Residual tensile strength monitoring of drilled composite materials by acoustic emission
Authors:
- Navid Zarif KarimiNKNavid Zarif Karimi
- Hossein HeidaryHHHossein Heidary
- Mehdi AhmadiMAMehdi Ahmadi
- 1 September 2012
- journal article
- Published by Elsevier in Materials & Design (1980-2015)
- Vol. 40, 229-236
Abstract
No abstract availableThis publication has 24 references indexed in Scilit:
- An integrated approach based on acoustic emission and mechanical information to evaluate the delamination fracture toughness at mode I in composite laminateMaterials & Design (1980-2015), 2011
- Taguchi analysis of the residual tensile strength after drilling in glass fiber reinforced epoxy compositesMaterials & Design (1980-2015), 2009
- Delamination analysis in drilling process of glass fiber reinforced plastic (GFRP) composite materialsJournal of Materials Processing Technology, 2007
- Effects of special drill bits on drilling-induced delamination of composite materialsInternational Journal of Machine Tools and Manufacture, 2006
- Workpiece damping and its effect on delamination damage in drilling thin composite laminatesJournal of Materials Processing Technology, 2004
- Study of delamination in drilling carbon fiber reinforced plastics (CFRP) using design experimentsComposite Structures, 2003
- An approach for development of damage-free drilling of carbon fiber reinforced thermosetsInternational Journal of Machine Tools and Manufacture, 2001
- Application of acoustic emission in drilling of composite laminatesNDT & E International, 2000
- Effects of hole machining defects on strength and fatigue life of composite laminatesComposites Part A: Applied Science and Manufacturing, 1997
- Effect of drilling parameters on the finish and mechanical properties of GFRP compositesInternational Journal of Machine Tools and Manufacture, 1990