Comparison of Physicochemical, Binding, and Antibacterial Properties of Chitosans Prepared without and with Deproteinization Process
Authors:
- 20 November 2003
- journal article
- research article
- Published by American Chemical Society (ACS) in Journal of Agricultural and Food Chemistry
- Vol. 51 (26) , 7659-7663
Abstract
Physicochemical, binding, and antibacterial properties of chitosans prepared without and with deproteinization (DP) process (5, 10, 15, and 30 min at 15 psi/121 °C) were compared. Chitosan from DP 0 min had comparable nitrogen content, lower degree of deacetylation and solubility, but higher molecular weight and viscosity than chitosans from DP 5−30 min. The latter four chitosans showed differences only in molecular weight. Deproteinization treatment resulted in slightly decreased L* values and increased a* and b* values compared with those of DP 0 min. Chitosan from DP 0 min had comparable water and fat-binding capacity (FBC) except for chitosan from DP 15 min, which had a higher FBC but lower dye-binding capacity than those of the four chitosans from DP 5−30 min. The antibacterial activities of chitosans against seven different bacteria showed that the inhibitory effects varied with the deproteinization time and the particular bacterium. Keywords: Chitosan; deproteinization; physicochemical characteristics; binding capacity; antibacterial activityKeywords
This publication has 6 references indexed in Scilit:
- Antibacterial action of chitosanFood Biotechnology, 1992
- Growth-inhibitory effect of hexa-N-acetylchitohexaose and chitohexaose against Meth-A solid tumor.Chemical and Pharmaceutical Bulletin, 1988
- Functional Properties of Chitin and ChitosanJournal of Food Science, 1982
- Formation of spherical chitosan biocatalysts by ionotropic gelationBiotechnology Letters, 1981
- A conductometric method for colloid titrationsAnalytica Chimica Acta, 1976
- The analysis of p-nitrophenyl diethyl thiophosphate, E605, parathionThe Analyst, 1950