Abstract
The present study evaluated the biodegradability of biopolymers produced from cassava starch ( Manihot esculenta ) reinforced with lignocellulosic particles from cocoa pod husks ( Theobroma cacao L.). The biopolymers were manufactured by thermocompression, incorporating 0%, 5%, 10%, and 15% cocoa husk content. Mechanical properties were determined through tensile tests (ASTM D‐638), and biodegradability was assessed under controlled composting conditions (ASTM D5338‐15) using a respirometric system to quantify CO 2 release. The results showed that the addition of cocoa particles significantly improved the mechanical properties, reaching maximum values in the formulation with 10% content (T2), with a tensile strength of 1.95 MPa and an elastic modulus of 51.88 MPa. Regarding biodegradation, T2 achieved 18.43% biodegradation after 42 days. Comparative bibliographic analysis confirms that composting accelerates degradation compared to soil burial and that material composition influences the kinetics of the process.
Funding Information
  • Universidad Científica del Sur (454-2019-PRE11)

This publication has 30 references indexed in Scilit: