Diffusible hydrogen content in submerged arc welds of a S960 type steel
Author:
- 23 May 2016
- journal article
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 58 (6) , 561-568
Abstract
Hydrogen induced damage is a dangerous phenomenon affecting the weld quality with regard to construction service life even without visible indication. The determination of diffusible hydrogen in weld metal has been standardized at an international level in ISO 3690:2012. This international standard specifies the sampling and analytical procedure for the determination of diffusible hydrogen in martensitic, bainitic and ferritic steel weld metal which arises from the welding of such steels using arc welding processes with filler metal. In this study, S960QL steel is extensively used in the heavy transport, lifting and mining industry, where mobile or fixed structures have to carry high loads – often in safety critical situations. In order to sustain extreme characteristics of these high strength low alloy steels, it is a must to reduce the manufacturing defects. In the investigations presented in this paper, the influence of arc length on the weld metal hydrogen concentration was studied according to the ISO DIS 3690 in S960QL type steel with submerged arc welding. Measurement of the diffusible hydrogen was carried out by means of carrier gas hot extraction method. The weld seams with different arc length have similar chemical compositions. Maximum hardness values in the range of 410–425 HV1 were measured in the HAZ on both vertical and horizontal rows in welded structure with two mm wire diameter due to recrystallization condition. For four mm wire diameter, the hardness decreasing which is depending on the grain coarsening in the welded samples with two mm was not occurred in the weld seam-HAZ interface. The larger weld pool and the long arc length increased possibility of hydrogen pick-up and absorbing. Because of this reason, the diffusible hydrogen contents in the welded structure increased in accordance with the arc length.Keywords
This publication has 27 references indexed in Scilit:
- Strengthening mechanisms in a pipeline microalloyed steel with a complex microstructureMaterials Science and Engineering: A, 2013
- Strengthening of HSLA steels by cool deformationMaterials Science and Engineering: A, 2010
- Effect of vanadium and titanium modification on the microstructure and mechanical properties of a microalloyed HSLA steelMaterials Science and Engineering: A, 2010
- Fatigue assessment of root failures in HSLA steel welded joints: A comparison among local approachesInternational Journal of Fatigue, 2009
- Effect of heat-input on austenite grain size in the heat-affected zone of HSLA-100 steelMaterials Science and Engineering: A, 2007
- Effect of nickel and molybdenum additions on weld metal toughness in a submerged arc welded HSLA line-pipe steelJournal of Materials Processing Technology, 2006
- Hydrogen assisted cracking of high-strength weldable steels in sea-waterJournal of Materials Processing Technology, 2005
- Effects of cooling rate and isothermal holding on the precipitation behavior during continuous casting of Nb–Ti bearing HSLA steelsScripta Materialia, 2003
- Complex heterogeneous precipitation in titanium–niobium microalloyed Al-killed HSLA steels—II. Non-titanium based particlesActa Materialia, 2000
- Effect of increasing deposition rate on the bead geometry of submerged arc weldsJournal of Materials Processing Technology, 1997