Abstract
Well-defined 200 nm size titania–silica (Si/Ti atomic ratio of 0.19–1.5) spherical particles containing octadecylamine (ODA) were prepared by the hydrolysis and co-condensation of titanium tetraisopropoxide and tetraethoxysilane in the presence of ODA. ODA was extracted from the spherical particles using acidic ethanol to obtain nanoporous particles. The nanoporous titania–silica particles were calcined at 800 °C for 1 h to obtain nanoporous titania–silica particles composed of anatase crystallites and amorphous silica. Depending on the Si/Ti ratio, the size of anatase crystallites varied: 10 nm for the titania–silica particles at the Si/Ti ratio of 0.19 and 2 nm for those at the Si/Ti ratio of 1.5. The efficiency of photocatalytic decomposition of methylene blue was remarkably suppressed when the titania–silica particles at the Si/Ti ratio of 1.5 were used, though the bandgap absorption was possible at the same wavelength region for all the products.