Abstract
Iron-loaded granular activated carbon (Fe-GAC) was prepared, characterized, and its performance as a catalyst in the Fenton oxidation of tetracycline (TC) was compared with that of carbon grains without iron supplementation. The characterization results revealed that the Fe 2+ was successfully introduced onto the original granular activated carbon (GAC) and diversified the surface morphology and elemental compounds of materials. Adsorption tests confirmed that the adsorption of TC on both materials can be described using pseudo-second-order kinetic model and Langmuir isotherm model. The response characteristics and influencing factors of degradation of TC in two systems were evaluated. TC removal over 60min at pH 3 was 89.5% for the GAC/Fenton system and 92.6% for the Fe-GAC/Fenton system.Moreover, the Fe-GAC/Fenton system displayed a lower Fe 2+ dosage than that of GAC/Fenton (an Fe 2+ /H 2 O 2 molar ratio of 0.04:1 versus 0.007:1). Excitation-emission matrix fluorescence spectroscopy showed that Fe-GAC/Fenton system delivered better mineralization, at least with TC. Fourteen intermediates were detected using quadrupole time-of-flight liquid chromatography coupled with mass system, and three possible degradation pathways for TC are proposed. Catalyst regeneration treatments was evaluated over six cycles. The regeneration was 6.5% more effective with the iron-supplemented carbon granules.

This publication has 29 references indexed in Scilit: