Abstract
Behavior and characteristics of tungsten materials under impinging high heat fluxes are investigated. Experiments with inertially - not actively - cooled samples have been carried out in the plasma edge of the TEXTOR tokamak to study the changes of material properties such as grain size and abundance of voids or bubbles. In addition, the effects of electron beam impact regarding subsequent W power handling have been studied in view of future devices. The parallel heat flux at the radial position in TEXTOR impinging on the plasma-facing components (PFCs) ranges around q∥ ˜ 45 MW/m2 allowing samples to be exposed at an impact angle of 35 deg to 20 to 30 MW/m2. Melt layer motion perpendicular to the magnetic field is observed following a Lorentz force originating from thermoelectric emission of the hot W sample. Up to 3 g of molten W are redistributed forming hill-like structures at the plasma-connected edge of the sample. The typical melt layer thickness is 1.0 to 1.5 mm. Those hills are, due to the changes in the local geometry, particularly susceptible to even higher heat fluxes of up to the full q∥; hence, locally the temperature of W can reach up to 6000 K, and thus boiling can occur. In terms of material degradation, several aspects are considered: formation of leading edges by redistributed melt, bubble formation, and recrystallization. Bubbles are occurring in sizes between 1 and 200 μm while recrystallization increases the grain size up to 1.5 mm. The power-handling capabilities are severely degraded by all those aspects. Melting of tungsten in future devices is highly unfavorable and needs to be avoided especially in light of uncontrolled transients and possible unshaped PFCs. Predamaged samples from the TEXTOR exposures have also been exposed in the JUDITH 1 facility under transient heat loads (up to ˜1 GW/m2, energy impact: 36 MW · m−2 · s1/2). The samples show an unfavorable increase in the ductile-to-brittle transition temperature. In addition, surface cracks lose their directionality recrystallizing toward a more isotropic state from the manufactured monodirectional state. The increased grain size leads to a more brittle behavior under transient thermal loads with respect to crack progression.Keywords
This publication has 19 references indexed in Scilit:
- Physics basis and design of the ITER plasma-facing componentsJournal of Nuclear Materials, 2011
- Tungsten melt layer motion and splashing on castellated tungsten surfaces at the tokamak TEXTORJournal of Nuclear Materials, 2011
- Analysis of tungsten melt-layer motion and splashing under tokamak conditions at TEXTORNuclear Fusion, 2011
- Main chamber sources and edge transport of tungsten in H-mode plasmas at ASDEX UpgradeNuclear Fusion, 2011
- Calculation and experimental test of the cooling factor of tungstenNuclear Fusion, 2010
- Status of electron temperature and density measurement with beam emission spectroscopy on thermal helium at TEXTORPlasma Physics and Controlled Fusion, 2008
- Investigation of tungsten and beryllium behaviour under short transient eventsFusion Engineering and Design, 2007
- Melt damage simulation of W-macrobrush and divertor gaps after multiple transient events in ITERJournal of Nuclear Materials, 2007
- Experience with bulk tungsten test-limiters under high heat loads: melting and melt layer propagationPhysica Scripta, 2007
- ITER Relevant High Heat Flux Testing on Plasma Facing SurfacesMATERIALS TRANSACTIONS, 2005