Thermal shock behaviour of unidirectional silicon carbide fibre reinforced calcium aluminosilicate
Authors:
- 1 January 1997
- journal article
- Published by Springer Nature in Journal of Materials Science
- Vol. 32 (2) , 317-325
Abstract
No abstract availableKeywords
This publication has 29 references indexed in Scilit:
- Methodology for the determination of the interfacial properties of brittle matrix compositesJournal of Materials Science, 1994
- Thermal shock resistance of SiC fibrerein-forced borosilicate glass and lithium aluminosilicate matrix compositesJournal of Materials Science, 1993
- Stability of interfaces in calcium aluminosilicate matrix/Nicalon SiC fibre compositesJournal of Materials Science Letters, 1993
- Inhibition of intermediate temperature degradation of calcium aluminosilicate/Nicalon by high temperature pretreatmentJournal of Materials Science Letters, 1993
- Interface characterization and fracture of calcium aluminosilicate glass-ceramic reinforced with nicalon fibresJournal of Materials Science, 1992
- Behaviour of unidirectional and crossply ceramic matrix composites under quasi-static tensile loadingJournal of Materials Science, 1992
- Structure and chemistry of fibre-matrix interfaces in silicon carbide fibre-reinforced glass-ceramic composites: an electron microscopy studyJournal of Materials Science, 1987
- Silicon carbide fibre reinforced glass-ceramic matrix composites exhibiting high strength and toughnessJournal of Materials Science, 1982
- Effect of bath and specimen temperature on the thermal stress resistance of brittle ceramics subjected to thermal quenchingJournal of Materials Science, 1981
- Approximate stress intensity factor for an embedded elliptical crack near two parallel free surfacesInternational Journal of Fracture, 1965