Crystallization Behavior of CaO–P 2 O 5 Glass with TiO 2 , SiO 2 , and Al 2 O 3 Additions

Authors:

Abstract
TiO 2 above 4 mol% is an effective nucleating agent for CaO–P 2 O 5 glass which also contains substantial SiO 2 and Al 2 O 3 additions. Glass ceramics can be made from this glass using a single slow heating ramp with no need for a nucleating heat treatment step. Powder of this composition crystallizes rapidly to β‐Ca 2 P 2 O 7 , whereas bulk glass crystallizes from diphasic nuclei consisting of a central cubic Ca‐P‐Ti‐Si‐Al oxide phase surrounded by impure AlPO 4 dendrites. Metastable calcium phosphate grows on the AlPO 4 dendrites and later transforms to β‐Ca 2 P 2 O 7 .

This publication has 13 references indexed in Scilit: