Photodegradation of rigid PVC formulations. I. Wavelength sensitivity to light‐induced yellowing by monochromatic light

Authors:

Abstract
Light‐induced yellowing of extruded rigid poly(vinyl chloride) formulations containing 0, 2.5, and 5 phr of titanium dioxide under exposure to monochromatic light was studied. Both photoyellowing and photobleaching were observed as wavelength‐dependent phenomena in the range of 280–500 nm. Action spectra for yellowing of the different compounds were similar. In the case of the formulation with no titanium dioxide, significant color changes were observed on the back surface of the sample, indicating transmission of the longer wavelength light through the 1‐mm thickness of the sample.

This publication has 34 references indexed in Scilit: