Deposition and electrical properties of i n s i t u phosphorus-doped silicon films formed by low-pressure chemical vapor deposition
Authors:
- 1 March 1987
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 61 (5) , 1898-1904
Abstract
The low‐pressure chemical vapor deposition of phosphorus‐doped silicon films on oxidized silicon wafers was investigated as a function of phosphine/silane mole ratio, silane partial pressure, temperature, and wafer spacing. The deposition rate decreases, concomitant with increased phosphorus incorporation, as the mole ratio increases. The deposition rate tends to saturate or vary linearly with silane partial pressure for undoped and heavily doped films, respectively. This, together with differing deposition‐rate activation energies of 1.5 and 2.0 eV for undoped and doped films, respectively, is indicative of different reaction mechanisms in the two regimes. As the mole ratio increases, the deposition rate becomes increasingly dependent on the wafer spacing and the radial position on a wafer. Because phosphorus incorporation varies inversely with deposition rate, it develops similar dependencies on wafer spacing and radial position. The majority of these observations are interpretable in terms of a model that has been defined for the growth of oxide from the silane‐oxygen reaction where the phosphorus and oxygen play analogous roles. The resistivity of annealed films decreases with increased phosphorus incorporation (mole ratio) and for 0.5‐μm‐thick films reaches a minimum value of approximately 440 μΩ cm at about 1021 phosphorus atoms cm−3. The resistivity decreases with increasing deposition temperature which may be attributable to one or a combination of the decreased phosphorus incorporation at higher temperature or deposition rate, or decreased grain size at higher temperature. The decrease in resistivity with increased thickness is attributed to increased grain size with increasing thickness. At least for thicknesses less than 0.5 μm, lower resistivity is achieved by in situ doping than by doping of films subsequent to deposition.Keywords
This publication has 19 references indexed in Scilit:
- Fabrication and Characterization of Epitaxial Heavily Phosphorus‐Doped SiliconJournal of the Electrochemical Society, 1985
- Characterization of Oxide Growth at High Temperatures and Low Pressures from Silane/Nitrous Oxide ReactionJournal of the Electrochemical Society, 1985
- Modeling of the Reaction for Low Pressure Chemical Vapor Deposition of Silicon DioxideJournal of the Electrochemical Society, 1985
- Phosphorus‐Doped Polycrystalline Silicon via LPCVD: I . Process CharacterizationJournal of the Electrochemical Society, 1984
- P‐Doped Polysilicon Film Growth TechnologyJournal of the Electrochemical Society, 1982
- The LPCVD Polysilicon Phosphorus Doped In Situ as an Industrial ProcessJournal of the Electrochemical Society, 1982
- Semi-insulating polysilicon (SIPOS) deposition in a low pressure CVD reactor: I. Growth kineticsJournal of Crystal Growth, 1981
- Discussion of “The Incorporation of Phosphorus in Silicon Epitaxial Layer Growth” [J. Bloem, L. J. Gilling, and M. W. M. Graef (pp. 1354–1357, Vol. 121, No. 10)]Journal of the Electrochemical Society, 1975
- The Incorporation of Phosphorus in Silicon Epitaxial Layer GrowthJournal of the Electrochemical Society, 1974
- Doping in chemically vapour deposited epitaxial siliconJournal of Crystal Growth, 1972