during the heap bioleaching stage were observed in pellets prepared using sulfuric acid. To obtain iron sulfate crystal hydrates, sulfuric acid leaching of the ore dressing tailings (both as-received and ground to -71 µm) was conducted under static conditions at a temperature of ~22 °C. This selected regime yielded crystal hydrates of ferrous sulfate—rozenite and melanterite.