Magnetic properties of electrodeposited Co-W thin films
Authors:
- 1 September 1987
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 62 (5) , 1943-1947
Abstract
Thin films of Co‐W, 300–500 Å thick, were electrodeposited at various compositions under a wide range of plating conditions. The saturation magnetization, coercivity, and squareness ratio of the films were derived from the parallel (in‐plane) and perpendicular hysteresis loops, measured by using a vibrating sample magnetometer. The magnetic properties of the films are strongly related to their microstructure. The nonmagnetic alloying element (W) affects the saturation magnetization via the dilution mechanism. The in‐plane coercivity, which increases with increasing content of the hexagonal phase and with decreasing degree of [0001]h texture, is in the range of 100–600 Oe for the crystalline deposits and decreases to a few oersteds for amorphous deposits. The in‐plane squareness ratio increases with the fcc or amorphous phase content and with decreasing degree of [0001]h texture. The magnetic measurements suggest that films that appeared amorphous according to their electron diffraction patterns are actually microcrystalline or at least partially crystallized.Keywords
This publication has 5 references indexed in Scilit:
- Microstructure of electrodeposited Co-W thin filmsJournal of Applied Physics, 1986
- Structure and magnetic properties of electrodeposited cobaltSurface Technology, 1978
- Structure of Noncrystalline Co-25 a/o W ElectrodepositJournal of the Electrochemical Society, 1972
- High coercive force films of cobalt-nickel with additions of group VA and VIB elementsIEEE Transactions on Magnetics, 1970
- Electrocrystallography of Cobalt and Cobalt-Nickel Alloys1961