Abstract
This study examines how pulsed-energy timing and spacing are associated with weld geometry, tensile response, and modelled thermal history in 2-mm-thick 4J50 butt joints. Four conditions were welded at a nominal average power of 227.5 W and compared with a three-dimensional transient thermal model. The A–B and C–D pairs hold nominal frequency and pulse duration fixed while changing travel speed; these changes also alter line energy and pulse spacing. Cases A and D share a nominal peak power of about 3.79 kW and a line energy of 22.75 J/mm, yet the measured penetration depth in D is 2.33 times that in A. Across the four calibration conditions, the mean absolute differences between the simulated segment means and the measured values were 0.050 mm for penetration depth and 0.064 mm for weld width. With one tensile specimen tested per condition, peak nominal stress followed the same rank order as measured penetration depth. These results highlight the coupled roles of pulse energy, duration, spacing, and off-time in weld formation.
Funding Information
  • Guizhou Province Science and Technology Planning Project (Qianke He Jichu ZK [2023] Yiban 134)
  • Guizhou Province Science and Technology Planning Project (Qianke He Zhicheng ZK [2024] Yiban182)
  • Guizhou Province Science and Technology Planning Project (Qianke He Pingtai JSZK [2025] 015)
  • Major Science and Technology Special Project of Guizhou province (Qiankehe Rencai XKBF [2025] 008)

This publication has 29 references indexed in Scilit: