Abstract
The intrinsic brittleness of GeTe-based thermoelectric materials limits their mechanical reliability. SiC whiskers were introduced into a GeTe-based thermoelectric matrix for the first time as a reinforcing secondary phase. Ge0.9Sb0.1Te was used as the matrix, and two whisker geometries were combined with dry and ethanol-assisted ball milling to examine their effects on the post-milling whisker state, microstructure, thermoelectric transport, and mechanical response. Ethanol-assisted milling retained longer whisker segments in both whisker systems, although the coarse- and fine-whisker composites exhibited different microstructural and property responses. Increasing the SiC whisker content did not produce a monotonic improvement in thermoelectric performance. Among the ethanol-milled coarse-whisker composites, the 0.5 vol% sample showed a favorable balance between electrical and thermal transport and reached a ZT of approximately 2.04 at 773 K. By contrast, the corresponding fine-whisker composite showed a greater mechanical improvement, with a flexural strength of 50.7 MPa and a fracture toughness of 1.60 MPa m1/2. Fracture-surface observations revealed whisker pullout, crack bridging, and crack deflection, consistent with increased resistance to crack propagation. The results indicate that whisker retention alone does not determine the overall performance of the composites. Processing conditions that favor thermoelectric transport are therefore not necessarily those that provide the greatest mechanical reinforcement.

This publication has 21 references indexed in Scilit: