Abstract
In this study, the sulfur resistance and thermal regeneration of a series of MOx-WO3/TiO2 (denoted as MW/Ti, M=Fe, Mn, Cu, V) catalysts were investigated. After in situ sulfur poisoning, the SCR activity of the poisoned catalysts was inhibited at low temperatures but was promoted at high temperatures. After thermal regeneration, FeW/Ti catalyst was more thoroughly regenerated among non-vanadium based catalysts. To investigate the impacts of sulfur poisoning, characterizations including XRD, TGA, H2-TPR, and SO2-TPD were applied. It was discovered that different sulfur-containing species blocked the adsorption of NH3/ NO to a distinct extent over all of the catalysts, thus affecting the catalytic activity. The effect depends on which are dominant (NO or NH3) during the reaction at different temperatures. The difference in regeneration depends on the formation of sulfates species. The ratio of Mx(SO4)y to NH4HSO4 generated on the catalysts was adopted to assess the possibility of regeneration. The ratios were 0.5, 1.4, 1.5, 1.7 for VW/Ti, FeW/Ti, CuW/Ti and MnW/Ti catalysts, respectively. The lower the ratio was, the easier the catalyst could be regenerated. Meanwhile, the sulfate species could be decomposed more easily on the poisoned FeW/Ti catalyst. FeW/Ti is an excellent candidate for low and medium-temperature NH3-SCR among non-vanadium based catalysts.
Funding Information
  • Ministry of Science and Technology of the People's Republic of China (2016YFC0203900, 2016YFC0203901)
  • National Natural Science Foundation of China (51778619, 51938014)

This publication has 72 references indexed in Scilit: