The cyclic crack-growth resistance of a Ti-6Al-4V-0.20 w/o 0 alloy, originally mill annealed, is found to be improved significantly through beta annealing. This improvement is particularly pronounced below a transition point in the crack-growth behavior of the beta-annealed material, which occurs at a stress-intensity range Delta K = 23 MPa.(m to the 1/2 power). Below this point, the exponent in the growth rate law (da/dN = C(Delta K)to the m power) changes from approximately 3.1 (above) to 6.3 (below). Consequently, crack-growth rates da/dN below the transition point are reduced by as much as an order of magnitude below the levels determined for the mill-annealed condition at comparable Delta K levels. This reduction is due to crack bifurcation.