Impact of Intensity of Residual Stress Field Upon Reyielding and Re-Autofrettage of an Autofrettaged Thick Cylinder
- 9 July 2012
- journal article
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 134 (4) , 041003
Abstract
Re-autofrettage has been identified as a significant, cost-effective method to achieve higher reyield pressure (RYP) and/or weight reduction in large caliber gun tubes. For a given overstrain, residual stress profiles for hydraulic and swage autofrettage may differ significantly in their intensity. The simplest representation of this “intensity” effect is the magnitude of the bending moment “locked in” via the residual hoop stress. Hill’s analytical, plane strain, Von Mises analysis predicts a larger “locked-in” moment than does the equivalent open-end condition. By assuming a range of stress-field intensities (f) scaling from 1.0 to 1.4 times that were produced by open-end hydraulic autofrettage, it was possible to assess reyield behavior following initial autofrettage via a generic numerical study. In cases where Bauschinger effect is absent, reyield initiates at the original elastic–plastic interface. This includes the ideal Hill distribution. When Bauschinger effect is present, reyield for initiates at the bore and after further pressurization at the original elastic–plastic interface within two zones. For , the reverse is the case, with initial yield at the original elastic–plastic interface and subsequently at the bore. RYP increases with increasing f up to f = 1.175 and then decreases significantly. This loss of RYP may be mitigated by hydraulic re-autofrettage. At f = 1.0 re-autofrettage increases RYP by 4%. At f = 1.4, RYP is increased by 19%. There are modest increases in safe maximum pressure (SMP) as a result of re-autofrettage. RYP closely approaching re-autofrettage pressure is achievable for . Within this range, re-autofrettage offers a significant benefit. Re-autofrettage also produces beneficial effects via increased bore hoop compressive stress, this increase varying from 20% for f = 1% to 0% for f = 1.4. Such increased compression will benefit fatigue lifetime for fatigue cracks initiating at the bore. Conversely, tensile outside diameter (OD) hoop stress increases, with increasing f, by a maximum of 6%.
Keywords
This publication has 12 references indexed in Scilit:
- Hydraulic Re-Autofrettage of a Swage Autofrettaged Tube2009
- 3D Finite Element Modeling of the Swage Autofrettage Process Including the Bauschinger Effect2007
- Hill Stress Calculations for Autofrettaged Tubes Compared With Neutron Diffraction Residual Stresses and Measured Yield Pressure and Fatigue Life2007
- An Improved Method for Recovering Residual Stress From Strain Measurements in Cylinders and Rings2006
- A Re-Autofrettage Procedure for Mitigation of Bauschinger Effect in Thick CylindersJournal of Pressure Vessel Technology, 2004
- Experimental Data, Numerical Fit and Fatigue Life Calculations Relating to the Bauschinger Effect in High Strength Armament SteelsJournal of Pressure Vessel Technology, 2003
- Characterization of Steels Using a Revised Kinematic Hardening Model Incorporating Bauschinger EffectJournal of Pressure Vessel Technology, 2003
- Autofrettage of Open-End Tubes—Pressures, Stresses, Strains, and Code ComparisonsJournal of Pressure Vessel Technology, 2000
- Stress Intensity and Fatigue Crack Growth in a Pressurized, Autofrettaged Thick Cylinder1983
- Technical note: On the equivalence of axisymmetric bending, thermal, and autofrettage residual stress fieldsThe Journal of Strain Analysis for Engineering Design, 1980