Improved hardness and wear resistance in B 4 C–SiC–TiC reinforced AA6061 composites produced by powder metallurgy: A comparative study of monolithic and hybrid structures
Author:
- 22 August 2025
- journal article
- Published by SAGE Publications in Journal of Composite Materials
- Vol. 59 (30) , 3431-3452
Abstract
Aluminium matrix composites (AMCs) are increasingly used in wear-critical applications, yet improving their mechanical and tribological properties remains a key challenge. This study addresses this gap by investigating the effects of different ceramic reinforcements—silicon carbide (SiC), boron carbide (B 4 C), and titanium carbide (TiC)—on the microstructure, hardness, and wear behaviour of AA6061-based monolithic and hybrid composites. The composites were fabricated using the powder metallurgy method, followed by compaction and sintering. Microstructural analysis revealed a uniform distribution of reinforcements and good interfacial bonding. The results showed that increasing the reinforcement ratio significantly enhanced hardness, with B 4 C providing the greatest improvement due to its high thermal stability and strong bonding characteristics. The AA6061/B 4 C monolithic composite exhibited an 85.7% increase in hardness, while the AA6061/SiC/B 4 C hybrid composite showed a 101.2% increase. Similarly, wear resistance improved by 46% and 47% for the B 4 C and B 4 C + SiC reinforced composites, respectively, due to the synergistic reinforcement effect. All samples showed successful densification, with relative densities between 92% and 97%, and porosity ranging from 3% to 8%. The coefficient of friction remained stable (0.1–0.2) across all samples. These findings demonstrate that B 4 C, especially when combined with SiC, is a highly effective reinforcement strategy for enhancing the performance of AA6061 matrix composites.Keywords
This publication has 53 references indexed in Scilit:
- Effect of SiC Particle Size on the Mechanical and Wear Behavior of Al356 Metal Matrix CompositesSilicon, 2023
- Optimizing the Wear Behaviour of AA7178 Metal Matrix Composites Reinforced with SiC and TiO2 Nanoparticles: A Comparative Study Using Evolutionary and Statistical MethodsSilicon, 2023
- Mechanical Characteristics and Wear Behaviour of Al/SiC and Al/SiC/B4C Hybrid Metal Matrix Composites Fabricated Through Powder Metallurgy RouteSilicon, 2023
- The Effect of Hot Rolling Temperature on the Wear Properties of NiTi RodsTransactions of the Indian Institute of Metals, 2022
- Structural, Mechanical, and Electrical Behavior of Ceramic-Reinforced Copper Metal Matrix Hybrid CompositesJournal of Materials Engineering and Performance, 2019
- Composite Materials2019
- Effect of Production Route on the Microstructure and Mechanical Properties of Cu–SiC $_{\mathrm{p}}$ p CompositesArabian Journal for Science and Engineering, 2018
- Synthesis of Copper Metal Matrix Hybrid Composites Using Stir Casting Technique and Its Mechanical, Optical and Electrical BehavioursTransactions of the Indian Institute of Metals, 2017
- EDM of hybrid Al–SiCp–B4Cp and Al–SiCp–Glassp MMCsThe International Journal of Advanced Manufacturing Technology, 2009
- Aluminium matrix composites: Challenges and opportunitiesSādhanā, 2003