Microstructures and Mechanical Properties of V-Modified Ti-Zr-Cu-Ni Filler Metals
Open Access
Abstract
TA2 titanium alloy was brazed with Ti-Zr-Cu-Ni-V filler metals developed in a laboratory. The melting properties, the microstructures, phase compositions of filler metals and wettability, erosion properties, tensile properties of the brazed joint were studied in detail. The results show that with the increase of V content, the solidus–liquidus temperature of Ti-Zr-Cu-Ni-V filler metals increased, but the temperature difference basically remained unchanged, trace V element had a limited influence on the melting temperature range of Ti-Zr-Cu-Ni filler metals. The microstructure of Ti-Zr-Cu-Ni-1.5V filler metal was composed of Ti, Zr matrix, (Zr, Cu) solid solution and crystal phase. With the addition of V content, these phases containing V such as Ni3VZr2, NiV3, Ni2V in the molten filler metals increased. V was more inclined to combine with Ni to slow down the diffusion of Ni to titanium matrix. The wettability of filler metal with trace (≤0.5 wt.%) V to TA2 titanium alloy became worse, the wettability improved significantly with continuous increase of V content. The thickness of embrittlement layer and intergranular infiltration region decreased significantly by adding V. With the increase of V content, V could regulate the brazing interface reaction, more strengthened phases generated, which resulted the significant increase of the strength (302.72 MPa) and plasticity index (16.3%) of the brazed joint with Ti-Zr-Cu-Ni-1.5V filler metal.Keywords
Funding Information
- 2021 Shaanxi Provincial Department of Education Special scientific research Plan project (21JK0739, HNKJ20-H42)
- Science and Technology Project of China Huaneng Group Co., Ltd. (21JK0739, HNKJ20-H42)
This publication has 19 references indexed in Scilit:
- The influence of Zr content on the performance of TiZrCuNi brazing fillerMaterials Science and Engineering: A, 2016
- Microstructures and Mechanical Properties of Vacuum Brazed Ti3Al/TiAl Joints Using Two Ti-based Filler MetalsJournal of Materials Science & Technology, 2016
- Influence of grain size, aging conditions and tension rate on the mechanical behavior of titanium low-cost metastable beta-alloy in thermally hardened conditionMaterials Science and Engineering: A, 2015
- Microstructural, mechanical and fractographical study of titanium-CP and Ti–6Al–4V similar brazing with Ti-based fillerMaterials Science and Engineering: A, 2013
- Infrared brazing Ti–6Al–4V and SP-700 alloys using the Ti–20Zr–20Cu–20Ni braze alloyMaterials Letters, 2007
- Infrared brazing of high-strength titanium alloys by Ti–15Cu–15Ni and Ti–15Cu–25Ni filler foilsMaterials Science and Engineering: A, 2006
- Brazing of Titanium and Production of All Titanium Heat ExchangerDenki-Seiko[Electric Furnace Steel], 2003
- Diffusion brazing of Ti-21V-4Al .BETA.-Type titanium alloy using Ti-Base filler.QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY, 1989
- Microstructure of titanium joint made with Ti-Zr base brazing fillers.QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY, 1989
- Structure and mechanical properties of CP Ti and Ti-6Al-4V alloy brazed joints with Ti-base amorphous filler metals.QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY, 1987