Lithium ion battery usage has grown significantly in recent years. To obtain the best from the li-ion battery technology, it is important to understand both advantages and the limitations from the fundamental point of view. In lithium-ion batteries, layer structured graphite is the most commonly used anode material and NMC is one of the modern choices of cathode materials for high capacity Li-ion batteries in the electric vehicle applications [1,2,3]. During the first charging process, the electrochemical reduction of electrolyte components gets deposited on the surface of anode resulting solid electrolyte interface (SEI) layer formation [4,5,6]. It is widely accepted that the batteries benefit from a proper SEI formation, as it can improve their lifetime, cycle life, power capability and safety [7]. Morphological structure of SEI layer formed on HOPG and cathode electrolyte interface (CEI) layer formed on NMC plays an important role in lithium-ion battery (LIB), particularly for its cyclability and safety. For the development of high-performance LIB’s, it is crucial to understand the SEI layer formation on anode side [8] and the less studied corresponding layer formed on cathode side termed as CEI, whose composition and role are debated [9]. Microscopic techniques, which include scanning tunneling microscopy (STM) and atomic force microscopy (AFM) are the most powerful tools to measure the electric current and surface topography [10,11]. Within this work, we present in-situ electrochemical atomic force microscopic (EC-AFM) studies of surface reaction and topographic evolution of SEI and CEI layers formed on HOPG and NMC811 substrates. EC-AFM morphological analysis is also complemented with XPS (X-ray Photoemission Spectroscopy) characterisation for elemental composition, which brings a new insight in the comparison of SEI/CEI decomposition products. Acknowledgements: This work is partially supported by Faraday Institution (EP/S003053/1) and North-East Centre of Energy Materials-NECEM (EP/R021503/1) funded by EPSRC. References: [1] H. Sun and K. Zhao, J Physical Chem C, 2017, 121, 6002-6010. [2] S. Bak, E. Hu, Y.Zhou, X.Yu, S.D. Senanayake, S. Cho, K. Kim, K.Y. Chung, X. Q. Yang and K. W. Nam, ACS Applied Materials &Interfaces, 2014, 6, 22594-22601. [3] P. Rozier and J. M. Tarascon, J Electrochem. Soc, 2015, 162, A2490-A2499. [4] L.Seidl, S.Martens, J. Ma, U.Stimming and O.Schneider, Nanoscale,2016, 8, 14004. [5] D.Xin, L.XingRui, Y. Huijuan,W.Dong and W.Lijun, Chem. Methodol,2014,57,178-183. [6] M.Steinhauer, M.Stich, M. Kurniawan, B.K. Seidlhofer, M.Trapp, A. Bund, N.wagner and K.A.Friedrich, ACS Appl.Mater.Interfaces, 2017,9,35794-35801. [7] P.B. Balbuena and Y.Wang, Lithium-ion batteries solid-electrolyte interface, imperial college press,2004. [8] V. A. Agubra, J. W. Fergus, J. Power Sources, 2014, 268, 153−162. [9] L. Yao-min, G.N. Bruno, L. E. Jennifer, A.G. Andrew, J. Anal.Chem,2016,88,7171-7177. [10] C. Shen, M. Buck, Beilstein J. Nanotechnol, 2014, 5, 258−267. [11] C. Shen, I. Cebula, C. Brown, J. L. Zhao, M. Zharnikov, M. Buck, Chem. Sci, 2012, 3, 1858−1865. Figure 1