Abstract
Reducing the environmental impact is a key reason for developing recyclable insulation materials for high-voltage industries. In this study, polypropylene (PP) blends were prepared via melt mixing with styrene–ethylene–butylene–styrene (SEBS), a thermoplastic elastomer, to improve breakdown strengths at various cooling speeds. A systematic investigation was conducted to evaluate the influence of crystal size, degree of crystallinity, and nucleation growth rate on the breakdown strength. Crystallization behavior was analyzed using isothermal and non-isothermal methods based on the Avrami model. Increasing SEBS content reduced crystallinity, with the lowest nucleation growth rate observed at 35% SEBS. Breakdown strength correlated with crystallization behavior and was further validated by Weibull distribution method. Notably, PP/SEBS blends containing 35% SEBS exhibited the highest breakdown strength of 66.4 kV/mm at a cooling speed of 10 °C/mm. This improvement reflected a reduction in the degree of crystallinity from 36.0% to 22.9% and the lowest growth rate constant (k) at 35% SEBS. Furthermore, the predicted lifetime of PP/SEBS blend containing 35% SEBS, calculated using the oxidation induction time and the Arrhenius equation, was 42 years. These findings demonstrate that SEBS content and cooling rate effectively modulate crystallization and breakdown strength, enabling recyclable PP/SEBS with XLPE-comparable performance for sustainable high-voltage insulation.Keywords
This publication has 36 references indexed in Scilit:
- Comparison for Accelerated Degradation of New and Old 6.6 kV AC XLPE CablesJournal of Electrical Engineering & Technology, 2024
- Insight into the stabilization activity of n-SiO2 powder in SEBS phaseJournal of Thermal Analysis and Calorimetry, 2024
- Fabrication and toughening mechanism of high toughness PP/SEBS/HDPE blends with core‐shell particlesJournal of Polymer Science, 2023
- Structure–properties correlations in compatibilized polyamide/thermoplastic elastomer/nanoclay mixtures: interrelationship among non-isothermal crystallization kinetics, morphology and viscoelastic responsesJournal of Thermal Analysis and Calorimetry, 2023
- Crystallization kinetics of compatibilized blends of polypropylene and polyethylenimineJournal of Thermal Analysis and Calorimetry, 2021
- High flow polypropylene/SEBS composites reinforced with differently treated hemp fibers for injection molded partsComposites Part B: Engineering, 2019
- Dynamically vulcanized PP/EPDM blends with balanced stiffness and toughness via in-situ compatibilization of MAA and excess ZnO nanoparticles: Preparation, structure and propertiesComposites Part B: Engineering, 2019
- Crystallization, mechanical, and electromagnetic properties of conductive polypropylene/SEBS compositesJournal of Polymer Research, 2016
- An investigation of the potential of ethylene vinyl acetate/polyethylene blends for use in recyclable high voltage cable insulation systemsJournal of Materials Science, 2010
- Use of Monomethyl Itaconate Grafted Poly(propylene) (PP) and Ethylene Propylene Rubber (EPR) as Compatibilizers for PP/EPR BlendsMacromolecular Materials and Engineering, 2003