Abstract
The cathode efficiency for intermediate temperature solid oxide fuel cells is largely limited by the catalytic activity for oxygen reduction reaction. Here by, we design and synthesize CuCo 2 O 4 decorated Er 0.4 Bi 1.6 O 3 cathode by means of a simple gelation method and then screen‐print it on scandium‐stabilized zirconia electrolyte cell followed by a relatively lower temperature sintering process. The decoration of CuCo 2 O 4 adequately enhances the electro‐catalytic activity of the composite cathode for the ORR. In addition, Er 0.4 Bi 1.6 O 3 matrix also reduces the sintering temperature (from 1000 °C to 850 °C) compared to the pristine CuCo 2 O 4 electrode. The CuCo 2 O 4 ‐decorated‐Er 0.4 Bi 1.6 O 3 composite cathode demonstrates a lower polarization resistance (0.016 Ω cm 2 at 800 °C) in air, exhibiting an 87% decrease in comparison to the primary CuCo 2 O 4 cathode.
Funding Information
  • National Natural Science Foundation of China (21646012)
  • State Key Laboratory of Urban Water Resource and Environment
  • Harbin Institute of Technology (2016DX08)
  • China Postdoctoral Science Foundation (2016 M600253, 2017T100246)

This publication has 31 references indexed in Scilit: