Effect of Si and Ca Addition on Delayed Fracture of High-strength Steels
Authors:
Open Access
- 1 January 1993
- journal article
- Published by Iron and Steel Institute of Japan in Tetsu-to-Hagane
- Vol. 79 (6) , 685-691
Abstract
Effect of Si and Ca Addition on Delayed Fracture of High-strength Steels Kenichi TAKAI, Jun-ichi SEKI, Eiichi SAKITA and Kouichi TAKAYAMA Synopsis : Effects of Si and Ca addition on delayed fracture of medium carbon steels with 1400N/mm2 strength were investigated. Silicon and calcium were added at concentrations of 0-2.0% and 30-70ppm, respectively. The delayed fracture characteristics were evaluated by FIP (Federation Internationale de la Precontrainte) test which is a constant tensile load test in 20% NH4SCN solution at 323 K. In order to make clear the effect of adding Ca and Si, the fracture surfaces were examined , and the hydrogen evolution behavior, the diffusion coefficient of hydrogen, and the hydrogen content were measured. It was found that 0.5%Si steels have no effect on the time to fracture regardless of Ca content, while 1.5%Si-30ppm Ca steel has the longest time to fracture. Fractography showed that adding Ca to 0.5%Si steels did not change the intergranular fracture area fraction. However, adding Ca to 1.5%Si steels changed the fracture from intergranular fracture to microvoid coalescence fracture. As for hydrogen behavior after three months from FIP test , 0.5%Si steel released hydrogen at the peak of 500 K, while for the 1.5%Si-30ppm Ca steel the peak was at 700 K. It was suggested that hydrogen released at around 500 K was crucial for delayed fracture characteristics.Keywords
This publication has 1 reference indexed in Scilit:
- Thermal analysis of trapped hydrogen in pure ironMetallurgical Transactions A, 1982