Abstract
LiBH4 exhibits lithium superionic conduction accompanied by structural transition at around 390 K. Addition of LiCl to LiBH4 drastically affects both the transition and electrical conductivity: Transition from low-temperature (LT) to high-temperature (HT) phases in LiBH4 is observed at 370 K upon heating and the HT phase can be retained at 350–330 K upon cooling. Further, the conductivity in the LT phase is more than one or two orders of magnitude higher than that of pure LiBH4 . These properties could be attributed to the dissolution of LiCl into LiBH4 , suggested by in situ x-ray diffraction measurement.