Low‐Temperature Spark Plasma Sintering of Pure Nano WC Powder
- 2 May 2013
- journal article
- research article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 96 (6) , 1702-1705
Abstract
For the first time we have demonstrated the densification of high‐purity nanostructured (d avg ≈ 60 nm) tungsten carbide by High Pressure Spark Plasma Sintering ( HPSPS ) in the unusually low temperature range of 1200°C–1400°C. The high‐pressure sintering (i.e., 300 MPa) produced dense material at a temperature as low as 1400°C. In comparison with more conventional sintering techniques, such as SPS (80 MPa) or hot isostatic pressing, HPSPS lowered the temperature required for full densification by 400°C–500°C. High Pressure Spark Plasma Sintering, even in absence of any sintering aid or grain growth inhibitor, retained a very fine microstructure resulting in a significant improvement in both hardness (2721 HV 10 ) and fracture toughness (7.2 MPa m 1/2 ).Keywords
This publication has 13 references indexed in Scilit:
- Influence and effectivity of VC and Cr3C2 grain growth inhibitors on sintering of binderless tungsten carbideInternational Journal of Refractory Metals and Hard Materials, 2012
- Highly Transparent Pure Alumina Fabricated by High‐Pressure Spark Plasma SinteringJournal of the American Ceramic Society, 2010
- Pressure Effect on the Homogeneity of Spark Plasma‐Sintered Tungsten Carbide PowderJournal of the American Ceramic Society, 2009
- Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide – A reviewInternational Journal of Refractory Metals and Hard Materials, 2009
- Sparking plasma sintering of nanometric tungsten carbideInternational Journal of Refractory Metals and Hard Materials, 2009
- Binderless WC and WC–VC materials obtained by pulsed electric current sinteringInternational Journal of Refractory Metals and Hard Materials, 2008
- Effects of AGG on fracture toughness of tungsten carbideMaterials Science and Engineering: A, 2007
- HRTEM Microstructure and Segregation Amount of Dopants at WC/Co Interfaces in TiC and TaC Mono-doped WC-Co Submicro-grained HardmetalsJournal of the Japan Society of Powder and Powder Metallurgy, 2006
- On hardness and toughness of ultrafine and nanocrystalline hard materialsInternational Journal of Refractory Metals and Hard Materials, 1999
- Indentation fracture of WC-Co cermetsJournal of Materials Science, 1985