Enhanced Energy Storage and Suppressed Dielectric Loss in Oxide Core–Shell–Polyolefin Nanocomposites by Moderating Internal Surface Area and Increasing Shell Thickness
- 27 August 2012
- journal article
- research article
- Published by Wiley in Advanced Materials
- Vol. 24 (44) , 5946-5953
Abstract
Dielectric loss in metal oxide core/Al2O3 shell polypropylene nanocomposites scales with the particle surface area. By moderating the interfacial surface area between the phases and using increasing shell thicknesses, dielectric loss is significantly reduced, and thus the energy stored within, and recoverable from, capacitors fabricated from these materials is significantly increased, to as high as 2.05 J/cm3.Keywords
This publication has 79 references indexed in Scilit:
- Studies of dielectric relaxation in natural fiber–polymer compositesJournal of Electrostatics, 2009
- High‐Energy Density Capacitors Utilizing 0.7 BaTiO 3 –0.3 BiScO 3 CeramicsJournal of the American Ceramic Society, 2009
- Significantly enhanced low-frequency dielectric permittivity in the BaTiO3/poly(vinylidene fluoride) nanocompositeApplied Physics Letters, 2007
- Introduction: PolymerizationProceedings of the National Academy of Sciences, 2006
- Preparation and electrochemical characteristics of LiNi1/3Mn1/3Co1/3O2 coated with metal oxides coatingJournal of Power Sources, 2006
- Polymer nanocomposite dielectrics - the role of the interfaceIEEE Transactions on Dielectrics and Electrical Insulation, 2005
- Zirconium Hydrocarbyl Chemisorption on Sulfated Metal Oxides: New Supports, Chemisorption Pathways, and Implications for CatalysisLangmuir, 2004
- Sulfated Tin Oxide Nanoparticles as Supports for Molecule-Based Olefin Polymerization CatalystsNano Letters, 2004
- Transport Properties of Random Media: A New Effective Medium TheoryPhysical Review Letters, 1995
- Percolation threshold and interface optimization in a HUP/C doublelayer supercapacitorJournal of Materials Science Letters, 1986