Abstract
A LiNi0.5Mn1.5O4LiNi0.5Mn1.5O4 material for use as a 5V5V spinel cathode for lithium-ion batteries was synthesized for the first time using a hydrothermal approach. The effects of the LiOH concentration and hydrothermal temperature on the hydrothermal products were investigated systematically, where the LiOH concentration (e.g., 1.1M1.1M ) was proven critical to successfully synthesize the 5V5V spinel. At low LiOH concentrations (e.g., 0.8–1.0M0.8–1.0M ), the obtained products may be MnOOH, α-MnO2α-MnO2 , and 4V4V spinel, while high concentrations (e.g., 1.8M1.8M ) favor the Li2MnO3Li2MnO3 phase. The particle size of the as-prepared 5V5V spinel is ca. 30nm30nm , and its formation is associated with the dissolution-recrystallization mechanism from an amorphous precursor. Cell tests show that the as-prepared LiNi0.5Mn1.5O4LiNi0.5Mn1.5O4 material obtained at 180°C180°C exhibits a capacity of ca. 100mAhg−1100mAhg−1 at a current density of 28mAg−128mAg−1 , where ca. 60mAhg−160mAhg−1 above 4.2V4.2V . Such a 5V5V material shows an excellent rate capability with a capacity of ca. 73mAhg−173mAhg−1 delivered at 2800mAg−12800mAg−1 , 73% of that obtained at 28mAg−128mAg−1 .

This publication has 33 references indexed in Scilit: