An internal synthesis method for producing a mullite–chromium carbide composite
Author:
- 1 August 1993
- journal article
- Published by Springer Nature in Journal of Materials Research
- Vol. 8 (8) , 2035-2039
Abstract
In situ formation of chromium carbide in mullite matrix through the reaction of Cr2O3, SiC, and Al2O3 has been studied. Three different chromium compounds, Cr3Si, Cr3C2, Cr7C3, and mullite were formed. The Cr3Si particles formed first and the Cr7C3 phase was only dominant above 1600 °C. The Cr3C2 phase was the main product chromium carbide at temperatures ranging from 1450–1550 °C. The mullite phase formed concurrently through the reaction of SiO2 with Al2O3. SiO2 is the product of the reaction between Cr2O3 and SiC. The composite hot-pressed at 1450 °C in argon gives a flexural strength and fracture toughness up to 407 MPa and 3.8 MPa m1/2, respectively.Keywords
This publication has 3 references indexed in Scilit:
- SiC matrix composites reinforced with internally synthesized TiB2Journal of Materials Science, 1990
- Toughening Behavior Involving Multiple Mechanisms: Whisker Reinforcement and Zirconia TougheningJournal of the American Ceramic Society, 1987
- Fractographic study of the alumina and zirconia particles embedded in mullite prepared by reaction sinteringJournal of Materials Science, 1986