Abstract
Preparing for the laminated magnetic core of racetrack inductors is complicated. To make matters worse, in order to ensure that a closed magnetic path is formed, core wings are introduced to ensure the top core overlaps the bottom core. However, these wings generate excess eddy current losses. In addition, the width of the devices is also increased, and so does the overall footprint. In this paper, a sequential electro-deposition of metal-polymer process has been developed to fabricate laminated magnetic core for flexible printed circuit board (PCB) integrated inductors. We analyze the influence of conductivity and thickness of the insulating layer on eddy current loss of the laminated core by finite element simulation, and select a 5 μm PEDOT as the insulating layer of the prepared NiFe/PEDOT/NiFe laminated core. Furthermore, an integrated forming process is adopted to simplify the preparation of the three-dimensional magnetic core of racetrack inductors, which remove the core wings. Combining these processes, a racetrack inductor with a wingless laminated core is fabricated and characterized. Compared with the single-layer core with core wings, given the same total thickness, the wingless laminated core improves the retention rate of normalized inductance from 80.6% to 93.1% at 10 MHz, and has a peak quality factor of 13.3 at 5 MHz.
Funding Information
  • Zhejiang Provincial Natural Science Foundation (LD21F040001)

This publication has 24 references indexed in Scilit: