Effect of Copper Addition to Titanium Alloy Prepared By Additive Manufacturing for Biomedical Applications

Authors:

Abstract
Infection remains one of the most serious complications in orthopedic and dental implants, and the ongoing search for effective solutions to reduce infection rates has been a focal point of research for decades. The challenge is to create a material with inherent antibacterial properties that do not compromise other essential biomaterial qualities. This study aimed to develop and characterize a novel material based on the widely used Ti-6Al-4V alloy commonly employed in orthopedic and dental medicine. Copper was added as an antimicrobial agent and an essential element in the human body, aiming to promote an intrinsic antibacterial ability of the material. The Ti-6Al-4V alloy was produced using additive manufacturing via laser-based direct energy deposition (DED-LB). A laser is applied to melt the locally fed Ti-6Al-4V metal powder and fuse it with the previously deposited layer. The Ti-6Al-4V- x Cu alloy was also produced using DED-LB, but copper powder was added to the Ti-6Al-4V powder. Materials characterization was performed using scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). Electrochemical tests were conducted in simulated physiological solutions (Hanks balanced salt solution, 0.9 wt.% sodium chloride and artificial saliva). Commercially available wrought Ti-6Al-4V alloy, produced by conventional metallurgical methods, was used as a reference (1). The microstructure and corrosion resistance of alloys manufactured by DED-LB have been addressed less extensively than those produced by power bed fusion processes. The composition, structure and electrochemical behaviour of Ti-6Al-4V alloy produced by two different methods: (i) wrought alloy produced by conventional metallurgy and (ii) additively manufactured (AM) alloy produced by DED-LB from Ti-6Al-4V without and with Cu powders were studied. Although the wrought and AM Ti-6Al-4V alloys shared identical chemical compositions, they exhibited distinct microstructures. The wrought alloy featured an α-phase matrix with intergranular β-phase, whereas the AM-produced alloys presented a lamellar Widmanstätten structure. Adding copper to the Ti-6Al-4V alloy reflected changes in the alloy’s microstructure and chemical composition. Both wrought, and DED-LB Ti-6Al-4V alloys exhibited passivation in the simulated physiological solution and showed no signs of localized corrosion. Moreover, the addition of copper did not compromise the alloy’s protective behavior in the simulated solutions, as confirmed by the long-term immersion and osseointegration tests. These results demonstrate that the properties of both DED-LB-produced Ti-6Al-4V and Ti-6Al-4V-Cu alloys are comparable to the commercial wrought alloy, highlighting their potential for further investigation regarding corrosion resistance and biological performance. References: Milošev, D. Sačer, B. Kapun, P. Rodič, The effect of metallographic preparation on the surface characteristics and corrosion behaviour of Ti-6Al-4V alloy in simulated physiological solutions, J. Electrochem. Soc. 171 (2024) 111503. Milošev, P. Rodič, B. Kapun, D. Sačer, A. Nair, D. Kramar, A. Jeromen, E. Govekar, Composition, microstructure and corrosion resistance of DED-LB additively manufactured Ti-6Al-4V alloy: comparison with wrought alloy, submitted. Milošev, B. Kapun, D. Sačer, P. Rodič, Effect of copper addition to titanium alloy prepared by laser-based directed energy deposition, in preparation. Acknowledgements: The Ti-6Al-4V(-Cu) alloys were manufactured at the Faculty of Mechanical Engineering of the University of Ljubljana, Slovenia. This study was financed by the Slovenian Research and Innovation Agency (project No. J7-4639, acronym BIOAD).