Abstract
The microstructure and mechanical properties of the Ti-43.7Al-3.2(Nb,Cr,Mo)-0.2B alloy in the as-cast state (after gasostatistic processing) and of the Ti-45Al-8Nb-0.2C alloy after hot extrusion at temperatures corresponding to the α + γ phase field followed by heat treatment have been studied. The extruded heavy-alloyed alloy has demonstrated significantly higher plastic/mechanical properties at room temperature with close values of the plasticity/tensile strength and long-term strength at elevated temperatures. A comparison of the results with literature data has shown the properties of the as-cast Ti-43.7Al-3.2(Nb,Cr,Mo)-0.2B to be similar to or superior to those of the best-known casting γ (TiAl) + α2 (Ti3Al) alloys.

This publication has 14 references indexed in Scilit: