Preparation of Aluminum Nitride–Silicon Carbide Nanocomposite Powder by the Nitridation of Aluminum Silicon Carbide

Authors:

Abstract
Aluminum nitride (AlN)–silicon carbide (SiC) nanocomposite powders were prepared by the nitridation of aluminum‐silicon carbide (Al 4 SiC 4 ) with the specific surface area of 15.5 m 2 ·g −1 . The powders nitrided at and above 1400°C for 3 h contained the 2H‐phases which consisted of AlN‐rich and SiC‐rich phases. The formation of homogeneous solid solution proceeded with increasing nitridation temperature from 1400° up to 1500°C. The specific surface area of the AlN–SiC powder nitrided at 1500°C for 3 h was 19.5 m 2 ·g −1 , whereas the primary particle size (assuming spherical particles) was estimated to be ∼100 nm.

This publication has 16 references indexed in Scilit: