The effect of slag addition on strength development of Class C fly ash geopolymer concrete at normal temperature
- 1 January 2017
- conference paper
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 1887, 020030
Abstract
This paper presents the effect of slag addition on strength development and workability of fly ash/slag based geopolymer (FASLG) concrete cured at normal temperature. Class C fly ash with high ferrite (Fe) content was used as the primary material. The proportions of fly ash (FA) to slag (SL) are: 1 FA : 0 SL, 0.9 FA : 0.1 SL, 0.7 FA : 0.3 SL, and 0.5 FA : 0.5 SL. The workability and strength properties were determined by slump, vikat, and compressive strength tests. The result shows that the highest compressive strength was achieved by FASLG-3 concrete with 30% slag addition and exhibited a comparable strength to that normal concrete at 28 days. The 30% slag addition also improve the workability and increase the setting time of FASLG concrete specimens. It can be concluded that the slag inclusion on fly ash will improve the performance of geopolymer concrete at normal temperature.Keywords
This publication has 8 references indexed in Scilit:
- Long Term Performance of Alkali Activated Slag ConcreteJournal of Advanced Concrete Technology, 2015
- The Strength of Alkali-activated Slag/fly Ash Mortar Blends at Ambient TemperatureProcedia Engineering, 2015
- Effect of GGBFS on setting, workability and early strength properties of fly ash geopolymer concrete cured in ambient conditionConstruction and Building Materials, 2014
- Modeling of Carbon Dioxide Measurement on Cement PlantsAdvanced Materials Research, 2012
- A review on the utilization of fly ashProgress in Energy and Combustion Science, 2010
- The greening of the concrete industryCement and Concrete Composites, 2009
- Properties of steel fiber reinforced fly ash concreteConstruction and Building Materials, 2009
- Utilization of copper slag in cement and concreteResources, Conservation and Recycling, 2008